Rapid Seismic Repair of Reinforced Concrete Bridge Columns

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Rapid Seismic Repair of Reinforced Concrete Bridge Columns

Author(s): Ruo-Yang Wu and Chris P. Pantelides

Publication: Structural Journal

Volume: 114

Issue: 5

Appears on pages(s): 1339-1350

Keywords: bridge; earthquake; fiber-reinforced polymer composites; finite element analysis; plastic hinge relocation; repair; resilience; seismic

DOI: 10.14359/51700789

Date: 9/1/2017

Abstract:
Experimental results are presented regarding the seismic repair of reinforced concrete bridge columns using a carbon fiber-reinforced polymer (CFRP) shell and epoxy-anchored headed steel bars. The CFRP shell, consisting of unidirectional laminates in the hoop and vertical direction, encloses the headed bars and is filled with non-shrink concrete to relocate the column plastic hinge. Two columns designed to current standards—one in a cap beam-to-column connection and the other in a footing-to-column connection—were damaged under cyclic forces. Damage included longitudinal bar fracture and buckling across multiple spiral hoops; concrete damage in the plastic hinge region included cracking and spalling of the column core concrete. Finite element analysis was used to design the CFRP shell and the headed bars were designed for the increased flexural demand on the repaired section. The seismic repair was rapid, required minimal intervention, and successfully relocated the plastic hinge and restored strength and displacement capacity.

Related References:

1. Marsh, M. L.; Buckle, I.; and Kavazanjian, E., “LRFD Seismic Analysis and Design of Bridges Reference Manual,” Report No. FHWA NHI-15-004, Federal Highway Administration, U.S. Department of Transportation, Washington, DC, 2014, 608 pp.

2. AASHTO, AASHTO Guide Specifications for LRFD Seismic Bridge Design, second edition, American Association of State Highway and Transportation Officials, Washington, DC, 2011, 331 pp.

3. Chai, Y.; Priestley, M.; and Seible, F., “Seismic Retrofit of Circular Bridge Columns for Enhanced Flexural Performance,” ACI Structural Journal, V. 88, No. 5, Sept.-Oct. 1991, pp. 572-584.

4. He, R.; Yang, Y.; and Sneed, L. H., “Seismic Repair of Reinforced Concrete Bridge Columns: Review of Research Findings,” Journal of Bridge Engineering, ASCE, V. 20, No. 12, 2015, 04015015 doi: 10.1061/(ASCE)BE.1943-5592.0000760

5. Kitada, T., “Ultimate Strength and Ductility of State-of-the-Art Concrete-Filled Steel Bridge Piers in Japan,” Engineering Structures, V. 20, No. 4-6, 1998, pp. 347-354. doi: 10.1016/S0141-0296(97)00026-6

6. Iacobucci, R. D.; Sheikh, S. A.; and Bayrak, O., “Retrofit of Square Concrete Columns with Carbon Fiber-Reinforced Polymer for Seismic Resistance,” ACI Structural Journal, V. 100, No. 6, Nov.-Dec. 2003, pp. 785-794.

7. Rodriguez, M., and Park, R., “Seismic Load Tests of Reinforced Concrete Columns Strengthened by Jacketing,” ACI Structural Journal, V. 91, No. 2, Mar.-Apr. 1994, pp. 150-159.

8. Lehman, D. E.; Gookin, S. E.; Nacamuli, A. M.; and Moehle, J. P., “Repair of Earthquake-Damaged Bridge Columns,” ACI Structural Journal, V. 98, No. 2, Mar.-Apr. 2001, pp. 233-238.

9. Saadatmanesh, H.; Ehsani, M. R.; and Jin, L., “Repair of Earthquake-Damaged RC Columns with FRP Wraps,” ACI Structural Journal, V. 94, No. 2, Mar.-Apr. 1997, pp. 206-215.

10. Kumar, P., and Mosalam, K. M., “Shaking Table Evaluation of Reinforced Concrete Bridge Columns Repaired Using Fiber-Reinforced Polymer Jackets,” Journal of Bridge Engineering, ASCE, V. 20, No. 12, 2015, p. 04015025 doi: 10.1061/(ASCE)BE.1943-5592.0000780

11. Saiidi, M. S., and Cheng, Z., “Effectiveness of Composites in Earthquake Damage Repair of Reinforced Concrete Flared Columns,” Journal of Composites for Construction, ASCE, V. 8, No. 4, 2004, pp. 306-314. doi: 10.1061/(ASCE)1090-0268(2004)8:4(306)

12. Vosooghi, A., and Saiidi, M. S., “Design Guidelines for Rapid Repair of Earthquake-Damaged Circular RC Bridge Columns Using CFRP,” Journal of Bridge Engineering, ASCE, V. 18, No. 9, 2013, pp. 827-836. doi: 10.1061/(ASCE)BE.1943-5592.0000426

