Protection against Reinforcement Corrosion Using Phosphoric Acid-Based Rust Converter

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Protection against Reinforcement Corrosion Using Phosphoric Acid-Based Rust Converter

Author(s): A. Alhozaimy, R. R. Hussain, A. Al-Negheimish, J. K. Singh, and D. D. N. Singh

Publication: Materials Journal

Volume: 115

Issue: 6

Appears on pages(s): 935-944

Keywords: chloride; corrosion; phosphoric acid; reinforcement; rust

DOI: 10.14359/51706943

Date: 11/1/2018

Abstract:
The protective properties of a newly developed phosphoric acidbased rust converter are investigated for reinforcement corrosion under chloride-contaminated concrete environment. The electrochemical evaluation of specimens after 6 years (2 years of wet-dry exposure in 3.5% sodium chloride solution and 4 years in dry laboratory environment) demonstrated that treating the reinforcing bar with the newly developed product significantly reduced the corrosion rate compared to the control reinforcing bar. Based on the results of Raman spectroscopy, X-ray diffraction (XRD), and scanning electron microscopy, a new mechanism is described for the transformation of unstable rust phases into stable phases. It is observed that iron phosphate remains entrapped with corrosion products formed on the surface of the treated steel reinforcing bar, even after 6 years of exposure.

Related References:

1. Kofstand, P., High Temperature Corrosion, Elsevier Applied Science Publishers, London, UK, 1998.

2. Gaur, B.; Singh, T. B.; and Singh, D. D. N., “Beneficial Role of Chloride Ions During Pickling of Steel in Sulfuric Acid,” Corrosion, V. 52, No. 2, 1996, pp. 154-159. doi: 10.5006/1.3292106

3. Singh, D. D. N.; Ghosh, R.; and Singh, J., “Corrosion Performance of Steel Reinforcing Bars Embedded in Chloride Contaminated Concrete Pore Mortars—Role of Surface Pre-Treatments,” Metals Materials and Processes, V. 16, 2003, pp. 313-326.

4. Ghods, P.; Isgor, O. B.; McRae, G. A.; Li, J.; and Gu, G. P., “Microscopic Investigation of Mill Scale and its Proposed Effect on the Variability of Chloride-Induced Depassivation of Carbon Steel Reinforcing Bar,” Corrosion Science, V. 53, No. 3, 3 2011, pp. 946-954.

5. Ghods, P.; Isgor, O. B.; McRae, G.; and Gu, G. P., “Electrochemical Investigation of Chloride-Induced Depassivation of Black Steel Rebar under Simulated Service Conditions,” Corrosion Science, V. 52, No. 5, 2010, pp. 1649-1659. doi: 10.1016/j.corsci.2010.02.016

6. Hurley, M. F., and Scully, J. R., “Threshold Chloride Concentrations of Selected Corrosion-Resistant Rebar Materials Compared to Carbon Steel,” Corrosion, V. 62, No. 10, 2006, pp. 892-904. doi: 10.5006/1.3279899

7. Li, L., and Sagüés, A. A., “Chloride Corrosion Threshold of Reinforcing Steel in Alkaline Solutions—Open-Circuit Immersion Tests,” Corrosion, V. 57, No. 1, 2001, pp. 19-28. doi: 10.5006/1.3290325

8. Deshpande, P. G.; Seddelmeyer, J. D.; Wheat, H. G.; Fowler, D. W.; and Jirsa, J. O., “Corrosion Performance of Polymer-Coated, Metal-Clad and Other Reinforcing Bars as Reinforcement in Concrete,” Report No. FHWA/TX-03/4904-2, May 2000, http://www.utexas.edu/research/ctr/pdf_reports/4904_2.pdf. (last accesed Nov. 16, 2018)

9. Khayat, K.; James, J.; Ramon, C.; and Harovel, W., “Macrocell Corrosion Study of Fabricated Epoxy Coated Reinforcement,” Corrosion and Corrosion Protection of Steel in Concrete, Proceedings of International Conference, R. Narayan Swamy, ed., Structural Integrity Research Institute, Centre for Cement and Concrete, University of Sheffield, Sheffield Academic Press, Sheffield, UK, 1994, pp. 1244-1253.

10. Chambers, B. D.; Taylor, S. R.; and Lane, D. S., “An Evaluation of New Inhibitors for Reinforcing bar Corrosion in Concrete,” Report VTRC 03-R8, Virginia Transportation Research Council, Charlottesville, VA, Mar. 2003, 61 pp.

11. Virmani, Y. P., “Effectiveness of Calcium Nitrite Admixture as a Corrosion Inhibitor,” Public Roads, V. 54, 1990, pp. 171-182.

12. Pyc, W. A.; Zemajtis, J.; Weyers, R. E.; and Sprinkel, M. M., “Evaluating Corrosion-Inhibiting Admixtures,” Concrete International, V. 21, No. 4, Apr. 1999, pp. 39-44.

13. Pyc, W. A.; Weyers, R. E.; and Sprinkel, M. M., “Corrosion Protection Performance of Corrosion Inhibitors and Epoxy-Coated Reinforcing Steel in a Simulated Concrete Pore Water Solution,” Virginia Transportation Research Council, Charlottesville, VA, 1998.

14. Griffin, D. F., “Corrosion Inhibitors for Reinforced Concrete,” Corrosion of Metals in Concrete, SP-49, L. Pepper, R. G. Pike, and J. A. Willett, eds., American Concrete Institute, Farmington Hills, MI, 1975, pp. 95-101.

15. Srinivasan, R.; Gopalan, P.; Zarriello, P. R.; Myles-Tochko, C. J.; and Meyer, J. H., “Design of Cathodic Protection of Reinforcing Bars in Concrete Structures: An Electrochemical Engineering Approach,” Johns Hopkins APL Technical Digest, V. 17, No. 4, 1996, pp. 363-370.

16. Funahasi, M.; Wagnerand, J.; and Young, W. T., “Cathodic Protection Developments for Prestressed Concrete Components,” Contract No. DTFH61-88-V-00054, Federal Highway Administration, McLean, VA, July 1994.

17. Parks, D. M., and Carello, R. A., “Cathodic Protection of a Reinforced Concrete Bridge and Soffit Using Metallized Zinc,” Report No. 65-328-631138, California State Department of Transportation, Sacramento, CA, Nov. 1992.

18. Simescu, F., and Idrissi, H., “Effect of Zinc Phosphate Chemical Conversion Coating on Corrosion Behaviour of Mild Steel in Alkaline Medium: Protection of Rebars in Reinforced Concrete,” Science and Technology of Advanced Materials, V. 9, No. 4, 2008, pp. 1-10. doi: 10.1088/1468-6996/9/4/045009

19. Girčienė, O.; Samulevičienė, M.; Burokas, V.; and Ramanauskas, R., “Corrosion Behaviour of Phosphated Reinforcing Steel in Alkaline Media Contaminated with Chloride Ions,” Chemija, V. 19, 2008, pp. 14-19.

20. Górecki, G., “Iron Phosphate Coatings—Composition and Corrosion Resistance,” Corrosion, V. 48, No. 7, 1992, pp. 613-616. doi: 10.5006/1.3315980

21. Weng, D.; Jokiel, P.; Uebleis, A.; and Boehni, H., “Corrosion and Protection Characteristics of Zinc and Manganese Phosphate Coatings,” Surface and Coatings Technology, V. 88, No. 1-3, 1997, pp. 147-156. doi: 10.1016/S0257-8972(96)02860-5

22. Ogle, K.; Tomandl, A.; Meddahi, N.; and Wolpers, M., “The Alkaline Stability of Phosphate Coatings I: ICP Atomic Emission Spectroelectrochemistry,” Corrosion Science, V. 46, No. 4, 2004, pp. 979-995. doi: 10.1016/S0010-938X(03)00182-3

