Experimental Investigation of Blast-Pressure Attenuation by Cellular Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Experimental Investigation of Blast-Pressure Attenuation by Cellular Concrete

Author(s): Weimin Nian, Kolluru V. L. Subramaniam, and Yiannis Andreopoulos

Publication: Materials Journal

Volume: 112

Issue: 1

Appears on pages(s): 21-28

Keywords: blast; cellular concrete; crushing; dissipation; protection; shock; impact; impulse

DOI: 10.14359/51687242

Date: 1/1/2015

Abstract:
Results from an experimental investigation of the dynamic response of cellular concrete subjected to blast-pressure loading are presented. The cellular concrete has large entrained porosity in the form of uniformly distributed air cells in a matrix of hardened cement. Under quasi-static loading, once the applied stress exceeds the crushing strength of the cellular concrete, crushing and densification of material results in an upward concave stress-strain response. The shock-tube experimental test setup used for generating blast-pressure loading in a controlled manner is described. Experimental results from the cellular concrete subjected to blast-pressure loading with pressure amplitude greater than its crushing strength indicate that a compression stress wave, which produces compaction of the material due to collapse of the cellular structure, is produced in the material. As the compaction front propagates in the material, there is a continuous decrease in its amplitude. The impulse of the blast pressure wave is conserved. When a sufficient length of the cellular concrete is present, the applied blast pressure wave is completely attenuated to a rectangular stress pulse. The transmitted stress to a substrate from cellular concrete when an applied blast pressure wave is completely attenuated resembles a rectangular stress pulse of amplitude slightly higher than the crushing strength of the material with a duration predicted by the applied blast impulse.

Related References:

1. Kingery, C. N., and Bulmash, G., “Air-Blast Parameters from TNT Spherical Air Burst and Hemi-spherical Surface Burst,” Technical Report ARBRL-TR-02555, U.S. Army Armament Research Development Center, Ballistic Research Laboratory, Aberdeen Proving Ground, MD, 1988.

2. U.S. Department of the Army, “Structures to Resist the Effects of Accidental Explosions,” Technical Manual TM5-1300, Washington, DC, 1990.

3. Conley, C. H., and Gregory, F. H., “Modeling of Blast-Loaded Structural Panels,” Proceedings of the Eighth Annual U.S. Army Research Laboratory/U.S. Military Academy Technical Symposium, The Mathematical Sciences Center of Excellence, West Point, NY, Nov. 2000, pp. 221-235.

4. Conley, C. H., and Gregory, F. H., “Vulnerability of Structural Panels to Blast Effects,” Proceedings of the 70th Shock & Vibration Symposium, Albuquerque, NM, Nov. 1999.

5. Mosalam, K. M., and Mosallam, A. S., “Nonlinear Transient Analysis of Reinforced Concrete Slabs Subjected to Blast Loading and Retrofitted with CFRP Composites,” Composites, Part B: Engineering, V. 32, No. 8, 2001, pp. 623-636. doi: 10.1016/S1359-8368(01)00044-0

6. Davidson, J. S.; Fisher, J. W.; Hammons, M. I.; Porter, J. R.; and Dinan, R. J., “Failure Mechanisms of Polymer-Reinforced Concrete Masonry Walls Subjected to Blast,” Journal of Structural Engineering, ASCE, V. 131, No. 8, 2005, pp. 1194-1205. doi: 10.1061/(ASCE)0733-9445(2005)131:8(1194)

7. Hamoush, S. A.; McGinley, M. W.; Mlakar, P.; and Murray, K., “Out-of-Plane Strengthening of Masonry Walls with Reinforced Composites,” Journal of Composites for Construction, ASCE, V. 5, No. 3, 2001, pp. 139-145. doi: 10.1061/(ASCE)1090-0268(2001)5:3(139)

8. DTRA/TSWG Program, “Blast Mitigation for Structures, 199 Status report on the DTRA/TSWG Program,” National Academy Press, Washington, DC, 1999.

9. Eamon, C. D.; Baylot, J. D.; and O’Daniel, J. L., “Modeling Concrete Masonry Walls Subjected to Explosive Loading,” Journal of Engineering Mechanics, ASCE, V. 130, No. 9, 2004, pp. 1098-1106. doi: 10.1061/(ASCE)0733-9399(2004)130:9(1098)

10. Tan, P. J.; Reid, S. R.; Harrigan, J. J.; Zou, Z.; and Li, S., “Dynamic Compressive Strength Properties of Aluminum Foams. Part I—Experimental Data and Observations,” Journal of the Mechanics and Physics of Solids, V. 53, No. 10, 2005, pp. 2174-2205. doi: 10.1016/j.jmps.2005.05.007

11. Gibson, L. J., and Ashby, M. F., Cellular Solids: Structures and Properties, Progress Press, Oxford, England, 1988.

12. Guruprasad, S., and Mukherjee, A., “Layered Sacrificial Claddings under Blast Loading. Part II: Experimental Studies,” International Journal of Impact Engineering, V. 24, No. 9, 2000, pp. 975-984. doi: 10.1016/S0734-743X(00)00005-1

13. Hanssen, A. G.; Enstock, L.; and Langseth, M., “Close Range Blast Loading of Aluminium Foam Panels,” International Journal of Impact Engineering, V. 27, No. 6, 2002, pp. 593-618. doi: 10.1016/S0734-743X(01)00155-5

14. Hoff, G. C., “New Application for Low-Density Concretes,” Lightweight Concrete, SP-29, American Concrete Institute, Farmington Hills, MI, 1971, pp. 181-220.

15. Bulson, P. S., Buried Structures: Static and Dynamic Strength, Taylor & Francis, Oxford, UK, 1984, 248 pp.

16. Ma, G. W., and Ye, Z. Q., “Analysis of Foam Claddings for Blast Alleviation,” International Journal of Impact Engineering, V. 34, No. 1, 2007, pp. 60-70. doi: 10.1016/j.ijimpeng.2005.10.005

17. Li, Q. M., and Meng, H., “Pressure-Impulse Diagram for Blast Loads Based on Dimensional Analysis and Single-Degree-of-Freedom Model,” Journal of Engineering Mechanics, ASCE, V. 128, No. 1, 2002, pp. 87-92. doi: 10.1061/(ASCE)0733-9399(2002)128:1(87)

18. Ye, Z. Q., and Ma, G. W., “Effects of Foam Claddings for Structure Protection against Blast Loads,” Journal of Engineering Mechanics, ASCE, V. 133, No. 1, 2007, pp. 41-47. doi: 10.1061/(ASCE)0733-9399(2007)133:1(41)

19. Nian, W.; Subramaniam, K. V.; and Andreopoulos, Y., “Dynamic Compaction of Foam under Blast Loading Considering Fluid-Structure Interaction Effects,” International Journal of Impact Engineering, V. 50, 2012, pp. 29-39. doi: 10.1016/j.ijimpeng.2012.06.005


ALSO AVAILABLE IN:

Electronic Materials Journal