Improving the Quality of Concrete Testing

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Improving the Quality of Concrete Testing

Author(s): Kevin Kane, Todd Laker, and Steve Morrical

Publication: Concrete International

Volume: 37

Issue: 8

Appears on pages(s): 33-40

Keywords: competency, field, laboratory, variation

DOI: 10.14359/51688027

Date: 8/1/2015

Abstract:
There is a concern among ready mixed concrete producers that quality assurance testing is not consistently performed in accordance with ASTM standards. All project participants are affected by substandard testing practices, as false-positive or false-negative test results can lead to rejections of good concrete loads or acceptance of bad quality concrete, respectively. The article makes recommendations for evaluating and improving the quality of concrete testing, and it describes a program that allows testing agencies and their technicians to assess their performance relative to their peers.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

2. ACI Committee 310, “Specifications for Structural Concrete (ACI 301-10),” American Concrete Institute, Farmington Hills, MI, 2010, 77 pp.

3. “Guide to Improving Specifications for Ready Mixed Concrete,” Publication 2PE003, National Ready Mixed Concrete Association, Silver Spring, MD, 2009, 22 pp. (www.nrmca.org/Research_Engineering/Documents/Improving_RMC_Specs_Guide_(May2009)_SECURED.pdf)

4. Pielert, J.H., “Quality Cement, Concrete, and Aggregates—The Role of the Testing Laboratories,” STP 169D, ASTM International, West Conshohocken, PA, pp. 51-55.

5. ACI Certification Programs Committee and ACI Committee C610, “Technician Workbook, CP-1 (15),” American Concrete Institute, Farmington Hills, MI, 2015, 42 pp.

6. Malisch, W.R., “How Producers can Correct Improper Test-Cylinder Curing,” The Aberdeen Group, 1997. (www.theconcreteproducer.com/images/How%20Producers%20Can%20Correct%20Improper%20Test-Cylinder%20Curing_tcm77-1373385.pdf)

7. “2014 Concrete Compressive Strength & Fine Aggregate Round Robin Test Results,” Colorado Department of Transportation, Denver, CO, Feb. 20, 2014.

8. Akhavan, R., and Malik, M., “Initial Curing of Portland Cement Concrete Cylinders,” Report No. CDOT-R&D-SM-99-4, Colorado Department of Transportation, Denver, CO, 1999, 32 pp.

9. “NRMCA-ASCC Checklist for the Concrete Pre-Construction Conference,” The Contractors Guide to Quality Concrete Construction, third edition, American Concrete Institute and American Society of Concrete Contractors, St. Louis, MO, 2005, 147 pp.

10. Snell, L., “Assessing Concrete Strength Results,” Concrete International, V. 25, No. 12, Dec. 2003, pp. 43-45.