Title: Rehabilitation of Flushing Viaduct

Author(s): Mysore Nagaraja and Raza A. Khan

Publication: Concrete International

Volume: 16

Issue: 8

Appears on pages(s): 44-47

Keywords: arches; ballast; columns (supports); efflorescence; elevated railways; repairs; spalling; viaducts; Construction

DOI:

Date: 8/1/1994

Abstract:
Flushing Viaduct, a concrete arch structure supporting the New York City Transit Authority's track, is being rehabilitated. The condition surveys and the investigation leading to the detection of the alkali-silica reactivity that contributed to the freeze-thaw damage are covered. The repair philosophy and major design decisions leading to a significant rehabilitation project are enumerated.




  