Seismic Performance of Precast Columns with Mechanically Spliced Column-Footing Connections

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance of Precast Columns with Mechanically Spliced Column-Footing Connections

Author(s): Zachary B. Haber, M. Saiid Saiidi, and David H. Sanders

Publication: Structural Journal

Volume: 111

Issue: 3

Appears on pages(s): 639-650

Keywords: accelerated bridge construction; cyclic loading; ductility; emulative; grout sleeve; mechanical coupler; plastic hinge

DOI: 10.14359/51686624

Date: 5/1/2014

Abstract:
This paper presents the results from a large-scale experimental study that was conducted at the University of Nevada, Reno, NV. Five half-scale bridge column models were constructed and tested under reversed slow cyclic loading. The study focused on developing four new moment connections at column-footing joints for accelerated bridge construction in regions of high seismicity. The new connections were employed in precast columns, each using mechanical splices to create connectivity with reinforcing bars in a cast-in-place footing. Two different mechanical splices were studied: an upset headed coupler and a grout-filled sleeve coupler. Along with the splice type, the location of couplers within the plastic hinge zone was also a test variable. All precast models were designed with the intent to emulate conventional cast-in-place construction and, thus, were compared with a conventional cast-in-place test model. Results indicate the behavior of these new connections was similar to that of conventional cast-in-place construction with respect to key response parameters, although the plastic hinge mechanism could be significantly affected by the couplers.