Properties of Tunnel Fireproof Mortar: Effect of Alkali Equivalent

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Properties of Tunnel Fireproof Mortar: Effect of Alkali Equivalent

Author(s): Shuanghui Wen, Wei Zhao, Xiaowen Zhao, Yongning Liang, and Tao Ji

Publication: Materials Journal

Volume: 123

Issue: 1

Appears on pages(s): 63-74

Keywords: alkali-activated slag; desulfurization gypsum; Na2O equivalent; tunnel fireproof mortar; wind and vibration resistance

DOI: 10.14359/51749269

Date: 1/1/2026

Abstract:
Desulfurization gypsum—alkali-activated slag-based tunnel fireproof mortar (GAM)—is a lightweight, cement-based fireproof material. A series of tests were conducted to investigate the effect of varying Na2O equivalents (2, 4, 6, and 8%) on the wind and vibration resistance of GAM, along with its bond strength, and so on. Through X-ray diffraction (XRD), thermogravimetric- derivative thermogravimetric analysis (TG-DTG), scanning electronic microscope (SEM), and mercury intrusion porosimetry (MIP) analyses, the underlying mechanisms were elucidated. The study indicates that as the Na2O equivalent increases, the weight loss of C-(A)-S-H gel and AFt phase exhibits an initial increase followed by a decrease. The weight loss of CaSO4·2H2O crystals, the crystal-to-gel ratio, and total porosity first decrease and then increase. Therefore, the fire resistance of GAM first decreases and then increases, while the dry density, compressive strength, bond strength, and wind and vibration resistance of GAM initially increase and subsequently decrease with increasing Na2O equivalent. GAM with an Na2O equivalent of 4% demonstrates optimal wind and vibration resistance.

Related References:

1. Wang, T. T.; Chiu, Y. C.; and Li, K. J., “Index for Assessing Spalling in Tunnel Lining Based on Displacement Monitoring and Crack Mapping,” Tunnelling and Underground Space Technology, V. 153, 2024, p. 105975. doi: 10.1016/j.tust.2024.105975

2. Kalech, B.; Bouterra, M.; and ElCafsi, A., “Numerical Analysis of Smoke Flow Under the Effect of Longitudinal Airflow in a Tunnel Fire,” Fire and Materials, V. 44, No. 8, 2020, pp. 1033-1043. doi: 10.1002/fam.2902

3. Tomar, M. S., and Khurana, S., “Impact of Passive Fire Protection on Heat Release Rates in Road Tunnel Fire: A Review,” Tunnelling and Underground Space Technology, V. 85, 2019, pp. 149-159. doi: 10.1016/j.tust.2018.12.018

4. Lee, J.-S.; Woo, J.-H.; Shin, K.-J.; and Lee, H., “Evaluation of Fire-Resistance Performance for Modular Structures Based on Fireproof Coating Types,” Structures, V. 67, 2024, p. 107000. doi: 10.1016/j.istruc.2024.107000

5. Ma, X.; Pan, J.; Cai, J.; Zhang, Z.; and Han, J., “A Review on Cement-Based Materials used in Steel Structures as Fireproof Coating,” Construction and Building Materials, V. 315, 2022, p. 125623. doi: 10.1016/j.conbuildmat.2021.125623

6. Ali, A. E.; Faried, A. S.; and Osman, K. M., “Effect of Elevated Temperature on Properties of Concrete Containing Different Types of Nano-Materials,” Construction and Building Materials, V. 438, 2024, p. 136988. doi: 10.1016/j.conbuildmat.2024.136988

7. Amran, M.; Huang, S.-S.; Debbarma, S.; and Rashid, R. S. M., “Fire Resistance of Geopolymer Concrete: A Critical Review,” Construction and Building Materials, V. 324, 2022, p. 126722. doi: 10.1016/j.conbuildmat.2022.126722

8. Manzoor, T.; Bhat, J. A.; and Shah, A. H., “Performance of Geopolymer Concrete at Elevated Temperature – A Critical Review,” Construction and Building Materials, V. 420, 2024, p. 135578. doi: 10.1016/j.conbuildmat.2024.135578

9. Liu, Y.; Tan, K. H.; Du, Y.; Su, J.; Hu, X.; Mao, Y.; and Shi, C., “Comparison of Axial Behavior of RC Columns Using Alkali-Activated Slag-Based Concrete and OPC Concrete During and After Fire,” Journal of Building Engineering, V. 77, 2023, p. 107444. doi: 10.1016/j.jobe.2023.107444