13. Gergely, I.; Pantelides, C. P.; and Reaveley, L. D., “Shear Strengthening of R/C T-Joints Using CFRP Composites,” Journal of Composites for Construction, ASCE, V. 4, No. 2, 2000, pp. 56-64. doi: 10.1061/(ASCE)1090-0268(2000)4:2(56)

14. Pantelides, C. P.; Gergely, J.; Reaveley, L.; and Volnyy, V., “Retrofit of RC Bridge Pier with CFRP Advanced Composites,” Journal of Structural Engineering, ASCE, V. 125, No. 10, 1999, pp. 1094-1099. doi: 10.1061/(ASCE)0733-9445(1999)125:10(1094)

15. Gergely, I.; Pantelides, C. P.; Nuismer, R.; and Reaveley, L., “Bridge Pier Retrofit Using Fiber-Reinforced Plastic Composites,” Journal of Composites for Construction, ASCE, V. 2, No. 4, 1998, pp. 165-174. doi: 10.1061/(ASCE)1090-0268(1998)2:4(165)

16. Pantelides, C.; Duffin, J.; and Reaveley, L., “Seismic Strengthening of Reinforced-Concrete Multicolumn Bridge Piers,” Earthquake Spectra, V. 23, No. 3, 2007, pp. 635-664. doi: 10.1193/1.2757194

17. He, R.; Sneed, L. H.; and Belarbi, A., “Rapid Repair of Severely Damaged RC Columns with Different Damage Conditions: An Experimental Study,” International Journal of Concrete Structures and Materials, V. 7, No. 1, 2013, pp. 35-50. doi: 10.1007/s40069-013-0030-7

18. Jiang, S. F.; Zeng, X.; Shen, S.; and Xu, X., “Experimental Studies on the Seismic Behavior of Earthquake-Damaged Circular Bridge Columns Repaired by Using Combination of Near-Surface-Mounted BFRP Bars with External BFRP Sheets Jacketing,” Engineering Structures, V. 106, Jan. 2016, pp. 317-331. doi: 10.1016/j.engstruct.2015.10.037

19. Yang, Y.; Sneed, L. H.; Morgan, A.; Saiidi, M. S.; and Belarbi, A., “Repair of RC Bridge Columns with Interlocking Spirals and Fractured Longitudinal Bars–An Experimental Study,” Construction and Building Materials, V. 78, 2015, pp. 405-420. doi: 10.1016/j.conbuildmat.2015.01.010

20. Fakharifar, M.; Chen, G.; Sneed, L.; and Dalvand, A., “Seismic Performance of Post-Mainshock FRP/steel Repaired RC Bridge Columns Subjected to Aftershocks,” Composites. Part B, Engineering, V. 72, 2015, pp. 183-198. doi: 10.1016/j.compositesb.2014.12.010

21. Fakharifar, M.; Chen, G.; Wu, C.; Shamsabadi, A.; Elgawady, M. A.; and Dalvand, A., “Rapid Repair of Earthquake-Damaged RC Columns with Prestressed Steel Jackets,” Journal of Bridge Engineering, ASCE, V. 21, No. 4, 2016, p. 04015075 doi: 10.1061/(ASCE)BE.1943-5592.0000840

22. Chen, Q., and Andrawes, B., “Experimentally Validated Modeling of Concrete Actively Confined Using SMA Reinforcement,” 10th National Conference in Earthquake Engineering, Anchorage, AK, 2014, 10 pp.

23. Shin, M., and Andrawes, B., “Emergency Repair of Severely Damaged Reinforced Concrete Columns Using Active Confinement with Shape Memory Alloys,” Smart Materials and Structures, V. 20, No. 6, 2011, p. 065018 doi: 10.1088/0964-1726/20/6/065018

24. Billah, A. H. M. M., and Alam, M. S., “Seismic Performance Evaluation of Multi-Column Bridge Bents Retrofitted with Different Alternatives Using Incremental Dynamic Analysis,” Engineering Structures, V. 62-63, Mar. 2014, pp. 105-117. doi: 10.1016/j.engstruct.2014.01.005

25. Xiao, Y.; Wu, H.; and Martin, G., “Prefabricated Composite Jacketing of RC Columns for Enhanced Shear Strength,” Journal of Structural Engineering, ASCE, V. 125, No. 3, 1999, pp. 255-264. doi: 10.1061/(ASCE)0733-9445(1999)125:3(255)

26. Ameli, M. J.; Parks, J. E.; Brown, D. N.; and Pantelides, C. P., “Seismic Evaluation of Grouted Splice Sleeve Connections for Reinforced Precast Concrete Column-to-Cap Beam Joints in Accelerated Bridge Construction,” PCI Journal, V. 60, No. 2, 2015, pp. 80-103. doi: 10.15554/pcij.03012015.80.103

27. Ameli, M. J.; Brown, D.; Parks, J.; and Pantelides, C. P., “Seismic Column-to-Footing Connections Using Grouted Splice Sleeves,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 1021-1030. doi: 10.14359/51688755

