Effects of Different Fibers and Cement Substituting Minerals on Mechanical Properties of Ultra-High- Performance Fiber-Reinforced Concrete

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effects of Different Fibers and Cement Substituting Minerals on Mechanical Properties of Ultra-High- Performance Fiber-Reinforced Concrete

Author(s): Nima Mohammadian Tabrizi, Davood Mostofinejad, and Mohammad Reza Eftekhar

Publication: Materials Journal

Volume: 120

Issue: 5

Appears on pages(s): 15-30

Keywords: cement replacement materials; curing; mechanical properties; synthetic fiber; ultra-high-performance concrete (UHPC)

DOI: 10.14359/51738888

Date: 9/1/2023

Abstract:
This paper is aimed at investigating the effects of different fiber inclusion on the mechanical properties of ultra-high-performance concrete (UHPC) by adding mineral admixtures as cement replacement materials to reduce production costs and CO2 emissions of UHPC. Throughout this research, 21 mixture designs containing four cement substitution materials (silica fume, slag cement, limestone powder, and quartz powder) and three fibers (steel, synthetic macrofibers, and polypropylene) under wet and combined (autoclave, oven, and water) curing were developed. To investigate the mechanical properties in this research, a total of 336 specimens were cast to evaluate compressive strength, the modulus of rupture (MOR), and the toughness index. The findings revealed that at the combined curing, regarded as a new procedure, all levels of cement replacement recorded a compressive strength higher than 150 MPa (21.76 ksi). Furthermore, the mechanical properties of the mixture design containing microsilica and slag (up to 15%) were found to be higher than other cement substitutes. Also, it was shown that all levels of the fiber presented the MOR significantly close together, and samples made of synthetic macrofibers and steel fibers exhibited deflection-hardening behavior after cracking. The mixture design containing microsilica, slag, limestone powder, and quartzpowder, despite the significant replacement of cement (approximately 50%) by substitution materials, experienced a slight drop in strength. Therefore, the development of this mixture is optimal both economically and environmentally.

Related References:

1. Fehling, E.; Schmidt, M.; Walraven, J.; Leutbecher, T.; and Fröhlich, S., Ultra-High Performance Concrete UHPC: Fundamentals, Design, Examples, John Wiley & Sons, Inc., New York, NY, 2015, 198 pp.

2. Kim, S.-K.; Kim, W.; and Han, S.-M., “Behavior Evaluation of Ultrahigh-Performance Concrete Beam Containing Para-Aramid Fibers,” Advances in Civil Engineering, V. 2019, 2019, Article No. 5187630, 17 pp. doi: 10.1155/2019/5187630

3. Kang, S.-T.; Lee, Y.; Park, Y.-D.; and Kim, J.-K., “Tensile Fracture Properties of an Ultra High Performance Fiber Reinforced Concrete (UHPFRC) With Steel Fiber,” Composite Structures, V. 92, No. 1, Jan. 2010, pp. 61-71. doi: 10.1016/j.compstruct.2009.06.012

4. Schmidt, M., and Fehling, E., “Ultra-High-Performance Concrete: Research, Development and Application in Europe,” Seventh International Symposium on the Utilization of High-Strength/High-Performance Concrete, SP-228, American Concrete Institute, Farmington Hills, MI, 2005, pp. 51-78.

5. Habel, K.; Denarié, E.; and Brühwiler, E., “Time Dependent Behavior of Elements Combining Ultra-High Performance Fiber Reinforced Concretes (UHPFRC) and Reinforced Concrete,” Materials and Structures, V. 39, No. 5, June 2006, pp. 557-569. doi: 10.1007/s11527-005-9045-0

6. Habert, G.; Denarié, E.; Šajna, A.; and Rossi, P., “Lowering the Global Warming Impact of Bridge Rehabilitations by Using Ultra High Performance Fibre Reinforced Concretes,” Cement and Concrete Composites, V. 38, Apr. 2013, pp. 1-11. doi: 10.1016/j.cemconcomp.2012.11.008

7. Friedlingstein, P.; Houghton, R. A.; Marland, G.; Hackler, J.; Boden, T. A.; Conway, T. J.; Canadell, J. G.; Raupach, M. R.; Ciais, P.; and Le Quéré, C., “Update on CO2 Emissions,” Nature Geoscience, V. 3, No. 12, Dec. 2010, pp. 811-812. doi: 10.1038/ngeo1022

8. Korpa, A.; Kowald, T.; and Trettin, R., “Phase Development in Normal and Ultra High Performance Cementitious Systems by Quantitative X-Ray Analysis and Thermoanalytical Methods,” Cement and Concrete Research, V. 39, No. 2, Feb. 2009, pp. 69-76. doi: 10.1016/j.cemconres.2008.11.003

9. Huang, W.; Kazemi-Kamyab, H.; Sun, W.; and Scrivener, K., “Effect of Replacement of Silica Fume with Calcined Clay on the Hydration and Microstructural Development of Eco-UHPFRC,” Materials & Design, V. 121, May 2017, pp. 36-46. doi: 10.1016/j.matdes.2017.02.052

10. Bahmani, H., and Mostofinejad, D., “Microstructure of Ultra-High-Performance Concrete (UHPC)—A Review Study,” Journal of Building Engineering, V. 50, June 2022, Article No. 104118. doi: 10.1016/j.jobe.2022.104118

11. Randl, N.; Steiner, T.; Ofner, S.; Baumgartner, E.; and Mészöly, T., “Development of UHPC Mixtures from an Ecological Point of View,” Construction and Building Materials, V. 67, Part C, Sept. 2014, pp. 373-378. doi: 10.1016/j.conbuildmat.2013.12.102

12. Ganesh, P., and Murthy, A. R., “Tensile Behaviour and Durability Aspects of Sustainable Ultra-High Performance Concrete Incorporated with GGBS as Cementitious Material,” Construction and Building Materials, V. 197, Feb. 2019, pp. 667-680. doi: 10.1016/j.conbuildmat.2018.11.240

13. Bahmani, H.; Mostofinejad, D.; and Dadvar, S. A., “Fiber Type and Curing Environment Effects on the Mechanical Performance of UHPFRC Containing Zeolite,” Iranian Journal of Science and Technology, Transactions of Civil Engineering, V. 46, No. 6, Dec. 2022, pp. 4151-4167. doi: 10.1007/s40996-022-00911-z

14. Kim, H.; Koh, T.; and Pyo, S., “Enhancing Flowability and Sustainability of Ultra High Performance Concrete Incorporating High Replacement Levels of Industrial Slags,” Construction and Building Materials, V. 123, Oct. 2016, pp. 153-160. doi: 10.1016/j.conbuildmat.2016.06.134

15. Abdulkareem, O. M.; Ben Fraj, A.; Bouasker, M.; and Khelidj, A., “Mixture Design and Early Age Investigations of More Sustainable UHPC,” Construction and Building Materials, V. 163, Feb. 2018, pp. 235-246. doi: 10.1016/j.conbuildmat.2017.12.107

16. Huang, W.; Kazemi-Kamyab, H.; Sun, W.; and Scrivener, K., “Effect of Cement Substitution by Limestone on the Hydration and Microstructural Development of Ultra-High Performance Concrete (UHPC),” Cement and Concrete Composites, V. 77, Mar. 2017, pp. 86-101. doi: 10.1016/j.cemconcomp.2016.12.009

17. Yu, R.; Tang, P.; Spiesz, P.; and Brouwers, H. J. H., “A Study of Multiple Effects of Nano-Silica and Hybrid Fibres on the Properties of Ultra-High Performance Fibre Reinforced Concrete (UHPFRC) Incorporating Waste Bottom Ash (WBA),” Construction and Building Materials, V. 60, June 2014, pp. 98-110. doi: 10.1016/j.conbuildmat.2014.02.059

18. Pourbaba, M.; Asefi, E.; Sadaghian, H.; and Mirmiran, A., “Effect of Age on the Compressive Strength of Ultra-High-Performance Fiber-Reinforced Concrete,” Construction and Building Materials, V. 175, June 2018, pp. 402-410. doi: 10.1016/j.conbuildmat.2018.04.203

19. Ghasemzadeh Mosavinejad, S. H.; Langaroudi, M. A. M.; Barandoust, J.; and Ghanizadeh, A., “Electrical and Microstructural Analysis of UHPC Containing Short PVA Fibers,” Construction and Building Materials, V. 235, Feb. 2020, Article No. 117448. doi: 10.1016/j.conbuildmat.2019.117448

20. Mostofinejad, D.; Moosaie, I.; Eftekhar, M.; and Hesami, E., “Ultra-High Performance Hybrid Polyvinyl Alcohol-Polypropylene Fiber-Reinforced Cementitious Composites with Augmented Toughness and Strain-Hardening Behavior,” Iranian Journal of Science and Technology, Transactions of Civil Engineering, V. 46, No. 3, June 2022, pp. 1997-2009. doi: 10.1007/s40996-021-00815-4

21. Yoo, D.-Y.; Shin, H.-O.; Yang, J.-M.; and Yoon, Y.-S., “Material and Bond Properties of Ultra High Performance Fiber Reinforced Concrete with Micro Steel Fibers,” Composites Part B: Engineering, V. 58, Mar. 2014, pp. 122-133. doi: 10.1016/j.compositesb.2013.10.081

22. Meng, W., and Khayat, K. H., “Effect of Hybrid Fibers on Fresh Properties, Mechanical Properties, and Autogenous Shrinkage of Cost-Effective UHPC,” Journal of Materials in Civil Engineering, ASCE, V. 30, No. 4, Apr. 2018, p. 04018030. doi: 10.1061/(ASCE)MT.1943-5533.0002212

23. Chun, B., and Yoo, D.-Y., “Hybrid Effect of Macro and Micro Steel Fibers on the Pullout and Tensile Behaviors of Ultra-High-Performance Concrete,” Composites Part B: Engineering, V. 162, Apr. 2019, pp. 344-360. doi: 10.1016/j.compositesb.2018.11.026

24. Bahmani, H.; Mostofinejad, D.; and Dadvar, S. A., “Effects of Synthetic Fibers and Different Levels of Partial Cement Replacement on Mechanical Properties of UHPFRC,” Journal of Materials in Civil Engineering, ASCE, V. 32, No. 12, Dec. 2020, p. 04020361. doi: 10.1061/(ASCE)MT.1943-5533.0003462

25. Bahmani, H.; Mostofinejad, D.; and Dadvar, S. A., “Mechanical Properties of Ultra-High-Performance Fiber-Reinforced Concrete Containing Synthetic and Mineral Fibers,” ACI Materials Journal, V. 117, No. 3, May 2020, pp. 155-168. doi: 10.14359/51724596

26. ASTM C150/C150M-16, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2016, 10 pp.

27. ASTM C1240-15, “Standard Specification for Silica Fume Used in Cementitious Mixtures,��� ASTM International, West Conshohocken, PA, 2015, 7 pp.

28. ASTM C494/C494M-05a, “Standard Specification for Chemical Admixtures for Concrete,” ASTM International, West Conshohocken, PA, 2005, 10 pp.

29. Mostofinejad, D.; Nikoo, M. R.; and Hosseini, S. A., “Determination of Optimized Mix Design and Curing Conditions of Reactive Powder Concrete (RPC),” Construction and Building Materials, V. 123, Oct. 2016, pp. 754-767. doi: 10.1016/j.conbuildmat.2016.07.082

30. ASTM C1437-13, “Standard Test Method for Flow of Hydraulic Cement Mortar,” ASTM International, West Conshohocken, PA, 2013, 2 pp.

31. Habel, K., and Gauvreau, P., “Response of Ultra-High Performance Fiber Reinforced Concrete (UHPFRC) to Impact and Static Loading,” Cement and Concrete Composites, V. 30, No. 10, Nov. 2008, pp. 938-946. doi: 10.1016/j.cemconcomp.2008.09.001

32. Máca, P.; Sovják, R.; and Konvalinka, P., “Mix Design of UHPFRC and Its Response to Projectile Impact,” International Journal of Impact Engineering, V. 63, Jan. 2014, pp. 158-163. doi: 10.1016/j.ijimpeng.2013.08.003

33. ASTM C109/C109M-11b, “Standard Test Method for Compressive Strength of Hydraulic Cement Mortars (Using 2-in. or [50-mm] Cube Specimens),” ASTM International, West Consohocken, PA, 2011, 10 pp.

34. ASTM C78/C78M-10, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2010, 4 pp.

35. Yu, R.; Spiesz, P.; and Brouwers, H. J. H., “Development of an Eco-Friendly Ultra-High Performance Concrete (UHPC) with Efficient Cement and Mineral Admixtures Uses,” Cement and Concrete Composites, V. 55, Jan. 2015, pp. 383-394. doi: 10.1016/j.cemconcomp.2014.09.024

36. Gupta, S., “Effect of Content and Fineness of Slag as High Volume Cement Replacement on Strength and Durability of Ultra-High Performance Mortar,” Journal of Building Materials and Structures, V. 3, No. 2, 2016, pp. 43-54. doi: 10.34118/jbms.v3i2.23

37. Chidiac, S. E., and Panesar, D. K., “Evolution of Mechanical Properties of Concrete Containing Ground Granulated Blast Furnace Slag and Effects on the Scaling Resistance Test at 28 Days,” Cement and Concrete Composites, V. 30, No. 2, Feb. 2008, pp. 63-71. doi: 10.1016/j.cemconcomp.2007.09.003

38. Kang, S.-H.; Jeong, Y.; Tan, K. H.; and Moon, J., “High-Volume Use of Limestone in Ultra-High Performance Fiber-Reinforced Concrete for Reducing Cement Content and Autogenous Shrinkage,” Construction and Building Materials, V. 213, July 2019, pp. 292-305. doi: 10.1016/j.conbuildmat.2019.04.091

39. Liu, S.-H., and Yan, P., “Influence of Limestone Powder on Filling Effect of Cement Paste and Pore Structure of Sand Grout,” Journal of the Chinese Ceramic Society, V. 36, No. 1, 2008, pp. 69-72, 77.

40. Haddad, R. H.; Al-Saleh, R. J.; and Al-Akhras, N. M., “Effect of Elevated Temperature on Bond between Steel Reinforcement and Fiber Reinforced Concrete,” Fire Safety Journal, V. 43, No. 5, July 2008, pp. 334-343. doi: 10.1016/j.firesaf.2007.11.002

41. Abdallah, S.; Fan, M.; and Cashell, K. A., “Bond-Slip Behaviour of Steel Fibres in Concrete after Exposure to Elevated Temperatures,” Construction and Building Materials, V. 140, June 2017, pp. 542-551. doi: 10.1016/j.conbuildmat.2017.02.148

42. ASTM C1018-97, “Standard Test Method for Flexural Toughness and First-Crack Strength of Fiber-Reinforced Concrete (Using Beam With Third-Point Loading) (Withdrawn 2006),” ASTM International, West Conshohocken, PA, 1997, 7 pp.

43. Kuruşcu, A. O., and Girgin, Z. C., “Efficiency of Structural Materials in Sustainable Design,” Journal of Civil Engineering and Architecture, V. 8, No. 10, Oct. 2014, pp. 1260-1265.

44. Long, G.; Gao, Y.; and Xie, Y., “Designing More Sustainable and Greener Self-Compacting Concrete,” Construction and Building Materials, V. 84, June 2015, pp. 301-306. doi: 10.1016/j.conbuildmat.2015.02.072

45. Turner, L. K., and Collins, F. G., “Carbon Dioxide Equivalent (CO2-e) Emissions: A Comparison between Geopolymer and OPC Cement Concrete,” Construction and Building Materials, V. 43, June 2013, pp. 125-130. doi: 10.1016/j.conbuildmat.2013.01.023


ALSO AVAILABLE IN:

Electronic Materials Journal



  

Edit Module Settings to define Page Content Reviewer