Title: The “New” ACI Concrete Transportation Construction Inspector Program

Author(s): Luke M. Snell

Publication: Concrete International

Volume: 40

Issue: 10

Appears on pages(s): 30-31

Keywords: certification, exam, inspection, classes

DOI: 10.14359/51711175

Date: 10/1/2018

Abstract:
The ACI Concrete Transportation Construction Inspector program has been updated. A candidate for this certification must pass two exams and show relevant work experience. The article discusses documents from ACI and other organizations containing information applicable for concrete transportation construction inspection, as well as training, exams, and sample questions.




  