Title: 
            Concrete Q&A: Concrete Slab Curling Over Vapor Retarders
        
        
            Author(s): 
            
        
        
            
                Publication: 
                Concrete International
            
            
                Volume: 
                38
            
            
                Issue: 
                9
            
            
                Appears on pages(s): 
                75-76
            
            
                Keywords: 
                
            
            
                DOI: 
                
            
        
        
            Date: 
            9/1/2016
        
        
            Abstract:
            Q. We have always been told that concrete slabs placed directly on a vapor retarder curl more than slabs cast directly on a prepared base. However, we recently measured a slab that we know had a vapor barrier only in limited areas. The portions cast over the vapor retarder had less curling than those cast directly on the base. What is the current industry understanding of this issue?