28. Ameli, M. J., and Pantelides, C. P., “Seismic Analysis of Precast Bridge Columns Connected with Grouted Splice Sleeve Connectors,” Journal of Structural Engineering, ASCE, V. 143, No. 2, 2017, pp. 04016176. doi: 10.1061/(ASCE)ST.1943-541X.0001678

29. Parks, J.; Brown, D.; Ameli, M. J.; and Pantelides, C. P., “Seismic Repair of Severely Damaged Precast Reinforced Concrete Bridge Columns Connected with Grouted Splice Sleeves,” ACI Structural Journal, V. 113, No. 3, May-June 2016, pp. 615-626. doi: 10.14359/51688756

30. Cheng, C. T.; Yang, J. C.; Yeh, Y. K.; and Chen, S. E., “Seismic Performance of Repaired Hollow-Bridge Piers,” Construction and Building Materials, V. 17, No. 5, 2003, pp. 339-351. doi: 10.1016/S0950-0618(02)00119-8

31. Kaya, A.; Dawood, M.; and Gencturk, B., “Repair of Corroded and Buckled Short Steel Columns Using Concrete-Filled GFRP Jackets,” Construction and Building Materials, V. 94, 2015, pp. 20-27. doi: 10.1016/j.conbuildmat.2015.06.040

32. Yang, Y.; Sneed, L.; Saiidi, M. S.; Belarbi, A.; Ehsani, M.; and He, R., “Emergency Repair of an RC Bridge Column with Fractured Bars Using Externally Bonded Prefabricated Thin CFRP Laminates and CFRP Strips,” Composite Structures, V. 133, 2015, pp. 727-738. doi: 10.1016/j.compstruct.2015.07.045

33. He, R.; Grelle, S.; Sneed, L. H.; and Belarbi, A., “Rapid Repair of a Severely Damaged RC Column Having Fractured Bars Using Externally Bonded CFRP,” Composite Structures, V. 101, 2013, pp. 225-242. doi: 10.1016/j.compstruct.2013.02.012

34. Caltrans, Seismic Design Criteria Version 1.7, Division of Engineering Services, Sacramento, CA, 2013.

35. ASTM C39/C39M-16b, “Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2016, 7 pp.

36. ASTM A370-16, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2016, 49 pp.

37. Vosooghi, A., and Saiidi, M., “Post-Earthquake Evaluation and Emergency Repair of Damaged RC Bridge Columns Using CFRP Materials,” Report No. CCEER-10-05, University of Nevada, Reno, Reno, NV, 2010.

38. Panagiotakos, T., and Fardis, M., “Deformation of Reinforced Concrete Memebers at Yielding and Ultimate,” ACI Structural Journal, V. 98, No. 2, Mar.-Apr. 2001, pp. 135-147.

39. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

40. SIMULIA, ABAQUS Analysis User’s Manual, Abaqus 6.12, SIMULIA, The Dassault Systèmes, Realistic Simulation, 2012.

41. ASTM D3039/D3039M-14. “Standard Test Method for Tensile Properties of Polymer Matrix Composite Materials,” ASTM International, West Conshohocken, PA, 2014, 13 pp.

42. Lee, J., and Fenves, G., “Plastic-Damage Model for Cyclic Loading of Concrete Structures,” Journal of Engineering Mechanics, ASCE, V. 124, No. 8, 1998, pp. 892-900. doi: 10.1061/(ASCE)0733-9399(1998)124:8(892)

43. CEB-FIB, “CEB-FIP Model Code 1990,” Comitè Euro-International du Béton and Fédération International de la Précontrainte (CEB-FIP), Thomas Telford Ltd., London, UK, 1993.

44. Jankowiak, T., and Lodygowski, T., “Identification of Parameters of Concrete Damage Plasticity Constitutive Model,” Foundations of Civil and Environmental Engineering, V. 6, 2005, pp. 53-69.

45. Hillerborg, A., “The Theoretical Basis of a Method to Determine the Fracture Energy GF of Concrete,” Materials and Structures, V. 18, No. 4, 1985, pp. 291-296. doi: 10.1007/BF02472919

46. CEB-FIB, “CEB-FIP Model Code 2010,” Comitè Euro-International du Béton and Fédération International de la Précontrainte (CEB-FIP), Thomas Telford Ltd., London, UK, 2010.

47. Sideris, P., “Seismic Analysis and Design Of Precast Concrete Segmental Bridges,” PhD dissertation, Department of Civil, Structural and Environmental Engineering, State University of New York at Buffalo, Buffalo, NY, 2012.

48. ACI Committee 440, “Guide for the Design and Construction of Externally Bonded FRP Systems for Strengthening Existing Structures (ACI 440.2R-08),” American Concrete Institute, Farmington Hills, MI, 2008, 76 pp.

49. ACI Committee 374, “Guide for Testing Reinforced Concrete Structural Elements under Slowly Applied Simulated Seismic Loads (ACI 374.2R-13),” American Concrete Institute, Farmington Hills, MI, 2013, 18 pp.

50. ASCE/SEI 41-13, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2013.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer