Investigation on Punching Behavior of Pile Cap under Column Reinforced by Section Steel Truss

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Investigation on Punching Behavior of Pile Cap under Column Reinforced by Section Steel Truss

Author(s): Honglei Guo

Publication: Structural Journal

Volume: 115

Issue: 2

Appears on pages(s): 379-390

Keywords: bearing capacity; pile cap; punching; section steel truss; strut-and-tie

DOI: 10.14359/51700948

Date: 3/1/2018

Abstract:
Despite many investigations on the spatial strut-and-tie mechanical mechanism on pile cap punching failure at present, little has been reported on its application. Meanwhile, compared with the steel-reinforced concrete structure extensively existing in the superstructure, that in the foundation structure is yet seldom seen. The real section steel truss of better material properties was used to replace the virtual truss originally regarded as the concrete stress flow for this reason. Aiming at the punching-force bearing behavior of this kind of the pile cap reinforced by the section steel truss, two series (the first is four six-pile caps and the second is two four-pile caps) of the full-size experimental study and the theoretical analysis have been made. Under the condition of the same reinforcing steel amount, in contrast to the ordinary reinforced pile cap, this kind of the section steel truss pile cap can increase the bearing capacity and ductility. It transfers load according to the spatial strut-and-tie. Before a definite column load, the column load is born jointly by the section steel truss and the concrete spatial strut-and-tie. Then, after the concrete strut is decomposed into the two ones coupled at the two ends, the section steel truss gradually shifts into the bearing main-body. With the total yield of the section steel strut and the complete damage to the concrete strut of the splitting in the midpart plus the shear-compression at the two ends, the punching cone is formed. The failure to the composite strut of the section steel and the concrete is an indication of the loss of the pile cap punching bearing capacity. The bearing capacity calculation formulas were deduced based on this, which agree well with the test results.

Related References:

1. Blévot, J. L., and Frémy, R., “Semelles sur Pieux,” Institute Technique du Bâtiment et des Travaux Publics, V. 20, No. 230, 1967, pp. 223-295.

2. Taylor, H. P. J., and Clarke, J. L., “Some Detailing Problems in Concrete Frame Structures,” The Structural Engineer, V. 54, No. 1, Jan. 1976, pp. 19-29.

3. Sabnis, G. M., and Gogate, A. B., “Investigation of Thick Slab (Pile Cap) Behavior,” ACI Journal Proceedings, V. 81, No. 1, Jan.-Feb. 1984, pp. 35-39.

4. Adebar, P.; Kuchma, D.; and Collins, M. P., “Strut-and-Tie Models for the Design of Pile Caps: An Experimental Study,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 81-92.

5. Suzuki, K.; Otsuki, K.; and Tsubata, T., “Experimental Study on Four-Pile Caps with Taper,” Transactions of the Japan Concrete Institute, V. 21, 1999, pp. 327-334.

6. Suzuki, K.; Otsuki, K.; and Tsuhiya, T., “Influence of Edge Distance on Failure Mechanism of Pile Caps,” Transactions of the Japan Concrete Institute, V. 22, 2000, pp. 361-368.

7. Suzuki, K., and Otsuki, K., “Experimental Study on Corner Shear Failure of Pile Caps,” Transactions of the Japan Concrete Institute, V. 23, 2002.

8. Adebar, P., and Zhou, Z., “Bearing Strength of Compressive Struts Confined by Plain Concrete,” ACI Structural Journal, V. 90, No. 5, Sep.-Oct. 1993, pp. 534-541.

9. Guo, H., “Evaluation of Column Load for Generally Uniform Grid-Reinforced Pile Cap Failing in Punching,” ACI Structural Journal, V. 112, No. 2, Mar.-Apr. 2015, pp. 123-134. doi: 10.14359/51687420

10. Schlaich, J.; Schafer, K.; and Jennewein, M., “Toward a Consistent Design of Structural Concrete,” PCI Journal, V. 32, No. 3, 1987, pp. 74-150. doi: 10.15554/pcij.05011987.74.150

11. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-08) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2008, 473 pp.

12. CAN/CSAA23, 3-04(R2010), “Design of Concrete Structures,” Canadian Standard Association, Toronto, ON, Canada, 2010, pp. 63-65.

13. BSEN 1992-1-1:2004, “Eurocode 2: Design of Concrete Structures-Part 1-1: General Rules and Rules for Buildings,” British Standards Institution, London, UK, 2004, pp. 107-110.

14. AS3600-2001, “Concrete Structures,” Council of Standards Australia, Sydney, Australia, 2001, pp. 124-125.

15. Klein, G. J., “Example 9: Pile Cap,” presented at ACI Fall Convention, on Examples for the Design of Structural Concrete with Strut-and-Tie Models, Phoenix, AZ, 2002, pp. 213-223.

16. HKS INC, “ABAQUS/Standard User’s Manual; ABAQUS Theory Manual,” Hibbitt, Karlsson and Sorensen, Inc., 2005.


ALSO AVAILABLE IN:

Electronic Structural Journal