Sliding Shear Resistance of Squat Walls under Reverse Loading: Mechanical Model and Parametric Study

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Sliding Shear Resistance of Squat Walls under Reverse Loading: Mechanical Model and Parametric Study

Author(s): Harald Schuler and Burkhart Trost

Publication: Structural Journal

Volume: 113

Issue: 4

Appears on pages(s): 711-721

Keywords: aggregate interlock; cold joint; curvature ductility; dowel action; earthquake loads; reverse loading; sliding shear failure; squat walls

DOI: 10.14359/51688748

Date: 7/1/2016

Abstract:
Shear walls are used to stabilize buildings against earthquakes under cyclic loading. A critical state in the loading procedure is the second half cycle (reverse loading) because a crack is opened along the complete wall length. This results in reduced sliding shear resistance, especially at cold joints, which are weak points. The article presents a model to analyze the sliding shear resistance on a flexural crack. The model is set up as a failure criterion plotted against the moment-curvature curve. It allows the studying of the single effects, aggregate interlock and the load-carrying capacity of the inclined compression strut, and dowel action and shear resistance of the reinforcement on the sliding shear resistance. A parametric study is carried out to investigate the influence of an axial force and different web reinforcement ratios.

Related References:

1. Bohl, A., and Adebar, P., “Plastic Hinge Lengths in High-Rise Concrete Shear Walls,” ACI Structural Journal, V. 108, No. 2, Mar.-Apr. 2011, pp. 148-157.

2. Beyer, K.; Dazio, A.; and Priestley, M. J. N., “Shear Deformations of Slender Reinforced Concrete Walls under Seismic Loading,” ACI Structural Journal, V. 108, No. 2, Mar.-Apr. 2011, pp. 167-177.

3. Synge, A. J., “Ductility of Squat Shear Walls,” Research Report No. 80-8, Department of Civil Engineering, University of Canterbury, Christchurch, New Zealand, 1980, 150 pp.

4. Paulay, T.; Priestley, M. J. N.; and Synge, A. J., “Ductility in Earthquake Resisting Squat Shearwalls,” ACI Structural Journal, V. 79, No. 4, July-Aug. 1982, pp. 257-269.

5. Luna, B. N.; Rivera, J. P.; Rocks, J. F.; Goksu, C.; Weinreber, S.; and Whittaker, A. S., “University at Buffalo—Low Aspect Ratio Rectangular Reinforced Concrete Shear Wall: Specimen SW8,” Network for Earthquake Engineering Simulation (distributor), Dataset, 2013, doi: 10.4231/D3XP6V35S

6. EN 1992-1-1, “Eurocode 2: Design of Concrete Structures—Part 1-1: General Rules and Rules for Buildings,” European Committee for Standardization, Brussels, Belgium, 237 pp.

7. fib Bulletin 56, “Model Code 2010,” first complete draft – Volume 2, 288 pp.

8. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-11) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2011, 503 pp.

9. SIA 262:2013, “Betonbau,” Schweizer Ingenieur- und Architektenverein, Zürich, Switzerland, 2013, 102 pp.

10. SIA 2018 Instruction Sheet, “Überprüfung bestehender Gebäude bezüglich Erdbeben,” Schweizer Ingenieur- und Architektenverein, Zürich, Switzerland, 2004, 38 pp.

11. Rassmusen, B. H., “Strength of Transversely Loaded Bolts and Dowels Embedded in Concrete,” Meddelelse Laboratoriet for Bugningastatik, Denmark Technical University, V. 34, No. 2, 1962, pp. 39-55.

12. Vintzeleou, E. N., and Tassios, T. P., “Mathematical Models for Dowel Action under Monotonic Conditions,” Magazine of Concrete Research, V. 38, No. 134, 1986, pp. 13-22. doi: 10.1680/macr.1986.38.134.13

13. Zilch, K., and Zehetmaier, G., “Bemessung im konstruktiven Betonbau,” Springer-Verlag Berlin Heidelberg, 2010, 627 pp.

14. Salonikios, T. N.; Kappos, A. J.; Tegos, I. A.; and Penelis, G. G., “Cyclic Load Behavior of Low-Slenderness Reinforced Concrete Walls: Design Basis and Test Results,” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 649-660.

15. Burgueno, R.; Liu, X.; and Hines, E. M., “Web Crushing Capacity of High-Strength Concrete Structural Walls: Experimental Study,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr. 2014, pp. 235-246.

16. Hines, E. M., and Seible, F., “Web Crushing of Hollow Rectangular Bridge Piers,” ACI Structural Journal, V. 101, No. 4, July-Aug. 2004, pp. 569-579.

17. Trost, B.; Schuler, H.; and Stojadinovic, B., “Experimental Investigation of Sliding of Walls on Compact Sliding Specimens,” Proceedings of the 15th European Conference on Earthquake Engineering, Istanbul, Turkey, Aug. 24-29, 2014, 10 pp.

18. Schuler, H., and Trost, B., “Sliding Resistance at the Joint between a Structural Wall and the Basement Ceiling: A Mechanical Model,” Proceedings of the 15th European Conference on Earthquake Engineering, Istanbul, Turkey, Aug. 24-29, 2014, 13 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal