Time-Dependent Diffusion Modeling of Concrete with Cement Containing Limestone and Inorganic Process Additions

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Time-Dependent Diffusion Modeling of Concrete with Cement Containing Limestone and Inorganic Process Additions

Author(s): Mustapha A. Ibrahim and Mohsen A. Issa

Publication: Materials Journal

Volume: 113

Issue: 6

Appears on pages(s): 837-848

Keywords: chloride diffusion; inorganic process additions; insoluble residue; modeling; supplementary cementitious materials; surface chloride concentration

DOI: 10.14359/51689243

Date: 11/1/2016

Abstract:
Replacing cement with limestone and inorganic process additions (IPAs) and increasing the insoluble residue (IR) can aid in reducing the CO2 emission. This paper investigates the effect of adding IPA and increasing IR on the diffusivity characteristics of concrete. Also, the effect of replacing cement with supplementary cementitious materials while batching them with two sand types was demonstrated. To show the effect of these materials, the chloride diffusion test was conducted on 26 concrete mixtures with different proportions that were salt ponded for 90, 180, and 360 days. The IPA addition and increase in IR did not show any notable influence on concrete diffusivity. On the basis of the experimental results, a diffusion model with time-dependent surface chloride and diffusion coefficient was developed. The proposed model was compared with existing service-life prediction software and models, and showed promising results, while the current equations adopted by the software were very conservative.

Related References:

1. Poulsen, E., and Mejlbro, L., Diffusion of Chloride in Concrete: Theory and Application, Modern Concrete Technology, first edition, CRC Press, Bacon Raton, FL, 2006, 480 pp.

2. Bentz, D. P.; Garboczi, E. J.; Haecker, C. J.; and Jensen, O. M., “Effects of Cement Particle Size Distribution on Performance Properties of Portland Cement-Based Materials,” Cement and Concrete Research, V. 29, No. 10, 1999, pp. 1663-1671. doi: 10.1016/S0008-8846(99)00163-5

3. Oh, B. H., and Jang, S. Y., “Effects of Material and Environmental Parameters on Chloride Penetration Profiles in Concrete Structures,” Cement and Concrete Research, V. 37, No. 1, 2007, pp. 47-53. doi: 10.1016/j.cemconres.2006.09.005

4. Yang, C. C., “A Comparison of Transport Properties for Concrete Using the Ponding Test and the Accelerated Chloride Migration Test,” Materials and Structures, V. 38, No. 3, 2005, pp. 313-320. doi: 10.1007/BF02479296

5. ASTM C150/C150M, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2011, 9 pp.

6. Thomas, M. D. A.; Shehata, M. H.; Shashiprakash, S. G.; Hopkins, D. S.; and Cail, K., “Use of Ternary Cementitious Systems Containing Silica Fume and Fly Ash in Concrete,” Cement and Concrete Research, V. 29, No. 8, 1999, pp. 1207-1214. doi: 10.1016/S0008-8846(99)00096-4

7. Burris, L. E., and Riding, K. A., “Diffusivity of Binary and Ternary Concrete Mixture Blends,” ACI Materials Journal, V. 111, No. 4, July-Aug. 2014, pp. 373-382. doi: 10.14359/51686826

8. ASTM C219/C219M, “Standard Terminology Relating to Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2014, 4 pp.

9. Taylor, P. C., “Specifications and Protocols for Acceptance Tests on Processing Additions in Cement Manufacturing,” NCHRP Report 607, Transportation Research Board, Washington, DC, 2007, 87 pp.

10. Dhir, R. K., “Additional Materials and Allowable Cements in Cement,” Euro-Cements Impact of ENV 196 on Concrete Construction, R. K. Dhir and M. R. Jones, ed., University of Dundee, Dundee, Scotland, E&FN Spon, 1994, pp. 51-63.

11. Gebhardt, R. F., “Survey of North American Portland Cements: 1994,” Cement, Concrete and Aggregates, V. 17, No. 2, 1995, pp. 145-189. doi: 10.1520/CCA10140J

12. Tang, L., and Nilsson, L. O., “Chloride Diffusivity in High Strength Concrete at Different Ages,” Nordic Concrete Research Publication, V. 11, 1992, pp. 162-171.

13. Maage, M.; Poulsen, E.; Vennesland, O.; and Carlsen, J. E., “Service Life Model for Concrete Structures Exposed to Marine Environment,” LIGHTCON Report No. 2.4, STF70 A94082 SINTEF, Trondheim, Norway, 1995.

14. Frederiksen, J. M.; Nilsson, L. O.; Poulsen, E.; Sandberg, P.; Tang, L.; and Andersen, A., “HETEK, A System for Estimation of Chloride Ingress into Concrete, Theoretical Background,” Report No. 83, The Danish Road Directorate, 1997, 107 pp.

15. Takewaka, K., and Mastumoto, S., “Quality and Cover Thickness of Concrete based on the Estimation of Chloride Penetration in Marine Environments,” Concrete in Marine Environment, SP-109, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1988, pp. 381-400.

16. Mustafa, M. A., and Yusof, K. M., “Atmospheric Chloride Penetration into Concrete in Semi-Tropical Marine Environment,” Cement and Concrete Research, V. 24, No. 4, 1994, pp. 661-670. doi: 10.1016/0008-8846(94)90190-2

17. Swamy, R. N.; Suryavanshi, A. K.; and Tanikawa, S., “Protective Ability of an Acrylic-Based Surface Coating System against Chloride and Carbonation Penetration into the Concrete,” ACI Materials Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 101-112.

18. Costa, A., and Appleton, J., “Chloride Penetration into Concrete in Marine Environment—Part 1: Main Parameters Affecting Chloride Penetration,” Materials and Structures, V. 32, No. 4, May 1999, pp. 252-259. doi: 10.1007/BF02479594

19. Uji, K.; Matsuoka, Y.; and Maruya, T., “Formulation of an Equation for Surface Chloride Content of Concrete Due to Permeation of Chloride,” Corrosion of Reinforcement in Concrete, C. L. Page, K. W. J. Treadway, and P. B. Bamforth, eds., Elsevier Science, Barking, UK, 1990, pp. 258-267.

20. Purvis, R. L.; Babaei, K.; Clear, K. C.; and Markow, M. J., Life-Cycle Cost Analysis for Protection and Rehabilitation of Concrete Bridges Relative to Reinforcement Corrosion, Strategic Highway Research Program, SHRP-S-377, National Research Council, Washington, DC, 1994, 289 pp.

21. Kato, E.; Kato, Y.; and Uomoto, T., “Development of Simulation Model of Chloride Ion Transportation in Cracked Concrete,” Journal of Advanced Concrete Technology, V. 3, No. 1, 2005, pp. 85-94. doi: 10.3151/jact.3.85

22. Shin, C. B., and Kim, E. K., “Modeling of Chloride Ion Ingress in Coastal Concrete,” Cement and Concrete Research, V. 32, No. 5, 2002, pp. 757-762. doi: 10.1016/S0008-8846(01)00756-6

23. ASTM C192/C192M-12, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2012, 8 pp.

24. ASTM C143/C143M-12, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2012, 4 pp.

25. ASTM C231/C231M-10, “Standard Test Method for Air Content of Freshly Mixed Concrete by the Pressure Method,” ASTM International, West Conshohocken, PA, 2010, 10 pp.

26. ASTM C1543-10a, “Standard Test Method for Determining the Penetration of Chloride Ion into Concrete by Ponding,” ASTM International, West Conshohocken, PA, 2010, 4 pp.

27. ASTM C1152/1152M-04, “Standard Test Method for Acid-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2004, 4 pp.

28. Suryavanshi, A. K.; Swamy, R. N.; and McHugh, S., “Chloride Penetration into Reinforced Concrete Slabs,” Canadian Journal of Civil Engineering, V. 25, No. 1, 1998, pp. 87-95. doi: 10.1139/l97-046

29. ASTM C1556/1556M-11, “Standard Test Method for Determining the Apparent Chloride Diffusion Coefficient of Cementitious Mixtures by Bulk Diffusion,” ASTM International, West Conshohocken, PA, 2011, 7 pp.

30. Meira, G. R.; Andrade, C.; Alonso, C.; Borba, J. C. Jr.; and Padilha, M. Jr., “Durability of Concrete Structures in Marine Atmosphere Zones—The Use of Chloride Deposition Rate on the Wet Candle as an Environmental Indicator,” Cement and Concrete Composites, V. 32, No. 6, 2010, pp. 427-435. doi: 10.1016/j.cemconcomp.2010.03.002

31. Swamy, R. N., and Laiw, J. C., “Effectiveness of Supplementary Cementing Materials in Controlling Chloride Penetration into Concrete,” Fly Ash, Silica Fume, Slag, and Natural Pozzolans in Concrete, Proceedings of the Fifth International Conference, SP-153, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 1995, pp. 657-674.

32. Crank, J., The Mathematics of Diffusion, second edition, Clarendon Press, Oxford, UK, 1975, 424 pp.

33. Mendham, J.; Denney, R. C.; Barnes, J. D.; and Thomas, M. J. K., Vogel’s Textbook of Quantitative Chemical Analysis, sixth edition, Prentice Hall, Singapore, 2000, 836 pp.

34. Stanish, K., and Thomas, M., “The Use of Bulk Diffusion Tests to Establish Time-Dependent Concrete Chloride Diffusion Coefficients,” Cement and Concrete Research, V. 33, No. 1, 2003, pp. 55-62. doi: 10.1016/S0008-8846(02)00925-0

35. ACI Committee 365, “Service-Life Prediction—State-of-the-Art Report (ACI 365.1R-00),” American Concrete Institute, Farmington Hills, MI, 2000, 44 pp.

36. Zhou, S., “Modeling Chloride Diffusion in Concrete with Linear Increase of Surface Chloride,” ACI Materials Journal, V. 111, No. 5, Sept.-Oct. 2014, pp. 483-490. doi: 10.14359/51686989

37. Bentz, E. C., and Thomas, M. D. A., “Life-365 Service Life Prediction Model, Version 2.2.1,” 2014, http://www.life-365.org/. (last accessed Jan. 15, 2014)

38. Riding, K. A.; Thomas, M. D. A.; and Folliard, K. J., “Apparent Diffusivity Model for Concrete Containing Supplementary Cementitious Materials,” ACI Materials Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 705-714.

39. Daigle, L.; Lounis, Z.; Cusson, D.; and Smithson, L. D., “Numerical Prediction of Early-Age Cracking and Corrosion in High Performance Concrete Bridges-Case Study,” Innovations in Bridge Engineering Session, The 2004 Annual Conference of the Transportation Association of Canada, Quebec City, QC, Canada, 2004, 20 pp.

40. Issa, M. A., and Khalil, A. A., “Diffusivity and Permeability of High-Performance Concrete (HPC) for Bridge Decks,” PCI Journal, V. 55, No. 2, 2010, pp. 82-95. doi: 10.15554/pcij.03012010.82.95

41. Hornain, H.; Marchand, J.; Duhot, V.; and Moranville-Regourd, M., “Diffusion of Chloride Ions in Limestone Filler Blended Cement Pastes and Mortars,” Cement and Concrete Research, V. 25, No. 8, 1995, pp. 1667-1678. doi: 10.1016/0008-8846(95)00163-8

42. Akrout, K.; Ltifi, M.; and Ouezdou, M. B., “Chloride Diffusion in Mortars-Effect of the Use of Limestone Sand; Part II: Immersion Test,” International Journal of Concrete Structures and Materials, V. 4, No. 2, 2010, pp. 109-112. doi: 10.4334/IJCSM.2010.4.2.109

43. Siddique, R., and Khan, M. I., Supplementary Cementing Materials, first edition, Engineering Materials, Springer, Berlin, Germany, 2011, 287 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal