Title: Industry Works Toward Reducing Embodied Carbon

Author(s):

Publication: Concrete International

Volume: 45

Issue: 5

Appears on pages(s): 54-55

Keywords: concrete, mixture, performance, clinker

DOI:

Date: 5/1/2023

Abstract:
Pilot research programs are being conducted to develop commercially viable options that can potentially impact the carbon footprint of concrete industry. The article discusses two such programs: developing a high-performance, graphene-enhanced cement and creating a software for optimizing concrete mixtures based on historical data on materials and mixture performance.




  