10. Palizi, S., and Toufigh, V., “Fire-induced Damage Assessment of Cementless Alkali-Activated Slag-Based Concrete,” Construction and Building Materials, V. 393, 2023, p. 132002. doi: 10.1016/j.conbuildmat.2023.132002

11. Dener, M.; Karatas, M.; and Mohabbi, M., “High Temperature Resistance of Self Compacting Alkali Activated Slag/Portland Cement Composite using Lightweight Aggregate,” Construction and Building Materials, V. 290, 2021, p. 123250. doi: 10.1016/j.conbuildmat.2021.123250

12. Tran, V. A., and Nguyen, H. A., “Evaluation on Comprehensive Properties and Bonding Performance of Practical Slag-Fly Ash Blending Based Alkali-Activated Material,” Journal of Building Engineering, V. 62, 2022, p. 105350. doi: 10.1016/j.jobe.2022.105350

13. Manjunath, R.; Narasimhan, M. C.; Bhanu Prakash, G.; and Saipuspharaj, M., “Bond Strength Characteristics of High Strength Alkali Activated Slag Concrete Mixes,” Materials Today: Proceedings, 2023. doi: 10.1016/j.matpr.2023.05.573

14. Ye, H., and Radlińska, A., “Shrinkage Mechanisms of Alkali-Activated Slag,” Cement and Concrete Research, V. 88, 2016, pp. 126-135. doi: 10.1016/j.cemconres.2016.07.001

15. Huang, D.; Chen, P.; Peng, H.; Yang, Y.; Yuan, Q.; and Su, M., “A Review and Comparison Study on Drying Shrinkage Prediction Between Alkali-Activated Fly Ash/Slag and Ordinary Portland Cement,” Construction and Building Materials, V. 305, 2021, p. 124760. doi: 10.1016/j.conbuildmat.2021.124760

16. Boccarusso, L.; Capasso, I.; De Fazio, D.; Durante, M.; Lucolano, F.; and Langella, A., “Manufacturing and Mechanical Performance of Lightened Gypsum Reinforced by Hemp/Epoxy Composites,” Materials and Structures, V. 57, 2024.

17. Dima, C.; Badanoiu, A.; Cirstea, S.; Nicoara, A. I.; and Stoleriu, S., “Lightweight Gypsum Materials with Potential Use for Thermal Insulations,” Materials, V. 13, No. 23, 2020, p. 5454. doi: 10.3390/ma13235454

18. Hanjitsuwan, S.; Injorhor, B.; Phoo-Ngernkham, T.; Damrongwiriyanupap, N.; Li, L.-Y.; Sukontasukkul, P.; and Chindaprasirt, P., “Drying Shrinkage, Strength and Microstructure of Alkali-Activated High-Calcium Fly Ash Using FGD-Gypsum and Dolomite as Expansive Additive,” Cement and Concrete Composites, V. 114, 2020, p. 103760. doi: 10.1016/j.cemconcomp.2020.103760

19. Cho, B. S.; Koo, K. M.; and Choi, S. J., “Compressive Strength and Microstructure Properties of Alkali-Activated Systems with Blast Furnace Slag, Desulfurization Slag, and Gypsum,” Advances in Civil Engineering, V. 2018, No. 1, 2018, pp. 1-9. doi: 10.1155/2018/6123070

20. Zhu, G.; Zhu, W.; Qi, Z.; Yan, B.; Jiang, H.; and Hou, C., “One-part Alkali-Activated Slag Binder for Cemented Fine Tailings Backfill: Proportion Optimization and Properties Evaluation,” Environmental Science and Pollution Research International, V. 29, No. 49, 2022, pp. 73865-73877. doi: 10.1007/s11356-022-20331-w

21. Choi, S., and Lee, K. M., “Influence of Na2O Content and Ms (SiO2/Na2O) of Alkaline Activator on Workability and Setting of Alkali-Activated Slag Paste,” Materials, V. 12, No. 13, 2019, p. 2072. doi: 10.3390/ma12132072

22. Marvila, M. T.; Garcez De Azevedo, A. R.; Tostes Linhares Júnior, J. A.; and Fontes Vieira, C. M., “Activated Alkali Cement Based on Blast Furnace Slag: Effect of Curing Type And Concentration of Na2O,” Journal of Materials Research and Technology, V. 23, 2023, pp. 4551-4565. doi: 10.1016/j.jmrt.2023.02.088

23. Wang, L.; Si, C.; Li, C.; Sun, X.; Zhou, H.; and Guo, S., “Effect of Potassium Hydroxide-Sodium Water Glass Activator on Properties of Alkali-Activated Slag Cementitious Materials,” Bulletin of the Chinese Ceramic Society, V. 41, No. 8, 2022, pp. 2654-2662+2695. (in Chinese)

24. Langaro, E. A.; Costa De Moraes, M.; Buth, I. S.; Angulski da Luz, C.; Pereira Filho, J. I.; and Matoski, A., “Use of Slag (GBFS) Generated in Charcoal Blast Furnace as Raw Material in Alkali-Activated Cement,” Journal of Thermal Analysis and Calorimetry, V. 142, No. 3, 2020, pp. 1223-1231. doi: 10.1007/s10973-020-09632-9

25. Zhao, R.; Gao, X.; Gu, Q.; Fan, X.; Yang, T.; and Cheng, D., “Properties of Gypsum-Slag Cementitious Materials Modified by Alkali-Activators,” Concrete, V. 10, 2023, pp. 133-137. (in Chinese)

26. Zhuang, Y.; Liang, Y.; Chen, Y. F.; Ji, T.; and Ng, Z., “Bond Strength of Alkali-Activated Slag Based Tunnel Fireproof Coating Material,” Materialprüfung, V. 60, No. 12, 2018, pp. 1241-1248. doi: 10.3139/120.111274

27. Jin, G.; Ji, T.; and Lin, X., “Effect of Activators on Bonding Strength of Alkali-Activated Slag Tunnel Fireproof Coating,” Fire Science and Technology, V. 38, No. 7, 2019, pp. 994-997. (in Chinese)

28. GB/T 8074-2008, “Testing Method for Specific Surface of Cement-Blaine Method,” Standardization Administration of China, Beijing, China, 2008. (in Chinese)

29. Lu, G.; Ji, T.; Zhang, B.; Ma, Y.; and Liao, C., “Influence Factors and Prediction Model of Bond Strength of Tunnel Fireproof Coating under Freeze-Thaw Cycles,” Materials, V. 14, No. 6, 2021, p. 1544. doi: 10.3390/ma14061544

30. Zhang, J., and Scherer, G. W., “Comparison of Methods for Arresting Hydration of Cement,” Cement and Concrete Research, V. 41, No. 10, 2011, pp. 1024-1036. doi: 10.1016/j.cemconres.2011.06.003

31. Zoungrana, J. B.; Sorgho, B.; Bakouan, C.; Sawadogo, S.; Ouedraogo, R. D.; Guel, B.; and Blanchart, P., “Mineralogical Study of Phosphate Rocks by Quantitative Rietveld Refinement,” Open Ceramics, V. 18, 2024, p. 100567. doi: 10.1016/j.oceram.2024.100567

32. GB 14907-2018, “Fire Resistive Coating for Steel Structure,” Standardization Administration of China, Beijing, China, 2018. (in Chinese)

33. JT/T 1308-2020, “Tunnel Fire Resistive Coatings for Highway Engineering,” Standardization Administration of China, Beijing, China, 2020. (in Chinese)

34. GB 12441-2018, “Finishing Fire Resistant Coating,” Standardization Administration of China, Beijing, China, 2018. (in Chinese)

35. JC/T 626-2008, “Fiber Reinforced Low Alkalinity Cement Flat Sheets for Building,” Standardization Administration of China, Beijing, China, 2008. (in Chinese)

36. JG/T 24-2018, “Sand Textured Building Coating Based on Synthetic Resin Emulsion,” Standardization Administration of China, Beijing, China, 2018. (in Chinese)

37. T/CECS 901-2021, “Technical Specification for Application of Tunnel Fireproof Coatings,” Standardization Administration of China, Beijing, China, 2021. (in Chinese)

38. Wang, Q.; Sun, S.; Yao, G.; Wang, Z.; and Lyu, X., “Preparation and Characterization of an Alkali-Activated Cementitious Material with Blast-Furnace Slag, Soda Sludge, and Industrial Gypsum,” Construction and Building Materials, V. 340, 2022, p. 127735. doi: 10.1016/j.conbuildmat.2022.127735

39. Chen, J.; Jia, J.; and Zhu, M., “Understanding the Effect of Alkali Content on Hydration, Hardening, and Performance of Portland Cement – A Comprehensive Review,” Materials Today. Communications, V. 40, 2024, p. 109728. doi: 10.1016/j.mtcomm.2024.109728

40. Shi, D.; Zhang, W.; Ye, J.; and Sun, J., “Effects of Curing Condition on Properties, Reaction Products and Microstructure of Calcium Silicate Slag-Based Alkali-Activated Cementitious Materials,” Journal of the Chinese Ceramic Society, V. 45, No. 8, 2017, pp. 1080-1087.

41. Li, X.; Han, J.; Liu, Y.; Dou, Z.; and Zhang, T., “Summary of Research Progress on Industrial Flue Gas Desulfurization Technology,” Separation and Purification Technology, V. 281, 2022, p. 119849. doi: 10.1016/j.seppur.2021.119849

42. Song, H.; Jeong, Y.; Bae, S.; Jun, Y.; Yoon, S.; and Eun Oh, J., “A Study of Thermal Decomposition of Phases in Cementitious Systems Using HT-XRD and TG,” Construction and Building Materials, V. 169, 2018, pp. 648-661. doi: 10.1016/j.conbuildmat.2018.03.001

43. Scrivener, K.; Snellings, R.; and Lothenbach, B., A Practical Guide to Microstructural Analysis of Cementitious Materials, CRC Press, Boca Raton, FL, 2018.

44. Baquerizo, L. G.; Matschei, T.; and Scrivener, K. L., “Impact of Water Activity on the Stability of Ettringite,” Cement and Concrete Research, V. 79, 2016, pp. 31-44. doi: 10.1016/j.cemconres.2015.07.008

45. Masoudi, R., and Hooton, R. D., “Examining the Hydration Mechanism of Supersulfated Cements Made with High and Low-Alumina Slags,” Cement and Concrete Composites, V. 103, 2019, pp. 193-203. doi: 10.1016/j.cemconcomp.2019.05.001

46. Le Saoût, G.; Kocaba, V.; and Scrivener, K., “Application of the Rietveld Method to the Analysis of Anhydrous Cement,” Cement and Concrete Research, V. 41, No. 2, 2011, pp. 133-148. doi: 10.1016/j.cemconres.2010.10.003

47. Huang, G.; Pudasainee, D.; Gupta, R.; and Liu, W. V., “Thermal Properties of Calcium Sulfoaluminate Cement-Based Mortars Incorporated with Expanded Perlite Cured at Cold Temperatures,” Construction and Building Materials, V. 274, 2021, p. 122082. doi: 10.1016/j.conbuildmat.2020.122082

48. Chen, X.; Wu, Q.; Gao, J.; and Tang, Y., “Hydration Characteristics and Mechanism Analysis of β-Calcium Sulfate Hemihydrate,” Construction and Building Materials, V. 296, 2021, p. 123714. doi: 10.1016/j.conbuildmat.2021.123714

49. Sun, H.; Qian, J.; Yang, Y.; Fan, C.; and Yue, Y., “Optimization of Gypsum and Slag Contents in Blended Cement Containing Slag,” Cement and Concrete Composites, V. 112, 2020, p. 103674. doi: 10.1016/j.cemconcomp.2020.103674

50. Wu, Q.; Xue, Q.; and Yu, Z., “Research Status of Super Sulfate Cement,” Journal of Cleaner Production, V. 294, 2021, p. 126228. doi: 10.1016/j.jclepro.2021.126228

51. Yuan, B.; Yu, Q. L.; Dainese, E.; and Brouwers, H. J. H., “Autogenous and Drying Shrinkage of Sodium Carbonate Activated Slag Altered by Limestone Powder Incorporation,” Construction and Building Materials, V. 153, 2017, pp. 459-468. doi: 10.1016/j.conbuildmat.2017.07.112

52. Seo, J.; Kim, S.; Park, S.; Bae, S. J.; and Lee, H. K., “Microstructural Evolution and Carbonation Behavior of Lime-Slag Binary Binders,” Cement and Concrete Composites, V. 119, 2021, p. 104000. doi: 10.1016/j.cemconcomp.2021.104000

53. Li, Z.; Lu, T.; Liang, X.; Dong, H.; and Ye, G., “Mechanisms of Autogenous Shrinkage of Alkali-Activated Slag and Fly Ash Pastes,” Cement and Concrete Research, V. 135, 2020, p. 106107. doi: 10.1016/j.cemconres.2020.106107

54. Sumirat, I.; Ando, Y.; and Shimamura, S., “Theoretical Consideration of the Effect of Porosity on Thermal Conductivity of Porous Materials,” Journal of Porous Materials, V. 13, No. 3-4, 2006, pp. 439-443. doi: 10.1007/s10934-006-8043-0

55. Liu, N.; Peng, L.; and Shi, C., “Experimental Study on Influence of Tunnel Bed Stiffness to Fatigue Damage Characteristics of Invert Concrete,” Journal of Huazhong University of Science and Technology (Natural Science Edition), V. 44, No. 12, 2016, pp. 31-37.


ALSO AVAILABLE IN:

Electronic Materials Journal