Q; What cover depth should be used for balconies with post-tensioned (PT) and mild reinforcement? Q: I have been informed that ACI 315-99, Details and Detailing of Concrete Reinforcement,1 has been superseded. Which ACI document serves as a replacement to this standard?
Related References:
1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.
2. ACI Innovation Task Group 7, “Specification for Tolerances for Precast Concrete (ACI ITG-7-09),” American Concrete Institute, Farmington Hills, MI, 2009, 37 pp.
3. ACI Committee 315, “Details and Detailing of Concrete Reinforcement (ACI 315-99),” American Concrete Institute, Farmington Hills, MI, 1999, 44 pp.
4. Joint ACI-CRSI Committee 315, “Guide to Presenting Reinforcing Steel Design Details (ACI 315R-18),” American Concrete Institute, Farmington Hills, MI, 2018, 50 pp.