Assessment of Punching Shear of Flat Slabs Using Ground Slag

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Assessment of Punching Shear of Flat Slabs Using Ground Slag

Author(s): Shahab Samad, Attaullah Shah, and Mukesh C. Limbachiya

Publication: Materials Journal

Volume: 115

Issue: 3

Appears on pages(s): 459-469

Keywords: flat slab; ground-granulated blast-furnace slag (GGBS); punching shear

DOI: 10.14359/51702012

Date: 5/1/2018

Abstract:
Limited research work exists on assessment of punching shear of reinforced concrete (RC) flat slabs made with blended cement incorporating ground-granulated blast-furnace slag (GGBS). This research is aimed at analyzing the punching shear strength of RC flat slabs cast from blended cement having GGBS in different proportions as partial replacement of cement. Four flat slabs supported on the ends were tested under column load such that one flat slab was cast from normal concrete with no GGBS and the remaining three flat slabs were cast with 30, 40, and 50% replacement of cement by GGBS. Experimental punching shear, midspan deflections, strain in the steel bars, and cracking pattern of the slabs were determined. The results of punching shear of flat slabs from the tests were compared with the nominal punching shear capacities proposed by BS 8110, BS EN1992-1-1/EC2, and ACI 318. The provisions of these building codes for the punching shear were observed as safe and conservative for the RC flat slab made from blended cement incorporating GGBS.

Related References:

1. Rashad, A. M.; Seleem, H. E.-D. H.; and Shaheen, A. F., “Effect of Silica Fume and Slag on Compressive Strength and Abrasion Resistance of HVFA Concrete,” International Journal of Concrete Structures and Materials, V. 8, No. 1, 2014, pp. 69-81. doi: 10.1007/s40069-013-0051-2

2. Jin, Z.; Lu, X.; and Hu, S., “Alkali Activation of Granulated Blast Furnace Slag,” Advanced Materials Research, V. 158, No. 1, 2011, pp. 1-11.

3. Ling, W.; Pei, T.; and Yan, Y., “Application of Ground Granulated Blast Furnace Slag in High Performance Concrete in China,” International Workshop on Sustainable Development and Concrete Technology, Beijing, China, 2004, pp. 309-317.

4. Nakamura, N.; Saki, M.; and Swamy, R. N., “Effect of Slag Fineness on the Development of Concrete Strength and Microstructure,” Fly Ash, Silica Fume, Slag, and Natural Pozzolans and Natural Pozzolans in Concrete, Proceedings of the Fourth Internanational Conference, SP-132, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1993, pp. 1343-1366.

5. Lim, D. T. Y.; Xu, D.; Divsholi, B. S.; Kondraivendhan, B.; and Teng, S., “Effect of Ultra Fine Slag Replacement on Durability and Mechanical Properties of High Strength Concrete,” 36th Conference on ‘Our World in Concrete & Structures’, Singapore, 2011, 11 pp.

6. Swamy, R. N., “Role of Slag in the Development of Durable and Sustainable High Strength Concretes,” Proceedings of International Symposium on Concrete Technology for Sustainable Development in the 21st Century, Hyderabad, India, 1999, pp. 186-221.

7. Parshwanath, R. N.; Peter, J. A.; Dattatreya, J. K.; Neelamegam, M.; and Gopalakrishnan, S., “Improvement in Properties of High Performance Concrete with Partial Replacement of Cement by Ground Granulated Blast Furnace Slag,” Journal of the Institution of Engineers (India), V. 84, No. 8, 2003, pp. 38-42.

8. Bernal, S. A.; Rodríguez, E. D.; Mejía de Gutiérrez, R.; and Provis, J. L., “Performance at High Temperature of Alkali-Activated Slag Pastes Produced with Silica Fume and Rice Husk Ash Based Activators,” Materiales de Construcción, V. 65, No. 318, 2015, pp. 1-10. doi: 10.3989/mc.2015.03114

9. Bernal, S. A.; Nicolas, R. S.; van Deventer, J. S. J.; and Provis, J. L., “Alkali-Activated Slag Cements Produced with a Blended Sodium Carbonate/Sodium Silicate Activator,” Advances in Cement Research, V. 28, No. 4, 2016, pp. 262-273. doi: 10.1680/jadcr.15.00013

10. “Market Study for a Voluntary Common European Union Certification Scheme for the Energy Performance of Non-Residential Buildings,” Final Report, European Commission, DG Energy, Rotterdam, the Netherlands, 2014, 176 pp.

11. Ragheb, K. S., “Study Punching Shear of Steel Fiber Reinforced Self Compacting Concrete Slabs by Nonlinear Analysis,” World Academy of Science, Engineering and Technology, International Journal of Civil, Environmental, Structural, Construction and Architectural Engineering, 2013, 12 pp.

12. Desai, S. B., “Limits on Load Carrying Capacity of Flat Slab,” The Structural Engineer, V. 78, No. 22, 2000, pp. 26-29.

13. Ruiz, M. F.; Muttoni, A.; and Kunz, J., “Strengthening of Flat Slabs Against Punching Shear Using Post-Installed Shear Reinforcement,” ACI Structural Journal, V. 107, No. 4, July-Aug. 2010, pp. 434-442.

14. Ferreira, M. P.; Melo, G. S.; Regan, P. E.; and Vollum, R. L., “Punching of Reinforced Concrete Flat Slabs with Double Headed Shear Reinforcement,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 363-374.

15. Muttoni, A., “Punching Shear Strength of Reinforced Concrete Slabs without Transverse Reinforcement,” ACI Structural Journal, V. 105, No. 4, July-Aug. 2008, pp. 440-450.

16. Polak, M. A., ed., Punching Shear in Reinforced Concrete Slabs, SP-232, American Concrete Institute, Farmington Hills, MI, 2005, 302 pp.

17. Alexander, S. D. B., and Simmonds, S. H., “Punching Shear Tests of Concrete Slab-Column Joints Containing Fiber Reinforcement,” ACI Structural Journal, V. 89, No. 4, July-Aug. 1992, pp. 425-432.

18. Naaman, A. E.; Likhitruangsilp, V.; and Parra-Montesinos, G. J., “Punching Shear Response of High-Performance Fiber-Reinforced Cementitious Composite Slabs,” ACI Structural Journal, V. 104, No. 2, Mar.-Apr. 2007, pp. 170-177.

19. Cheng, M. Y., and Parra-Montesinos, G. J., “Evaluation Steel Fiber Reinforcement for Punching Shear Resistance in Slab-Column Connections—Part 1: Monotonically Increased Load,” ACI Structural Journal, V. 107, No. 1, Jan.-Feb. 2010, pp. 101-109.

20. De Hanai, J. B., and Holanda, K. M. A., “Similarities between Punching and Shear Strength of Steel Fiber Reinforced Concrete (SFRC) Slabs and Beams,” IBRACON Structures and Material Journal, V. 1, No. 1, Mar. 2008, pp. 1-16.

21. Tan, J., “The Effect of GGBS on Concrete and its Applications,” Guangdong Jiancai, V. 2, 2007, pp. 15-17.

22. Zheng, L.; Paine, K. A.; and Dhir, R. K., “Early-Age Temperature Rises in GGBS Concrete: Part 1: Determination of T1 Values,” Proceedings of International Congress – Global Construction: Ultimate Concrete Opportunities, Thomas Telford, London, UK, 2005, pp. 173-182.

23. Tang, K., “Early-Age Structural and Thermal Performance of GGBS Concrete,” World Academy of Science, Engineering and Technology International Journal of Civil, Environmental, Structural, Construction and Architectural Engineering, 2005, 4 pp.

24. Ngo, D. T., “Punching Shear Resistance of High-Strength Concrete Slabs,” Electronic Journal of Structural Engineering, V. 1, 2001, pp. 52-59.

