Title: Role of Rheology in Achieving Successful Concrete Performance

Author(s): Chiara F. Ferraris, Peter Billberg, Raissa Ferron, Dimitri Feys, Jiong Hu, Shiho Kawashima, Eric Koehler, Mohammed Sonebi, Jussara Tanesi, and Nathan Tregger

Publication: Concrete International

Volume: 39

Issue: 6

Appears on pages(s): 43-51

Keywords: yield, viscosity, flow, thixotropy

DOI:

Date: 6/1/2017

Abstract:
Concrete rheology is introduced, and insights are provided into how rheology applies to mixture design and quality control, segregation, pumping, formwork pressure, and surface finish. Basic terminology is provided along with explanations of typical measuring instruments and testing procedures used to determine rheological properties.




  


ABOUT THE INTERNATIONAL CONCRETE ABSTRACTS PORTAL

  • The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

Edit Module Settings to define Page Content Reviewer