Title: NEU news

Author(s):

Publication: Concrete International

Volume: 47

Issue: 11

Appears on pages(s): 40-41

Keywords:

DOI: 10.14359/51749285

Date: 11/1/2025

Abstract:
To help meet the carbon reduction goals of the cement and concrete industry, NEU: An ACI Center of Excellence for Carbon Neutral Concrete conducted a two-part online survey. The survey requested information from innovative low-carbon materials and technology companies. The questions were aimed at understanding the companies’ product characteristics, including manufacturing processes, availability, market presence, applications, and environmental performance.




  