Bond of Substandard Laps in Reinforced Concrete Beams Retrofitted with Post-Tensioned Metal Straps

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Bond of Substandard Laps in Reinforced Concrete Beams Retrofitted with Post-Tensioned Metal Straps

Author(s): Yasser Helal, Reyes Garcia, Kypros Pilakoutas, Maurizio Guadagnini, and Iman Hajirasouliha

Publication: Structural Journal

Volume: 113

Issue: 6

Appears on pages(s): 1197-1208

Keywords: beams; bond strength; lap splices; post-tensioned metal strap confinement; reinforced concrete; retrofitting; splitting strength

DOI: 10.14359/51689021

Date: 11/1/2016

Abstract:
This paper investigates the bond-splitting performance of lapped steel bars in tension. Twelve reinforced concrete (RC) beams with substandard laps (lap length = 25 bar diameters) at midspan were tested in flexure. The variables examined include the bar diameter, concrete cover, and three different confinement conditions at midspan: 1) no confinement; 2) internal steel stirrups; and 3) external post-tensioned metal straps (PTMSs). The test results show that, in comparison to unconfined specimens, PTMS confinement enhances the bond strength of the lapped bars by up to 120%. Based on the results of this study, an innovative equation is proposed and validated to calculate the additional bond strength provided by PTMS confinement. The equation can be used for assessment and retrofit of substandard lapped bars in RC structures and should prove useful in practical retrofitting applications.

Related References:

1. Ahmad, S.; Khan, S.; Pilakoutas, K.; and Khan, Q., “Empirical Vulnerability Assessment of the Non-Engineered Reinforced Concrete Structures Using the Kashmir Earthquake Damage Data,” Bulletin of Earthquake Engineering, V. 13, No. 9, 2015, pp. 2611-2628. doi: 10.1007/s10518-015-9735-0

2. Lynn, A. C.; Moehle, J. P.; Mahin, S. A.; and Holmes, W. T., “Seismic Evaluation of Existing Reinforced Concrete Building Columns,” Earthquake Spectra, V. 12, No. 4, 1996, pp. 715-739. doi: 10.1193/1.1585907

3. Melek, M.; Wallace, J. W.; and Conte, J. P., “Experimental Assessment of Columns with Short Lap Splices Subjected to Cyclic Loads,” Pacific Earthquake Engineering Research Center, College of Engineering, University of California, Berkeley, Berkeley, CA, 2003, 176 pp.

4. Aboutaha, R. S.; Engelhardt, M. D.; Jirsa, J. O.; and Kreger, M. E., “Retrofit of Concrete Columns with Inadequate Lap Splices by the Use of Rectangular Steel Jackets,” Earthquake Spectra, V. 12, No. 4, 1996, pp. 693-714. doi: 10.1193/1.1585906

5. ElGawady, M.; Endeshaw, M.; McLean, D.; and Sack, R., “Retrofitting of Rectangular Columns with Deficient Lap Splices,” Journal of Composites for Construction, ASCE, V. 14, No. 1, 2010, pp. 22-35. doi: 10.1061/(ASCE)CC.1943-5614.0000047

6. Bousias, S.; Spathis, A. L.; and Fardis, M. N., “Seismic Retrofitting of Columns with Lap Spliced Smooth Bars through FRP or Concrete Jackets,” Journal of Earthquake Engineering, V. 11, No. 5, 2007, pp. 653-674. doi: 10.1080/13632460601125714

7. Karayannis, C. G.; Chalioris, C. E.; and Sirkelis, G. M., “Local Retrofit of Exterior RC Beam-Column Joints Using Thin RC Jackets—An Experimental Study,” Earthquake Engineering and Structural Dynamics, V. 37, No. 5, 2008, pp. 727-746. doi: 10.1002/eqe.783

8. Priestley, M. J. N., and Seible, F., “Design of Seismic Retrofit Measures for Concrete and Masonry Structures,” Construction & Building Materials, V. 9, No. 6, 1995, pp. 365-377. doi: 10.1016/0950-0618(95)00049-6

9. Saadatmanesh, H.; Ehsani, M. R.; and Jin, L., “Seismic Strengthening of Circular Bridge Pier Models with Fiber Composites,” ACI Structural Journal, V. 93, No. 6, Nov.-Dec. 1996, pp. 639-647.

10. Sause, R.; Harries, K. A.; Walkup, S. L.; Pessiki, S.; and Ricles, J. M., “Flexural Behavior of Concrete Columns Retrofitted with Carbon Fiber-Reinforced Polymer Jackets,” ACI Structural Journal, V. 101, No. 5, Sept.-Oct. 2004, pp. 708-716.

11. Breña, S. F., and Schlick, B. M., “Hysteretic Behavior of Bridge Columns with FRP-Jacketed Lap Splices Designed for Moderate Ductility Enhancement,” Journal of Composites for Construction, ASCE, V. 11, No. 6, 2007, pp. 565-574. doi: 10.1061/(ASCE)1090-0268(2007)11:6(565)

12. Harajli, M. H., “Seismic Behavior of RC Columns with Bond-Critical Regions: Criteria for Bond Strengthening Using External FRP Jackets,” Journal of Composites for Construction, ASCE, V. 12, No. 1, 2008, pp. 69-79. doi: 10.1061/(ASCE)1090-0268(2008)12:1(69)

13. Bournas, D. A., and Triantafillou, T. C., “Bond Strength of Lap-Spliced Bars in Concrete Confined with Composite Jackets,” Journal of Composites for Construction, ASCE, V. 15, No. 2, 2011, pp. 156-167. doi: 10.1061/(ASCE)CC.1943-5614.0000078

14. Garcia, R.; Helal, Y.; Pilakoutas, K.; and Guadagnini, M., “Bond Strength of Short Lap Splices in RC Beams Confined with Steel Stirrups or External CFRP,” Materials and Structures, V. 48, No. 1-2, 2015, pp. 277-293. doi: 10.1617/s11527-013-0183-5

15. Frangou, M.; Pilakoutas, K.; and Dritsos, S., “Structural Repair Strengthening of RC Columns,” Construction and Building Materials, V. 9, No. 5, 1995, pp. 259-266. doi: 10.1016/0950-0618(95)00013-6

16. Moghaddam, H.; Samadi, M.; Pilakoutas, K.; and Mohebbi, S., “Axial Compressive Behavior of Concrete Actively Confined by Metal Strips; Part A: Experimental Study,” Materials and Structures, V. 43, No. 10, 2010, pp. 1369-1381. doi: 10.1617/s11527-010-9588-6

17. Lee, H.-P.; Awang, A. Z.; and Omar, W., “Steel Strap Confined High Strength Concrete under Uniaxial Cyclic Compression,” Construction and Building Materials, V. 72, 2014, pp. 48-55. doi: 10.1016/j.conbuildmat.2014.08.007

18. Garcia, R.; Hajirasouliha, I.; Guadagnini, M.; Helal, Y.; Jemaa, Y.; Pilakoutas, K.; Mongabure, P.; Chrysostomou, C.; Kyriakides, N.; Ilki, A.; Budescu, M.; Taranu, N.; Ciupala, M. A.; Torres, L.; and Saiidi, M., “Full-Scale Shaking Table Tests on a Substandard RC Building Repaired and Strengthened with Post-Tensioned Metal Straps,” Journal of Earthquake Engineering, V. 18, No. 2, 2014, pp. 187-213. doi: 10.1080/13632469.2013.847874

19. Garcia, R.; Pilakoutas, K.; Hajirasouliha, I.; Guadagnini, M.; Kyriakides, N.; and Ciupala, M. A., “Seismic Retrofitting of RC Buildings Using CFRP and Post-Tensioned Metal Straps: Shake Table Tests,” Bulletin of Earthquake Engineering, Aug. 2015, doi: 10.1007/s10518-015-9800-8

20. Samadi, M.; Moghaddam, H.; and Pilakoutas, K., “Seismic Retrofit of RC Columns with Inadequate Lap-Splice Length by External Post-Tensioned High-Strength Strips,” Proceedings of the 15th World Conference on Earthquake Engineering, Lisbon, Portugal, 2012.

21. Joint ACI-ASCE Committee 408, “Bond and Development of Straight Reinforcing Bars in Tension (ACI 408R-03),” American Concrete Institute, Farmington Hills, MI, 2003, 49 pp.

22. Helal, Y.; Garcia, R.; Pilakoutas, K.; Guadagnini, M.; and Hajirasouliha, I., “Strengthening of Short Splices in RC Beams Using Post-Tensioned Metal Straps,” Materials and Structures, V. 49, No. 1, 2016, pp. 133-147. doi: 10.1617/s11527-014-0481-6

23. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

24. CEN, “EN 12390-3:2009 Testing Hardened Concrete Part 3: Compressive Strength of Test Specimens,” Comité Européen de Normalisation, Lausanne, Switzerland, 2009, 19 pp.

25. CEN, “EN 12390-6:2009 Testing Hardened Concrete Part 6: Tensile Splitting Strength of Test Specimens,” Comité Européen de Normalisation, Lausanne, Switzerland, 2009, 11 pp.

26. CEN, “EN 12390-5:2009 Testing Hardened Concrete Part 5: Flexural Strength of Test Specimens,” Comité Européen de Normalisation, Lausanne, Switzerland, 2009, 11 pp.

27. BSI, “BS 4449:2005 Steel for the Reinforcement of Concrete—Weldable Reinforcing Steel-Bar, Coil and Decoiled Product—Specification,” British Standards Institution, London, UK, 2009, 27 pp.

28. Duranovic, N.; Pilakoutas, K.; and Waldron, P., “EUROCRETE Experimental Programme—Structural Testing on RC Beams: Tests for Beams 1 to 4 of Phase I,” Report No. CCC/95/19A, Department of Civil and Structural Engineering, University of Sheffield, UK, 1995, 30 pp.

29. Al-Sunna, R.; Pilakoutas, K.; Hajirasouliha, I.; and Guadagnini, M., “Deflection Behaviour of FRP Reinforced Concrete Beams and Slabs: An Experimental Investigation,” Composites. Part B, Engineering, V. 43, No. 5, 2012, pp. 2125-2134. doi: 10.1016/j.compositesb.2012.03.007

30. fib, “Bond of Reinforcement in Concrete—State-of-Art Report,” Bulletin No. 10, Fédération Internationale du Béton, Lausanne, Switzerland, 2000, 427 pp.

31. Harajli, M. H., “Bond Strengthening of Lap Spliced Reinforcement Using External FRP Jackets: An Effective Technique for Seismic Retrofit of Rectangular or Circular RC Columns,” Construction and Building Materials, V. 23, No. 3, 2009, pp. 1265-1278. doi: 10.1016/j.conbuildmat.2008.07.028

32. CEB-FIP, “CEB-FIP Model Code 1990,” CEB Bulletin d’Information 213/214, Thomas Telford Ltd, 1993, 462 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer