Experimental Study on Compression Behavior of Fiber- Reinforced Cellular Concrete Stack-Bonded Masonry Prisms

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Study on Compression Behavior of Fiber- Reinforced Cellular Concrete Stack-Bonded Masonry Prisms

Author(s): M. Abdur Rasheed and S. Suriya Prakash

Publication: Materials Journal

Volume: 115

Issue: 1

Appears on pages(s): 149-160

Keywords: analytical models; cellular lightweight concrete (CLC) prisms; compression; macro-/microfibers; stress-strain curves

DOI: 10.14359/51701241

Date: 1/1/2018

Abstract:
This paper presents the stress-strain behavior of structural synthetic fiber-reinforced cellular lightweight concrete (CLC) stack-bonded prisms under axial compression. Masonry compressive strength is typically obtained by testing stack-bonded prisms under compression normal to its bed joint. CLC prisms with cross-sectional dimensions of 200 x 150 mm (7.87 x 5.90 in.) with an overall height of 470 mm (1.54 ft) were cast with and without different dosages of synthetic fiber reinforcement. Polyolefin was used as a structural fiber reinforcement at different volume fractions (vf) of 0.22, 0.33, 0.44, and 0.55% with and without microfiber dosage of 0.02%. Experimental results indicate that the presence of fibers helps in the improvement of strength, stiffness, and ductility of CLC stackbonded prisms under compression. Test results also signify that the hybrid fiber reinforcement provides better crack bridging mechanism both at micro and macro levels when compared to only macrofibers. Simple analytical models were developed for stress-strain behavior of CLC blocks and stack-bonded CLC prisms based on the experimental results with and without fibers under compression.

Related References:

1. Zhang, B., and Poon, C. S., “Use of Furnace Bottom Ash for Producing Lightweight Aggregate Concrete with Thermal Insulation Properties,” Journal of Cleaner Production, V. 99, 2015, pp. 94-100. doi: 10.1016/j.jclepro.2015.03.007

2. Narayanan, N.; Jason, W.; and Jan, O., “Acoustically Efficient Concretes through Engineered Pore Structure,” Autoclaved Aerated Concrete—Properties and Structural Design, SP-226, C. Shi and F. H. Fouad, eds., American Concrete Institute, Farmington Hills, MI, 2005, pp. 135-152.

3. Estabragh, A. R.; Ranjbari, S.; and Javadi, A. A., “Properties of a Clay Soil and Soil Cement Reinforced with Polypropylene Fibers,” ACI Materials Journal, V. 114, No. 2, Mar.-Apr. 2017, pp. 195-206. doi: 10.14359/51689469

4. Albert, M. L.; Elwi, A. E.; and Cheng, J. J. R., “Strengthening of Unreinforced Masonry Walls Using FRPs,” Journal of Composites for Construction, ASCE, V. 5, No. 2, 2001, pp. 76-84. doi: 10.1061/(ASCE)1090-0268(2001)5:2(76)

5. FEMA 306, “Evaluation of Earthquake Damaged Concrete and Masonry Wall Buildings,” Basic Procedures Manual, Report No. ATC-43, Applied Technology Council, Federal Emergency Management Agency, Washington, DC, 1998, 270 pp.

6. Haldar, P.; Singh, Y.; and Paul, D. K., “Identification of Seismic Failure Modes of URM Infilled RC Frame Buildings,” Engineering Failure Analysis, V. 33, 2013, pp. 97-118. doi: 10.1016/j.engfailanal.2013.04.017

7. McNary, W. S., and Abrams, D. P., “Mechanics of Masonry in Compression,” Journal of Structural Engineering, ASCE, V. 111, No. 4, 1985, pp. 857-870. doi: 10.1061/(ASCE)0733-9445(1985)111:4(857)

8. Gumaste, K. S.; Nanjunda Rao, K. S.; Venkatarama Reddy, B. V.; and Jagadish, K. S., “Strength and Elasticity of Brick Masonry Prisms and Wallettes under Compression,” Materials and Structures, V. 40, No. 2, 2007, pp. 241-253. doi: 10.1617/s11527-006-9141-9

9. Venkatarama Reddy, B. V., and Uday Vyas, C. V., “Influence of Shear Bond Strength on Compressive Strength and Stress-Strain Characteristics of Masonry,” Materials and Structures, V. 41, No. 10, 2008, pp. 1697-1712. doi: 10.1617/s11527-008-9358-x

10. IS 1905-1987, “Structural Use of Unreinforced Masonry (third revision),” Bureau of Indian Standards (BIS), New Delhi, India, 1987.

11. Rasheed, M. A., and Prakash, S. S., “Mechanical Behavior of Sustainable Hybrid-Synthetic Fiber Reinforced Cellular Light Weight Concrete for Structural Applications of Masonry,” Construction and Building Materials, V. 98, 2015, pp. 631-640. doi: 10.1016/j.conbuildmat.2015.08.137

12. Prakash, S. S.; Aqhtarudin, M.; and Dhara, J. S., “Behaviour of Soft Brick Masonry Small Assemblies with and without Strengthening under Compression Loading,” Materials and Structures, V. 49, No. 7, 2016, pp. 2919-2934. doi: 10.1617/s11527-015-0695-2

13. Srikar, G.; Anand, G.; and Suriya Prakash, S., “A Study on Residual Compression Behavior of Structural Fiber Reinforced Concrete Exposed to Moderate Temperature Using Digital Image Correlation,” International Journal of Concrete Structures and Materials, V. 10, No. 1, 2016,

pp. 75-85. doi: 10.1007/s40069-016-0127-x

14. Zollo, R. F., and Hays, C. D., “Engineering Material Properties of a Fiber Reinforced Cellular Concrete,” ACI Materials Journal, V. 95, No. 5, Sept.-Oct. 1998, pp. 631-635.

15. Kearsley, E. P., and Mostert, H. F., “The Use of Foamcrete in Southern Africa,” High-Performance Concrete, SP-172, American Concrete Institute, Farmington Hills, MI, 1997, pp. 919-934.

16. Rasheed, M. A., and Prakash, S. S., “Behavior of Hybrid-Synthetic Fiber Reinforced Cellular Lightweight Concrete under Uni-Axial Tension - Experimental and Analytical Studies,” Construction and Building Materials, V. 162, 2017, pp. 857-870.

17. Valore, R. C. Jr, “Cellular Concrete Part 1 Composition and Methods of Production,” ACI Journal Proceedings, V. 50, No. 5, May 1954,

pp. 773-796.

18. Brugg Contec AG, “Concrix—Technical Datasheet,” Domat/Ems, Switzerland, http://www.bruggcontec.com/media/datasheet_concrix_es-en.pdf. (last accessed Jan. 9, 2018)

19. ASTM C869-91(1999), “Standard Specification for Foaming Agents Used in Making Preformed Foam for Cellular Concrete,” ASTM International, West Conshohocken, PA, 1991, 2 pp.

20. Wee, T. H.; Babu, D. S.; and Tamilselvan, T., “Air-Void Systems of Foamed Concrete and Its Effect on Mechanical Properties,” ACI Materials Journal, V. 103, No. 1, Jan.-Feb. 2006, pp. 45-52.

21. Drysdale, R. G., and Hamid, A. A., Masonry Structures: Behavior and Design, The Masonry Society, Boulder, CO, 2008.

22. Prakash, S. S., and Alagusundaramoorthy, P., “Load Resistance of Masonry Wallettes and Shear Triplets Retrofitted with GFRP Composites,” Journal of Cement Concrete and Composites, V. 30, No. 8, 2008, pp. 745-761. doi: 10.1016/j.cemconcomp.2007.11.005

23. Sarangapani, G.; Venkatarama Reddy, B. V.; and Jagadish, K. S., “Brick-Mortar Bond and Masonry Compressive Strength,” Journal of Materials in Civil Engineering, ASCE, V. 17, No. 2, 2005, pp. 229-237. doi: 10.1061/(ASCE)0899-1561(2005)17:2(229)

24. Kaushik, H. B.; Rai, D. C.; and Jain, S. K., “Stress-Strain Characteristics of Clay Brick Masonry under Uniaxial Compression,” Journal of Materials in Civil Engineering, ASCE, V. 19, No. 9, 2007, pp. 728-739. doi: 10.1061/(ASCE)0899-1561(2007)19:9(728)


ALSO AVAILABLE IN:

Electronic Materials Journal