Capacity of Reinforced Concrete One-Way Slabs under Concentrated Loads

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Capacity of Reinforced Concrete One-Way Slabs under Concentrated Loads

Author(s): Gabriela I. Zarate Garnica, Eva O. L. Lantsoght, Yuguang Yang, and Max A. N. Hendriks

Publication: Structural Journal

Volume: 123

Issue: 4

Appears on pages(s): 73-87

Keywords: bridge assessment; concentrated load; concrete bridges; flexure; large-scale testing; shear; slab bridge

DOI: 10.14359/51749407

Date: 7/1/2026

Abstract:
For the assessment of existing reinforced concrete slab bridges, the shear capacity under concentrated loads and transition to flexural failure are under discussion. Previous research showed an increased shear capacity for slabs under concentrated loads close to the support, so that for assessment, positions farther from the support became governing. This experimental research studies the flexural and shear capacity of reinforced concrete slabs under concentrated loads. For this purpose, six slabs representing 1:2-scale continuous slab bridges were tested at various positions from the support and along the width. The results show two main failure modes: flexural failure (onset of yielding of the reinforcement), and shear failure. Secondary punching was observed as well. The comparison between the test results and calculation methods shows that all considered methods perform reasonably well when both shear and flexure are considered, and the effective width in shear is included, with average tested-to-predicted capacities between 0.92 (Regan’s method) and 1.39 (Extended Strip Model [ESM]) and coefficients of variation between 15% (Regan’s method) and 25% (ACI 318-19 and Eurocode 2). These insights can be used for the assessment of existing reinforced concrete slab bridges.

Related References:

Abambres, M., and Lantsoght, E. O. L., 2020, “Neural Network-Based Formula for Shear Capacity Prediction of One-Way Slabs under Concentrated Loads,” Engineering Structures, V. 211, p. 110501. doi: 10.1016/j.engstruct.2020.110501

ACI Committee 318, 2019, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19) (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 623 pp.

Adam, V.; Classen, M.; Hillebrand, M.; and Hegger, J., 2019, “Shear in Continuous Slab Segments without Shear Reinforcement under Distributed Loads,” fib symposium 2019, Cracow, Poland.

Adam, V.; Schmidt, M.; and Hegger, J., 2023, “One-Way Flexural Shear Tests on Wide Reinforced Concrete Slab Segments with Simple and Intermediate Supports,” Structural Concrete, V. 24, No. 2, pp. 2911-2929. doi: 10.1002/suco.202200398

de Sousa, A. M.; Lantsoght, E. O.; Genikomsou, A. S.; Prado, L. P.; and El Debs, M. K., 2023a, “NLFEA of One-Way Slabs in Transition between Shear and Punching: Recommendations for Modeling,” Engineering Structures, V. 293, p. 116617. doi: 10.1016/j.engstruct.2023.116617

de Sousa, A. M. D.; Lantsoght, E. O. L.; Araújo, D. L.; Prado, L. P.; and El Debs, M. K., 2023d, “Recommendations to Assess the Shear and Punching Capacity of One-Way Slabs under Concentrated Loads According to the ABNT NBR 6118:2014,” Revista IBRACON de Estruturas e Materiais, V. 16, No. 3, p. e16308. doi: 10.1590/s1983-41952023000300008

de Sousa, A. M. D.; Lantsoght, E. O. L.; and El Debs, M. K., 2021a, “One-Way Shear Strength of Wide Reinforced Concrete Members without Stirrups,” Structural Concrete, V. 22, No. 2, pp. 968-992. doi: 10.1002/suco.202000034

de Sousa, A. M. D.; Lantsoght, E. O. L.; and El Debs, M. K., 2023b, “Failure Mechanism of One-Way Slabs under Concentrated Loads after Local Reinforcement Yielding,” Engineering Structures, V. 291, p. 116396. doi: 10.1016/j.engstruct.2023.116396

de Sousa, A. M. D.; Lantsoght, E. O. L.; and El Debs, M. K., 2023c, “Shear and Punching Capacity Predictions for One-Way Slabs under Concentrated Loads Considering the Transition between Failure Mechanisms,” Buildings, V. 13, No. 2, p. 434. doi: 10.3390/buildings13020434

de Sousa, A. M. D.; Lantsoght, E. O. L.; Yang, Y.; and El Debs, M. K., 2021b, “Extended CSDT Model for Shear Capacity Assessments of Bridge Deck Slabs,” Engineering Structures, V. 234, p. 111897. doi: 10.1016/j.engstruct.2021.111897

Elstner, R. C., and Hognestad, E., 1956, “Shearing Strength of Reinforced Concrete Slabs,” ACI Journal Proceedings, V. 53, No. 7, July, pp. 29-58.

Fernández, P. G.; Marí, A.; and Oller, E., 2021, “Experimental Investigation of the Shear Strength of One-Way Reinforced Concrete (RC) Slabs Subjected to Concentrated Loads and In-Plane Transverse Axial Tension,” Structural Concrete, V. 22, No. 6, pp. 3661-3676. doi: 10.1002/suco.202100447

Fernández, P. G.; Marí, A.; and Oller, E., 2023, “Theoretical Prediction of the Shear Strength of Reinforced Concrete Slabs under Concentrated Loads Close to Linear Supports,” Structure and Infrastructure Engineering, V. 19, No. 7, pp. 890-903. doi: 10.1080/15732479.2021.1988990

Gurutzeaga, M.; Oller, E.; Ribas, C.; Cladera, A.; and Marí, A., 2015, “Influence of the Longitudinal Reinforcement on the Shear Strength of One-Way Concrete Slabs,” Materials and Structures, V. 48, No. 8, pp. 2597-2612. doi: 10.1617/s11527-014-0340-5

Hawkins, N. M., and Mitchell, D., 1979, “Progressive Collapse of Flate-Plate Structures,” ACI Journal Proceedings, V. 76, No. 7, July, pp. 775-808.

Hillerborg, A., 1975, “Strip Method of Design,” Viewpoint Publications, Cement and Concrete Association, Wexham Springs, UK.

Hillerborg, A., 1982, “The Advanced Strip Method - A Simple Design Tool,” Magazine of Concrete Research, V. 34, No. 121, pp. 175-181. doi: 10.1680/macr.1982.34.121.175

Hillerborg, A., 1996, Strip Method Design Handbook, E & FN Spon, London, UK.

Kani, G. N. J., 1964, “The Riddle of Shear Failure and Its Solution,” ACI Journal Proceedings, V. 61, No. 4, Apr., pp. 441-467.

Kani, G. N. J., 1966, “Basic Facts Concerning Shear Failure,” ACI Journal Proceedings, V. 63, No. 6, June, pp. 675-692.

Koekkoek, R. T., and Yang, Y., 2016, “Measurement Report on the Transition between Flexural and Shear Failure of RC Beams without Shear Reinforcement,” Stevin Report 25.5-16-04, Delft University of Technology, Delft, the Netherlands, 529 pp.

König, G., and Fischer, J., 1995, “Model Uncertainties Concerning Design Equations for the Shear Capacity of Concrete Members without Shear Reinforcement,” CEB Bulletin 224, Model Uncertainties and Concrete Barrier for Environmental Protection, July, pp. 49-100.

Kuchma, D. A.; Wei, S.; Sanders, D. H.; Belarbi, A.; and Novak, L. C., 2019, “Development of the One-Way Shear Design Provisions of ACI 318-19 for Reinforced Concrete,” ACI Structural Journal, V. 116, No. 4, July, pp. 285-295.

Lantsoght, E. O.; van der Veen, C.; de Boer, A.; and Alexander, S. D., 2017a, “Extended Strip Model for Reinforced Concrete Slabs under Concentrated Loads,” ACI Structural Journal, V. 114, No. 2, Mar.-Apr., pp. 565-574.

Lantsoght, E. O. L.; van der Veen, C.; De Boer, A.; and Walraven, J., 2014, “Influence of Width on Shear Capacity of Reinforced Concrete Members,” ACI Structural Journal, V. 111, No. 6, Nov.-Dec., pp. 1441-1450. doi: 10.14359/51687107

Lantsoght, E. O. L.; van der Veen, C.; de Boer, A.; and Walraven, J., 2015a, “One-Way Slabs Subjected to Combination of Loads Failing in Shear,” ACI Structural Journal, V. 112, No. 4, July-Aug., pp. 417-426.

Lantsoght, E. O. L.; van der Veen, C.; de Boer, A.; and Walraven, J. C., 2013a, “Recommendations for the Shear Assessment of Reinforced Concrete Slab Bridges from Experiments,” Structural Engineering International, V. 23, No. 4, pp. 418-426. doi: 10.2749/101686613X13627347100239

Lantsoght, E. O. L.; van der Veen, C.; Walraven, J.; and de Boer, A., 2015b, “Experimental Investigation on Shear Capacity of Reinforced Concrete Slabs with Plain Bars and Slabs on Elastomeric Bearings,” Engineering Structures, V. 103, pp. 1-14. doi: 10.1016/j.engstruct.2015.08.028

Lantsoght, E. O. L.; van der Veen, C.; and Walraven, J. C., 2013b, “Shear in One-Way Slabs under a Concentrated Load Close to the Support,” ACI Structural Journal, V. 110, No. 2, Mar.-Apr., pp. 275-284.

Lantsoght, E. O. L.; Yang, Y.; van der Veen, C.; de Boer, A.; and Hordijk, D. A., 2017b, “Beam Experiments on Acceptance Criteria for Bridge Load Tests,” ACI Structural Journal, V. 114, No. 4, July-Aug., pp. 1031-1041.

Leonhardt, F., and Walther, R., 1962, “Beitrage zur Behandlung der Schubprobleme in Stahlbetonbau - 2. Fortsetzung des Kapitels II. Versuchsberichte,” Beton- und Stahlbetonbau, V. 57, No. 3, pp. 54-64.

Lubell, A. S., 2006, “Shear in Wide Reinforced Concrete Members,” PhD dissertation, University of Toronto, Toronto, ON, Canada, 2006, 455 pp.

Lubell, A. S.; Bentz, E.; and Collins, M. P., 2008, “One-Way Shear in Wide Concrete Beams with Narrow Supports,” ASCE Structures Congress, Vancouver, BC, Canada, 10 pp.

Lubell, A. S.; Bentz, E. C.; and Collins, M. P., 2009a, “Shear Reinforcement Spacing in Wide Members,” ACI Structural Journal, V. 106, No. 2, Mar.-Apr., pp. 205-214.

Lubell, A. S.; Bentz, E. C.; and Collins, M. P., 2009b, “Influence of Longitudinal Reinforcement on One-Way Shear in Slabs and Wide Beams,” Journal of Structural Engineering, ASCE, V. 135, No. 1, Jan., pp. 78-87. doi: 10.1061/(ASCE)0733-9445(2009)135:1(78)

Lubell, A. S.; Sherwood, E. G.; Bentz, E.; and Collins, M. P., 2004, “Safe Shear Design of Large, Wide Beams,” Concrete International, V. 26, No. 1, Jan., pp. 67-78.

Marí, A.; Cladera, A.; Oller, E.; and Bairán, J. M., 2018, “A Punching Shear Mechanical Model for Reinforced Concrete Flat Slabs with and without Shear Reinforcement,” Engineering Structures, V. 166, pp. 413-426. doi: 10.1016/j.engstruct.2018.03.079

Muttoni, A., and Ruiz, M. F., 2012, “Levels-of-Approximation Approach in Codes of Practice,” Structural Engineering International, V. 22, No. 2, pp. 190-194. doi: 10.2749/101686612X13291382990688

Muttoni, A., and Simões, J. T., 2023, “Shear and Punching Shear According to the Critical Shear Crack Theory: Background, Recent Developments and Integration in Codes,” Revista IBRACON de Estruturas e Materiais, V. 16, No. 3, p. e16302. doi: 10.1590/s1983-41952023000300002

NEN-EN 1991-2:2003, 2003, “Eurocode 1 - Actions on Structures - Part 2: Traffic Loads on Bridges,” Comité Européen de Normalisation, Brussels, Belgium, 168 pp.

NEN-EN 1992-1-1:2005, 2005, “Eurocode 2: Design of Concrete Structures - Part 1-1 General Rules and Rules for Buildings,” Comité Européen de Normalisation, Brussels, Belgium, 229 pp.

Olonisakin, A. A., and Alexander, S. D. B., 1999, “Mechanism of Shear Transfer in a Reinforced Concrete Beam,” Canadian Journal of Civil Engineering, V. 26, No. 6, pp. 810-817. doi: 10.1139/l99-044

prEN 1992-1-1:2021-09, 2021, “Eurocode 2: Design of Concrete Structures - Part 1-1: General Rules - Rules for Buildings, Bridges and Civil Engineering Structures,” Comité Européen de Normalisation, Brussels, Belgium, 377 pp.

Regan, P., 1982, “Shear Resistance of Concrete Slabs at Concentrated Loads Close to Supports,” Polytechnic of Central London, London, UK, pp. 1-24.

Regan, P. E., 1987, “Shear Resistance of Members without Shear Reinforcement; Proposal for CEB Model Code MC90,” Polytechnic of Central London, London, UK, 28 pp.

Reissen, K.; Classen, M.; and Hegger, J., 2018, “Shear in Reinforced Concrete Slabs—Experimental Investigations in the Effective Shear Width of One‐Way Slabs under Concentrated Loads and with Different Degrees of Rotational Restraint,” Structural Concrete, V. 19, No. 1, pp. 36-48. doi: 10.1002/suco.201700067

Rijkswaterstaat, 2013, “Richtlijnen Beoordeling Kunstwerken - beoordeling van de constructieve veiligheid van een bestaand kunstwerk bij verbouw, gebruik en afkeur,” RTD 1006:2013, Utrecht, the Netherlands, 117 pp.

Rijkswaterstaat, 2022, “Richtlijnen Beoordeling Kunstwerken - beoordeling van de constructieve veiligheid van een bestaand kunstwerk bij verbouw, gebruik en afkeur RBK 1.2.1,” RTD 1006:2022, Utrecht, the Netherlands, 117 pp.

Sherwood, E. G., 2008, “One-Way Shear Behaviour of Large, Lightly-Reinforced Concrete Beams and Slabs,” PhD dissertation, University of Toronto, Toronto, ON, Canada, pp. 547.

Sherwood, E. G.; Lubell, A. S.; Bentz, E. C.; and Collins, M. R., 2006, “One-Way Shear Strength of Thick Slabs and Wide Beams,” ACI Structural Journal, V. 103, No. 6, Nov.-Dec., pp. 794-802.

Simmonds, S., 1999, “Using Theorums of Plasticity: History and Concept,” Design of Two-Way Slabs, SP-183, American Concrete Institute, Farmington Hills, MI, pp. 77-92.

Sinning, A.; Adam, V.; Classen, M.; and Hegger, J., 2023, “Impact of Distributed Loading and Intermediate Supports on Flexural Shear Behavior of Slab Segments Without Shear Reinforcement,” Springer Nature Switzerland, pp. 1420-1429.

Thorenfeldt, E., 1987, “Mechanical Properties of High-Strength Concrete and Applications in Design,” Symposium Proceedings, Utilization of High-Strength Concrete, Norway.

Van den Hoogen, M., 2013, “Beam or Truss Mechanism for Shear in Concrete,” MSc thesis, Delft University of Technology, Delft, the Netherlands.

Vervuurt, A.; Courage, W.; and Steenbergen, R., 2012, “Betonsterkte bestaande constructies,” Cement, V. 64, No. 4, pp. 36-39.

Zarate Garnica, G. I.; de Vries, R.; and Lantsoght, E. O. L., 2022, “Analysis Report of Reinforced Concrete Slabs for Stop Criteria,” Stevin Report 25.5-22-02, Delft University of Technology.

Zarate Garnica, G. I., and Lantsoght, E. O. L., 2020, “Preparation of Experiments on Reinforced Concrete Slabs for Determination of Stop Criteria,” Stevin Report 25.5-20-03, Delft University of Technology, Delft, the Netherlands, 164 pp.

Zarate Garnica, G. I., and Lantsoght, E. O. L., 2021, “Measurement Report of Reinforced Concrete Slabs,” Stevin Report 25.5-21-03, Delft University of Technology, Delft, the Netherlands.


ALSO AVAILABLE IN: