Title: Shallow Embedded Anchors

Author(s): Werner Fuchs and Jan Hofmann

Publication: Concrete International

Volume: 39

Issue: 2

Appears on pages(s): 45-53

Keywords: nonstructural, cover, redundant, reinforcement

DOI: 10.14359/51689626

Date: 2/1/2017

Abstract:
Although ACI 318-14 provides design requirements for anchors in concrete, it does not apply to specialty inserts used for anchoring nonstructural elements. Background information is provided on the ACI 318 design procedure, shallow anchors and related parameters are discussed, and modification factors are proposed for ACI 318 design values.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

2. “AC446: Acceptance Criteria for Headed Cast-in Specialty Inserts in Concrete,” International Code Council Evaluation Service, Inc. (ICC-ES), 2015, 13 pp.

3. “AC193: Acceptance Criteria for Mechanical Anchors in Concrete Elements,” International Code Council Evaluation Service, Inc. (ICC-ES), 2015, 45 pp.

4. ACI Committee 355, “Qualification of Post-Installed Mechanical Anchors in Concrete and Commentary (ACI 355.2-07),” American Concrete Institute, Farmington Hills, MI, 2007, 35 pp.

5. “EN 1992-4 Eurocode 2: Design of Concrete Structures—Part 4: Design of Fastenings for Use in Concrete,” Comité Européen de Normalisation (CEN), Brussels, Belgium, 2017.

6. Neville, A.M., Properties of Concrete, fifth edition, Trans-Atlantic Publications, Inc., Philadelphia, PA, 2012, 846 pp.

7. Kreijger, P.C., “The Skin of Concrete—Composition and Properties,” Materials and Structures, V. 17, No. 4, July 1984, pp. 275- 283.

8. Sourwerbren, C., Betontechnologie (Concrete Technology), Vereniging Nederlandse Cementindustrie, ‘s-Hertogenbosch, The Netherlands, 1991. (in Dutch)

9. Bretschneider, N., “Inverse Analyse zur Ermittlung der bruchmechanischen Eigenschaften entfestigender und verfestigender zementgebundener Werkstoffe (Inverse Analysis for the Determination of the Fracture Mechanical Characteristics of Chemically Softening and Hardening Cementiously Bonded Materials),” PhD thesis, University of Dresden, Dresden, Germany, 2011, 191 pp. (in German)

10. van Mier, J.G.M., Concrete Fracture: A Multiscale Approach, CRC Press, Boca Raton, FL, 2013, 379 pp.

11. Eligehausen, R.; Mallée, R.; and Silva, J.F., Anchorage in Concrete Construction, first edition, Ernst & Sohn, 2006, 391 pp.

12. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

13. Fuchs, W.; Eligehausen, R.; and Breen, J., “Concrete Capacity Design (CCD) Approach for Fastening to Concrete,” ACI Structural Journal, V. 92, No. 1, Jan.-Feb. 1995, pp. 73-93. Also discussion, ACI Structural Journal, V. 92, No. 6, Nov.-Dec., pp. 787-802.

14. “CEN/TR 17079: Design of Fastenings for Use in Concrete – Redundant Non-structural Systems,” Comité Européen de Normalisation (CEN), Brussels, Belgium, 2017.

15. Fuchs, W., “Tragverhalten von Befestigungen Verankert in der Biegezugzone von stark bewehrten Betonbalken (Load-bearing Behavior of Anchorages in the Bending Tensile Area of Heavy Reinforced Concrete Beams),” Report No. 10/8-86/12, Institut für Werkstoffe im Bauwesen, Universität Stuttgart, Stuttgart, Germany, Dec. 1985. (in German)

16. Hofmann, J., and Kaupp, A., “Behavior of Fasteners with an Embedment Depth of Smaller than 25 mm,” Proceedings of Second International Symposium on Connections between Steel and Concrete, Stuttgart, Germany, R. Eligehausen, W. Fuchs, P. Grosser, and G. Genesio, eds., 2007, pp. 453-460.

17. Olsen, J.; Lamanna, A.J.; and Pregartner, T., “Basis for Design of Screw Anchors in Concrete,” ACI Structural Journal, V. 109, No. 4, July-Aug. 2012, pp. 559-568.

18. Appl, J., “Tragverhalten von Verbunddübeln unter Zugbelastung (Load-bearing Behavior of Adhesive Anchors under Tension),” PhD thesis, University of Stuttgart, Stuttgart, Germany, 2009, 276 pp. (in German)