Optimum Design of Reactive Powder Concrete Mixture Proportion Based on Artificial Neural and Harmony Search Algorithm

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Optimum Design of Reactive Powder Concrete Mixture Proportion Based on Artificial Neural and Harmony Search Algorithm

Author(s): Tao Ji, Yu Yang, Mao-yuan Fu, Bao-chun Chen, and Hwai-Chung Wu

Publication: Materials Journal

Volume: 114

Issue: 1

Appears on pages(s): 41-47

Keywords: artificial neural network (ANN); cost; curing regime; harmony search (HS) algorithm; mixture proportion design; reactive powder concrete

DOI: 10.14359/51689476

Date: 1/1/2017

Abstract:
An optimum mixture proportion design method of reactive powder concrete (RPC) based on an artificial neural network (ANN) and harmony search (HS) algorithm was developed. ANNs were adopted to establish the relationship between design parameters (water-binder ratio, silica fume content, sand-binder ratio, and steel fiber content) and properties (compressive strength under standard curing and autoclaved curing, splitting tensile strength under autoclaved curing, and slump) of RPC, and the HS algorithm was used to design and optimize RPC mixture proportions with the objective criterion of minimum cost while meeting all property requirements. The proposed method can consider the influence of curing regimes, and its reliability was verified by experiment data.

Related References:

1. Richard, P., and Cheyrezy, M., “Composition of Reactive Powder Concretes,” Cement and Concrete Research, V. 25, No. 7, 1995, pp. 1501-1511. doi: 10.1016/0008-8846(95)00144-2

2. Bonneau, O.; Poulin, C.; Dugat, J.; Richard, P.; and Aïtcin, P. C., “Reactive Powder Concretes: From Theory to Practice,” Concrete International, V. 18, No. 4, Apr. 1996, pp. 47-49.

3. Yunsheng, Z.; Wei, S.; Sifeng, L.; Chujie, J.; and Jianzhong, L., “Preparation of C200 Green Reactive Powder Concrete and Its Static-Dynamic Behaviors,” Cement and Concrete Composites, V. 30, No. 9, 2008, pp. 831-838. doi: 10.1016/j.cemconcomp.2008.06.008

4. Yazıcı, H.; Deniz, E.; and Baradan, B., “The Effect of Autoclave Pressure, Temperature and Duration Time on Mechanical Properties of Reactive Powder Concrete,” Construction and Building Materials, V. 42, 2013, pp. 53-63. doi: 10.1016/j.conbuildmat.2013.01.003

5. Yazıcı, H.; Yardımcı, M. Y.; Aydın, S.; and Karabulut, A. Ş., “Mechanical Properties of Reactive Powder Concrete Containing Mineral Admixtures under Different Curing Regimes,” Construction and Building Materials, V. 23, No. 3, 2009, pp. 1223-1231. doi: 10.1016/j.conbuildmat.2008.08.003

6. Aïtcin, P. C., “Cements of Yesterday and Today: Concrete of Tomorrow,” Cement and Concrete Research, V. 30, No. 9, 2000, pp. 1349-1359. doi: 10.1016/S0008-8846(00)00365-3

7. Shi, C. J.; Wu, Z. M.; Xiao, J. F.; Wang, D. H.; Huang, Z. Y.; and Fang, Z., “A Review on Ultra High Performance Concrete: Part I. Raw Materials and Mixture Design,” Construction and Building Materials, V. 101, 2015, pp. 741-751. doi: 10.1016/j.conbuildmat.2015.10.088

8. Zhao, Q. X.; Liu, Z. Y.; and Hao, S. W., “Mixture Proportion Design of RPC Based on Orthogonal Theory,” Bulletin of the Chinese Ceramic Society, V. 29, No. 1, 2010, pp. 193-197.

9. Cui, G.; Liu, J. Z.; Yao, T.; and Lin, W., “Mix Proportion Design of Reactive Powder Concrete Based on Dinger-Funk Equation,” Journal of Southeast University, V. 40, No. 2, 2010, pp. 15-19. (Natural Science Edition)

10. Yeh, I. C., “Design of High-Performance Concrete Mixture Using Neural Networks and Nonlinear Programming,” Journal of Computing in Civil Engineering, ASCE, V. 13, No. 1, 1999, pp. 36-42. doi: 10.1061/(ASCE)0887-3801(1999)13:1(36)

11. Ji, T.; Lin, T. W.; and Lin, X. J., “Prediction Method of Concrete Compressive Strength Based on Artificial Neural Network,” Journal of Building Materials, V. 8, No. 6, 2005, pp. 677-681.

12. Yang, D. S.; Park, S. K.; and Lee, J. H., “A Prediction on Mix Proportion Factor and Strength of Concrete Using Neural Network,” KSCE Journal of Civil Engineering, V. 7, No. 5, 2003, pp. 525-536. doi: 10.1007/BF02838318

13. Ji, T.; Lin, T.; and Lin, X., “A Concrete Mix Proportion Design Algorithm Based on Artificial Neural Networks,” Cement and Concrete Research, V. 36, No. 7, 2006, pp. 1399-1408. doi: 10.1016/j.cemconres.2006.01.009

14. Lim, C. H.; Yoon, Y. S.; and Kim, J. H., “Genetic Algorithm in Mix Proportioning of High-Performance Concrete,” Cement and Concrete Research, V. 34, No. 3, 2004, pp. 409-420. doi: 10.1016/j.cemconres.2003.08.018

15. Chang, C. Y.; Huang, R.; Lee, P. C.; and Weng, T. L., “Application of a Weighted Grey-Taguchi Method for Optimizing Recycled Aggregate Concrete Mixtures,” Cement and Concrete Composites, V. 33, No. 10, 2011, pp. 1038-1049. doi: 10.1016/j.cemconcomp.2011.06.005

16. Mohammed, B. S.; Fang, O. C.; Hossain, K. M. A.; and Lachemi, M., “Mix Proportioning of Concrete Containing Paper Mill Residuals Using Response Surface Methodology,” Construction and Building Materials, V. 35, 2012, pp. 63-68. doi: 10.1016/j.conbuildmat.2012.02.050

17. Topçu, İ. B., and Sarıdemir, M., “Prediction of Compressive Strength of Concrete Containing Fly Ash Using Artificial Neural Networks and Fuzzy Logic,” Computational Materials Science, V. 41, No. 3, 2008, pp. 305-311. doi: 10.1016/j.commatsci.2007.04.009

18. Mahdavi, M.; Fesanghary, M.; and Damangir, E., “An Improved Harmony Search Algorithm for Solving Optimization Problems,” Applied Mathematics and Computation, V. 188, No. 2, 2007, pp. 1567-1579. doi: 10.1016/j.amc.2006.11.033

19. Lee, J. H., and Yoon, Y. S., “Modified Harmony Search Algorithm and Neural Networks for Concrete Mix Proportion Design,” Journal of Computing in Civil Engineering, ASCE, V. 23, No. 1, 2009, pp. 57-61. doi: 10.1061/(ASCE)0887-3801(2009)23:1(57)

20. Lee, J. H.; Yoon, Y. S.; and Kim, J. H., “A New Heuristic Algorithm for Mix Design of High-Performance Concrete,” KSCE Journal of Civil Engineering, V. 16, No. 6, 2012, pp. 974-979. doi: 10.1007/s12205-012-1011-0

21. Ji, T.; Zhuang, Y. Z.; Chen, B. C.; and Huang, Z. B., “Behavioral Prediction of Reactive Powder Concrete Based on Artificial Neural Network,” Advanced Materials Research, V. 168, 2011, pp. 1030-1033.

22. Aïtcin, P. C., High-Performance Concrete, CRC Press, Boca Raton, FL, 2011, 624 pp.

23. Geem, Z. W.; Kim, J. H.; and Loganathan, G. V., “A New Heuristic Optimization Algorithm: Harmony Search,” Simulation, V. 76, No. 2, 2001, pp. 60-68. doi: 10.1177/003754970107600201

24. GB/T 50080-2002, “Standard for Test Method of Performance on Ordinary Fresh Concrete,” China Building Industry Press, Beijing, China, 2003.

25. GB/T 50081-2002, “Standard for Test Method of Mechanical Properties on Ordinary Concrete,” China Building Industry Press, Beijing, China, 2003.