            Abstract:
            Ensuring adequate stability is critical in flowable and lean concrete prone to bleeding and segregation. This paper proposes a forced bleeding test method that can be used to determine the ability of fresh concrete to retain some of its mixing water under a pressure gradient across a drainage surface. The investigated concrete was proportioned with a water-cement ratio (w/c) of 0.55 to 0.65 with slump values varying between 70 and 240 mm (2.75 and 9.45 in.). The proposed forced bleeding test has an overhead pressure of 138 kPa (20 psi) with the pressure maintained for 1 minute. This short test duration and relatively low overhead pressure yielded better results than higher testing pressure gradients or longer test durations. Forced bleeding test results showed good correlations between the rate of forced bleeding at 1 minute and physical tests to evaluate stability. Physical tests included the determination of external bleeding for 2 hours, the measurement of coarse aggregate distribution along hardened concrete samples, as well as the variation in electrical conductivity along concrete sample height during the dormant period of cement hydration to evaluate homogeneity.
        
     
    
    
    
            Related References:
                
                        1. Kaplan, D., “de Larrard, F.; and Sedran. T., “Avoidance of Blockages in the Concrete Pumping Process,” ACI Materials Journal, V. 102, No. 3, May-June 2005, pp. 183-191.
                    
                        2. Chapdelaine, F., “Fundamental and Practice Study on Pumping Concrete,” PhD thesis, Université Laval, Quebec, QC, Canada, 2007, 126 pp. (in French)
                    
                        3. ASTM C232-87, “Standard Test Methods for Bleeding of Concrete,” ASTM International, West Conshohocken, PA, 1987, 4 pp.
                    
                        4. Swedish Standard, “Method for Measuring Water-Separation,” B5-33, 1965. (in Swedish)
                    
                        5. Josserand, L., and de Larrard, F., “A Method for Concrete Bleeding Measurement,” Materials and Structures, V. 37, No. 274, 2004, pp. 666-670. doi: 10.1617/14052
                    
                        6. Pavate, T. V.; Khayat, K. H.; and Jolicoeur, C., “In-Situ Conductivity Method for Monitoring Segregation, Bleeding, and Strength Development in Cement-Based Materials,” Sixth CANMET/ACI Conference on Superplasticizers and Other Chemical Admixtures in Concrete, SP-195, V. M. Malhotra, ed., American Concrete Institute, Farmington Hills, MI, 2000, pp. 535-547.
                    
                        7. Browne, R. D., and Bamforthe, P. B., “Tests of Establish Concrete Pumpability,” ACI Journal Proceedings, V. 74, No. 5, May 1977, pp. 193-207.
                    
                        8. Khayat, K. H.; Assaad, J.; and Daczko, J., “Comparison of Field-Oriented Test Methods to Assess Dynamic Stability of Self-Consolidating Concrete,” ACI Materials Journal, V. 101, No. 2, Mar.-Apr. 2004, pp. 168-176.
                    
                        9. Khayat, K. H.; Vanhove, Y.; Pavate, T. V.; and Jolicoeur, C., “Multi-Electrode Conductivity Method to Evaluate Static Stability of Flowable and Self-Consolidating Concrete,” ACI Materials Journal, V. 104, No. 4, July-Aug. 2007, pp. 424-433.
                    
                        10. Giaccio, G., and Giovambattista, A., “Bleeding: Evaluation of Its Effects on Concrete Behaviour,” Materials and Structures, V. 19, No. 4, 1986, pp. 265-271. doi: 10.1007/BF02472109
                    
                        11. Loh, C. K.; Tan, T. S.; Yong, T. S.; and Wee, T. H., “An Experimental Study on Bleeding and Channeling of Cement Paste and Mortar,” Advances in Cement Research, V. 10, No. 1, 1998, pp. 1-16. doi: 10.1680/adcr.1998.10.1.1