23. Jalili, M. M.; Moradian, S.; and Hosseinpour, D., “The Use of Inorganic Conversion Coatings to Enhance the Corrosion Resistance of Reinforcement and the Bond Strength at the Rebar/Concrete,” Construction and Building Materials, V. 23, No. 1, 2009, pp. 233-238. doi: 10.1016/j.conbuildmat.2007.12.011

24. Górecki, G., “Iron Phosphate Coatings Composition and Corrosion Resistance,” Corrosion, V. 19, 1992, pp. 247-328.

25. Rizkalla, S., and Zia, P., “Corrosion Activity of Steel Bars Embedded in Magnesium Phosphate Fiber Reinforced Cementitious Material ‘pcwgrancrete’,” 6th International Engineering and Construction Conference (IECC’6), Cairo, Egypt, American Society of Civil Engineers, 2010.

26. Selph, J. L., and Paul Jr., J. W., “Heat Resistant Phosphate Cement,” U.S. Patent 2013/0008349, Jan. 10, 2013.

27. Bricknell, F. S.; Croydon, W.; and Cork, H. A., “Treatment of Metal Surfaces,” U.S. patent 2,992,131, Patented July 11, 1961.

28. Manna, M., “Characterisation of Phosphate Coatings Obtained Using Nitric Acid Free Phosphate Solution on Three Steel Substrates: An Option to Simulate TMT Rebars Surfaces,” Surface and Coatings Technology, V. 203, No. 13, 2009, pp. 1913-1918. doi: 10.1016/j.surfcoat.2009.01.024

29. Manna, M.; Chakrabarti, I.; and Bandyopadhyay, N., “Effect of Steel Substrate for Phosphate Treatment: An Option to Simulate TMT Rebar Surface,” Corrosion Science, V. 51, No. 3, 2009, pp. 451-457. doi: 10.1016/j.corsci.2008.11.021

30. Manna, M.; Chakrabarti, I.; and Bandyopadhyay, N., “Phosphate Treatment of TMT Rebar Bundle to Avoid Early Rusting: An Option for Single Step Process,” Surface and Coatings Technology, V. 201, No. 3-4, 2006, pp. 1583-1588. doi: 10.1016/j.surfcoat.2006.02.041

31. Lindert, A., and Cormier, G. J., “Poly phenol Compounds and Treatment and After-Treatments Metallic, Plastic and Painted Surfaces Therewith,” U.S. patent No 5,298,289, March 29, 1999.

32. Jaén, E. Y.; Araúz, E. Y.; Iglesias, J.; and Delgado, Y., “Reactivity of Tannic Acid with Common Corrosion Products and Its Influence on the Hydrolysis of Iron in Alkaline Solutions,” Hyperfine Interactions, V. 148-149, No. 1-4, 2003, pp. 199-209. doi: 10.1023/B:HYPE.0000003781.45888.28

33. Yeomans, S. R., “Performance of Black, Galvanized, and Epoxy-Coated Reinforcing Steels in Chloride-Contaminated Concrete,” Corrosion, V. 50, No. 1, 1994, pp. 72-81. doi: 10.5006/1.3293496

34. Singh, D. D. N., and Bhattacharya, D., “Performance and Mechanism of Action of Self-Priming Organic Coating on Oxide Covered Steel Surface,” Progress in Organic Coatings, V. 68, No. 1-2, 2010, pp. 62-69. doi: 10.1016/j.porgcoat.2009.08.017

35. Hare, C. H., “Corrosion and Protection of Metallic Surfaces by Painting,” Federation Series on Coating Technology, Federation of Societies for Paint Technology, Philadelphia, PA, 1978, pp. 5-50.

36. Wu, M.-S.; Higuchi, W. I.; Fox, J. L.; and Friedman, M., “Kinetics and Mechanism of Hydroxyapatite Crystal Dissolution in Weak Acid Buffers Using the Rotating Disk Method,” Journal of Dental Research, V. 55, No. 3, 1976, pp. 496-505. doi: 10.1177/00220345760550033201

37. Higuchi, W. I.; Mir, N. A.; Patel, P. R.; Becker, J. W.; and Hefferren, J. J., “Quantitation of Enamel Demineralization Mechanisms: III. A Critical Examination of the Hydroxyapatite Model,” Journal of Dental Research, V. 48, No. 3, 1969, pp. 396-409. doi: 10.1177/00220345690480031201

38. Cornell, R. M., and Schwertmenn, U., The Iron Oxides: Structure, Properties, Reaction, Occurrence, and Uses,VCH, Weinheim, New York, 1996, 573 pp.

39. Reeves, N. J., and Mann, S., “Influence of Inorganic and Organic Additives on Tailored Synthesis of Iron Oxides,” Journal of the Chemical Society, Faraday Transactions, V. 87, No. 24, 1991, pp. 3875-3880. doi: 10.1039/ft9918703875

40. Morales, M. P.; Carrefio, G.; and Serna, C. J., “The Formation of a-Fe203 Monodispersed Particles in Solution,” Journal of Materials Research, V. 7, No. 9, 1992, pp. 2538-2545. doi: 10.1557/JMR.1992.2538

41. Ocafia, M.; Morales, M. P.; and Serna, C. J., “The Growth Mechanism of γ-Fe2O3 Ellipsoidal Particles in Solution,” Journal of Colloid and Interface Science, V. 171, 1995, pp. 2538-2545.

42. Sugimoto, T., and Muramatsu, A., “Formation Mechanism of Monodispersed α-Fe2O3 Particles in Dilute FeCl3 Solutions,” Journal of Colloid and Interface Science, V. 184, No. 2, 1996, pp. 626-638. doi: 10.1006/jcis.1996.0660

43. Barron, V.; Galvez, N.; Hochella, M. E. Jr.; and Torrent, J., “Epitaxial Overgrowth of Goethite on Hematite Synthesized in Phosphate Media: A Scanning Force and Transmission Electron Microscopy Study,” The American Mineralogist, V. 82, No. 11-12, 1997, pp. 1091-1100. doi: 10.2138/am-1997-11-1206

44. Galvez, N.; Barron, V.; and Torrent, J., “Effect of Phosphate on the Crystallization of Hematite, Goethite, and Lepidocrocite from Ferrihydrite,” Clays and Clay Minerals, V. 47, No. 3, 1999, pp. 304-311. doi: doi10.1346/CCMN.1999.0470306

45. Galvez, N.; Barron, V.; and Torrent, J., “Preparation and Properties of Hematite with Structural Phosphorus,” Clays and Clay Minerals, V. 47, No. 3, 1999, pp. 375-385. doi: 10.1346/CCMN.1999.0470314

46. Cumplido, J.; Barron, V.; and Torrent, J., “Effect of Phosphate on the Formation of Nanophase Lepidocrocite from Fe(ii) Sulfate,” Clays and Clay Minerals, V. 48, No. 5, 2000, pp. 503-510. doi: 10.1346/CCMN.2000.0480502

47. Balasubramaniam, R.; Ramesh Kumar, A. V.; and Dillmann, P., “Characterization of Rust on Ancient Indian Iron,” Current Science, V. 85, 2003, pp. 1546-1555.

48. Torrent, J., and Barron, V., “Key Role of Phosphorus in the Formation of the Iron Oxides in Mars Soils?” Icarus, V. 145, No. 2, 2000, pp. 645-647. doi: 10.1006/icar.2000.6408

49. Dreibus, G.; Brueckner, J.; Lugmair, G. W.; Rieder, R.; and Waenke, H., “Possible Indication of Sedimentary Products and Clay Minerals at the Mars Pathfinder Landing Site: Phosphorus in APXS X-Ray Spectra,” Suppl. EOS Trans. AGU, V. 80, 1999, pp. 375-385.

50. Barron, V., and Torrent, J., “Can the Phosphate Sorption and Occlusion Properties help to Elucidate the Genesis of Specular Hematite on the Mars Surface?” Lunar and Planetary Science, V. 35, 2004, 2 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal