GFRP-Reinforced Foundation Slab Design for 15 Story Residential Building

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: GFRP-Reinforced Foundation Slab Design for 15 Story Residential Building

Author(s): Vladimir Kakusha, Oleg Kornev, Mikhail Kovalev, Andrey Lapshinov, and Egor Litvinov

Publication: Symposium Paper

Volume: 326

Issue:

Appears on pages(s): 57.1-57.8

Keywords: glass fiber-reinforced polymer (GFRP) bars, concrete, foundation slab, durability, design, residential building

DOI: 10.14359/51711040

Date: 8/10/2018

Abstract:
This paper represents the summary of the design criteria and construction details for the GFRP (glass fiber-reinforced polymer) reinforced foundation slab. The idea was to improve the foundation slab durability by using GFRP bars. This included the use of GFRP bars as main longitudinal reinforcement for the foundation slabs which represents the world first application of this type. During the design procedures, several non-standard issues related to GFRP reinforcement have been solved. The method statement has been created for Construction Company with the consideration of the specific properties of GFRP bars in comparison to steel reinforcement. Before the casting of concrete, strain gauges were attached to GFRP bars and concrete surface to control the strains during the erection and the maintenance of building.