Title: 
            Problems and Solutions Pertaining to Rigid Pavement Joint Resealing
        
        
            Author(s): 
            J. Bugler
        
        
            
                Publication: 
                Symposium Paper
            
            
                Volume: 
                94
            
            
                Issue: 
                
            
            
                Appears on pages(s): 
                975-996
            
            
                Keywords: 
                abrasive blasting; cleaning; concrete pavements; inspection; installing; joint sealers; joints (junctions); maintenance; performance; safety; specifications; General
            
            
                DOI: 
                10.14359/3767
            
        
        
            Date: 
            7/1/1987
        
        
            Abstract:
            This paper describes field application problems experienced during the execution of a joint resealing program initiated within the limits of Region 10 (Nassau and Sufflok Counties) in the early 1980s. It describes what was done to overcome these problems. Solutions to such problems involved equipment modification and improved inspection technique. These modifications resulted in the virtual elimination of joint overfilling and a ten-fold performance improvement with regards to first-year intermittent bond adhesion failure. Worker safety and protection are discussed.