Repairing and Upgrading of a Heavy-Duty R/C Slab

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Repairing and Upgrading of a Heavy-Duty R/C Slab

Author(s): Pietro G. Gambarova, Francesco Lo Monte, Seyed M.S. Mousavi, Pietro L. Torregiani, and Mattia Zecchillo

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 104.1-104.10

Keywords: finite-element analysis (of slabs); mixed restraints (in slabs); reinforced-concrete slabs; stiffening beams (in slabs); structural fire design (of R/C slabs); yield-lines method

DOI: 10.14359/51711087

Date: 8/10/2018

Abstract:

A heavy-duty almost square R/C slab is studied in this paper based on two tests performed under the service loads, after adding a stiffening R/C beam along the only free edge. The very linear behavior exhibited during the tests was the starting point: (a) to perform a FE analysis to investigate the role of the mixed restraints; (b) to identify the most probable failure mechanisms – under distributed and concentrated loading - within the kinematic theorem of Limit Analysis (Yield-Line Method); (c) to quantify the extra strength provided by the stiffening beam; and (d) to study the bearing capacity in fire.

Slab sides are close to 8 m [27 ft] and the thickness is 35 cm [13.8 in.]. Two adjoining sides rest on walls, while the third side is partially supported and the fourth side - initially free – has been stiffened by casting an R/C beam along the extrados.

The mixed restraints show that (a) not always the yield lines and the failure mechanisms dictated by intuition are the most probable; (b) stiffening a free edge may not be required at the serviceability or ultimate limit states, but by the checks in fire; and (c) stiffening a free edge tends to shift the failure mechanism towards slab-localized mechanisms, because of the greater heat sensitivity of thin slabs compared with solid beams.