25. Zohrevand, P.; Yang, X.; Jiao, X.; and Mirmiran, A., “Punching Shear Enhancement of Flat Slabs with Partial Use of Ultrahigh-Performance Concrete,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 9, 2015, p. 04014255 doi: 10.1061/(ASCE)MT.1943-5533.0001219

26. Dönmez, A., and Bažant, Z. P., “Size Effect on Punching Strength of Reinforced Concrete Slabs with and without Shear Reinforcement,” ACI Structural Journal, V. 114, No. 4, July-Aug. 2017, pp. 875-886. doi: 10.14359/51689719

27. El-Ghandour, A. W.; Pilakoutas, K.; and Waldron, P., “Punching Shear Behavior of Fiber Reinforced Polymer Reinforced Concrete Flat Slabs: Experimental Study,” Journal of Composites for Construction, ASCE, V. 7, No. 3, 2003, pp. 258-265. doi: 10.1061/(ASCE)1090-0268(2003)7:3(258)

28. British Standards Institution, “Eurocode 2: Design of Concrete Structures: General Rules and Rules for Buildings (BS EN 1992-1: 2004),” BSI, London, UK, 2004, 230 pp.

29. British Standards Institution, “Structural Use of Concrete (BS 8110-1:1997),” BSI, London, UK, 1997, 168 pp.

30. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318M-14) and Commentary (ACI 318RM-14), American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

31. fib, “fib Model Code for Concrete Structures 2010,” International Federation of Concrete Structures, Lausanne, Switzerland, 2010, 312 pp.

32. Soares, L. F. S., and Vollum, R. L., “Comparison of Punching Shear Requirements in BS 8110, EC2 and MC2010,” Magazine of Concrete Research, V. 67, No. 24, 2015, pp. 1315-1328. doi: 10.1680/macr.14.00432

33. Toutlemonde, F.; Renaud, J.-C.; Lauvin, L.; Brisard, S.; and Resplendino, J., “Local Bending Tests and Punching Failure of a Ribbed UHPFRC Bridge Deck,” Fracture Mechanics of Concrete and Concrete Structures (FraMCos), Catania, Italy, A. Carpinteri, P. Gambarova, G. Ferro, and G. Plizzari, eds., 2007, pp. 1481-1489.

34. Chana, P. S., and Desai, S. P., “Design of Shear Reinforcement against Punching,” The Structural Engineer, V. 70, No. 9, 1992, pp. 159-164.

35. Park, H. G.; Choi, K. K.; and Chung, L., “Strain-Based Strength Model for Direct Punching Shear of Interior Slab-Column Connections,” Engineering Structures, V. 33, No. 3, 2011, pp. 1062-1073. doi: 10.1016/j.engstruct.2010.12.032

36. Chana, P. S., and Desai, S. B., “Membrane Action, and Design against Punching Shear,” The Structural Engineer, V. 70, No. 19, Oct. 1992, pp. 339-343.

37. Regan, P. E., “Punching of Slabs under Highly Concentrated Loads,” Proceedings of the Institution of Civil Engineers – Structures and Buildings, V. 157, No. 2, 2004, pp. 165-171. doi: 10.1680/stbu.2004.157.2.165

38. Papanikolaou, K. V.; Tegos, I. A.; and Kappos, A. J., “Punching Shear Testing of Reinforced Concrete Slabs, and Design Applications,” Magazine of Concrete Research, V. 57, No. 3, 2005, pp. 167-177. doi: 10.1680/macr.2005.57.3.167

39. Kotsovos, M. D., “A New Approach to Deigning Reinforcement to Resist Punching Shear,” The Structural Engineer, V. 88, No. 8, Apr. 2010, pp. 20-25.

40. Kupfer, H.; Hilsdorf, H. K.; and Riisch, H., “Behavior of Concrete Under Biaxial Stresses,” ACI Journal Proceedings, V. 66, Aug, 1969, pp. 656-666.


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer