Influence of Fluidized Ashes on Properties of Autoclaved Aerated Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Influence of Fluidized Ashes on Properties of Autoclaved Aerated Concrete

Author(s): Katarzyna Łaskawiec, Piotr Gebarowski, and Jan Małolepszy

Publication: Materials Journal

Volume: 113

Issue: 4

Appears on pages(s): 409-417

Keywords: autoclaved aerated concrete; environment assessment; fluidized ashes; siliceous ashes

DOI: 10.14359/51688984

Date: 7/1/2016

Abstract:
Coal fly ash, a by-product of coal combustion in thermal power plants, is one of the most complex and abundant anthropogenic materials. For several years, siliceous fly ash has been predominantly used as a substitute for material in the construction industry, either as a raw material or as an additive in the cement industry all over the world. Fly ash produced in coal-fired plants based on fluidized bed combustion technology accompanied by in-furnace desulfurization has significantly different properties compared to siliceous ashes. In this study, a brief characterization of fly ash from fluidized bed boilers is presented and possible alterations in fly ash use in autoclaved concrete production are discussed. Autoclaved aerated concrete production involving fluidized ashes proved to be more cost-effective and environmentally friendly. The content of lime and sulfates was found to be reduced by 10% to 20% and 60% to 100%, respectively, which limited the exploitation and consumption of the natural raw materials.

Related References:

1. Jatymowicz, H.; Siejko, J.; and Zapotoczna-Sytek, G., Technology of Autoclaved Aerated Concrete, Arkady, Warszawa, Poland, 1980, 202 pp. (in Polish)

2. Łaskawiec, K., “The Impact of Fluidized Bed Ash from Brown Coal on the Phase Composition and Properties of Autoclaved Aerated Concrete,” PhD thesis, University of Science and Technology, Kraków, Poland, 2010, 168 pp. (in Polish)

3. Kurdowski, W., and Pilch, M., “On the Mechanism of Scawtite Formation,” Proceedings of the 9th ICCC, New Delhi, India, V. 4, 1993, pp. 170-174.

4. de Silva, P. S., and Glasser, F. P., “Hydration of Cements Based on Metakaolin: Thermochemistry,” Advances in Cement Research, V. 3, No. 12, 1990, pp. 167-177. doi: 10.1680/adcr.1990.3.12.167

5. Ramachandran, V. S., and Zhang, C.-M., “Thermal Analysis of the 3CaO · Al2O3-CaSO4 · 2H2O-CaCO3-H2O System,” Thermochimica Acta, V. 106, 1986, pp. 273-282. doi: 10.1016/0040-6031(86)85139-5

6. Midgley, H. G. J., “The Use of Thermal Analysis Methods in Assessing the Quality of High Alumina Cement Concrete,” Journal of Thermal Analysis, V. 13, No. 3, 1978, pp. 515-524. doi: 10.1007/BF01912391

7. Midgley, H. G., and Midgley, A., “The Conversion of High Alumina Cement,” Magazine of Concrete Research, V. 27, No. 91, 1975, pp. 59-77. doi: 10.1680/macr.1975.27.91.59

8. Števula, L., and Petrovic, I., “Formation of Scawtite from Mixtures of CaO, Magnesite and Quartz under Hydrothermal Conditions,” Cement and Concrete Research, V. 11, No. 4, 1981, pp. 549-557. doi: 10.1016/0008-8846(81)90084-3

9. Watt, J. D., and Thome, D. J., “Composition and Pozzolanic Properties of Pulverized Fuel Ashes, II. Pozzolanic Properties of Fly Ashes, as Determined By Crushing Strength Tests on Lime Mortars,” Journal of Applied Chemistry, V. 16, 1965, pp. 595-604.

10. Venuat, M., “Ciments aux Cendres Volantes—Influence de la Propotion de Cendre sur les Proprieties de Ciments,” Cendre d’Etudes et de recherché de l’industrie des Liants, Hydrauliques, Paris, France, 1962, 8 pp.

11. Diamond, S., “The Characterization of Fly Ashes,” Effects of Fly Ash Incorporation in Cement and Concrete, Proceedings, Symposium N, Materials Research Society, Warrendale, PA, 1981, pp. 12-23.

12. Hulett, L. D., and Weinberger, A. J., “Some Etching Studies of the Microstructure and Composition of Large Aluminosilicate Particles in Fly Ash from Coal-Burning Power Plants,” Environmental Science & Technology, V. 14, No. 8, 1980, pp. 965-970. doi: 10.1021/es60168a013

13. Dudas, M. J., and Warren, X. J., “Submicroscopic Structure and Characteristics of Intermediate-Calcium Fly Ashes,” MRS Proceedings, Materials Research Society, Warrendale, PA, 1987, pp. 309-316.

14. EN-771-4:2011+A1:2015-10, “Specification for Masonry Units—Part 4: Autoclaved Aerated Concrete Masonry Units,” European Committee for Standardization, Brussels, Belgium, 2011, 48 pp.

15. EN-772-13:2000, “Methods of Test for Masonry Units. Determination of Net and Gross Dry Density of Masonry Units (Except for Natural Stone),” European Committee for Standardization, Brussels, Belgium, 2000, 12 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal