Selecting Exposure Classes and Requirements for Durability

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Selecting Exposure Classes and Requirements for Durability

Author(s): Karthik H. Obla and Colin L. Lobo

Publication: Concrete International

Volume: 45

Issue: 5

Appears on pages(s): 43-52

Keywords: freezing, sulfate, water, corrosion

DOI: 10.14359/51738797

Date: 5/1/2023

Abstract:
Project specifications may be overly conservative or not applicable to the project’s exposure conditions. The article provides guidance for designers on how to generate concrete specifications that minimize environmental impacts and result in durable structures using prescriptive- or performance-based durability approach and provides two case examples.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI CODE-318-19(22)) and Commentary (Reapproved 2022),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

2. ACI Committee 301, “Specifications for Concrete Construction (ACI SPEC-301-20),” American Concrete Institute, Farmington Hills, MI, 2020, 69 pp.

3. “Resources for Selecting Durability Exposure Classes and Concrete Requirements,” National Ready Mixed Concrete Association, Alexandria, VA, www.nrmca.org/association-resources/research-and-engineering/p2p/durability-exposure-classes/ (last accessed, Mar. 28, 2023)

4. ASTM C618-22, “Standard Specification for Coal Fly Ash and Raw or Calcined Natural Pozzolan for Use in Concrete,” ASTM International, West Conshohocken, PA, 2022, 5 pp.

5. ASTM C989/C989M-22, “Standard Specification for Slag Cement for Use in Concrete and Mortars,” ASTM International, West Conshohocken, PA, 2022, 7 pp.

6. ASTM C1240-20, “Standard Specification for Silica Fume Used in Cementitious Mixtures,” ASTM International, West Conshohocken, PA, 2020, 7 pp.

7. ASTM C1580-20, “Standard Test Method for Water-Soluble Sulfate in Soil,” ASTM International, West Conshohocken, PA, 2020, 4 pp.

8. ASTM D516-16, “Standard Test Method for Sulfate Ion in Water,” ASTM International, West Conshohocken, PA, 2016, 5 pp.

9. ASTM D4130-15, “Standard Test Method for Sulfate Ion in Brackish Water, Seawater, and Brines,” ASTM International, West Conshohocken, PA, 2015, 5 pp.

10. ASTM C150/C150M-22, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2022, 9 pp.

11. ASTM C595/C595M-21, “Standard Specification for Blended Hydraulic Cements,” ASTM International, West Conshohocken, PA, 2021, 10 pp.

12. ASTM C1157/C1157M-20a, “Standard Performance Specification for Hydraulic Cement,” ASTM International, West Conshohocken, PA, 2020, 5 pp.

13. ASTM C1012/C1012M-18b, “Standard Test Method for Length Change of Hydraulic-Cement Mortars Exposed to a Sulfate Solution,” ASTM International, West Conshohocken, PA, 2018, 9 pp.

14. ASTM C1778-22, “Standard Guide for Reducing the Risk of Deleterious Alkali-Aggregate Reaction in Concrete,” ASTM International, West Conshohocken, PA, 2022, 13 pp.

15. “MasterSpec®,” The American Institute of Architects, Washington, DC.

16. ASTM C1293-20a, “Standard Test Method for Determination of Length Change of Concrete Due to Alkali-Silica Reaction,” ASTM International, West Conshohocken, PA, 2020, 6 pp.

17. ASTM C1567-22, “Standard Test Method for Determining the Potential Alkali-Silica Reactivity of Combinations of Cementitious Materials and Aggregate (Accelerated Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2022, 6 pp.

18. ASTM C1260-22, “Standard Test Method for Potential Alkali Reactivity of Aggregates (Mortar-Bar Method),” ASTM International, West Conshohocken, PA, 2022, 5 pp.

19. ASTM C1218/C1218M-20, “Standard Test Method for Water-Soluble Chloride in Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2020, 3 pp.

20. ASTM C1202-22e1, “Standard Test Method for Electrical Indication of Concrete’s Ability to Resist Chloride Ion Penetration,” ASTM International, West Conshohocken, PA, 2022, 8 pp.

21. ASTM C1876-19, “Standard Test Method for Bulk Electrical Resistivity or Bulk Conductivity of Concrete,” ASTM International, West Conshohocken, PA, 2019, 7 pp.

22. Obla, K.H., and Lobo, C.L., “Acceptance Criteria for Durability Tests,” Concrete International, V. 29, No. 5, May 2007, pp. 43-48.

23. ASTM C157/C157M-17, “Standard Test Method for Length Change of Hardened Hydraulic-Cement Mortar and Concrete,” ASTM International, West Conshohocken, PA, 2017, 8 pp.

24. ASTM C192/C192M-19, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2019, 8 pp.

25. ASTM C469/C469M-22, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2022, 6 pp.

26. ASTM C567/C567M-19, “Standard Test Method for Determining Density of Structural Lightweight Concrete,” ASTM International, West Conshohocken, PA, 2019, 4 pp.

27. ACI Committee 308, “Guide to External Curing of Concrete (ACI 308R-16),” American Concrete Institute, Farmington Hills, MI, 2016, 36 pp.

28. ASTM C143/C143M-20, “Standard Test Method for Slump of Hydraulic-Cement Concrete,” ASTM International, West Conshohocken, PA, 2020, 4 pp.

29. ASTM C1611/C1611M-21, “Standard Test Method for Slump Flow of Self-Consolidating Concrete,” ASTM International, West Conshohocken, PA, 2021, 6 pp.

30. ASTM C94/C94M-22a, “Standard Specification for Ready-Mixed Concrete,” ASTM International, West Conshohocken, PA, 2022, 16 pp.

31. ASTM C672/C672M-12, “Standard Test Method for Scaling Resistance of Concrete Surfaces Exposed to Deicing Chemicals (Withdrawn 2021),” ASTM International, West Conshohocken, PA, 2012, 3 pp.

32. “Guide to Improving Specifications for Ready Mixed Concrete,” NRMCA Publication 2PE004-21, National Ready Mixed Concrete Association, Alexandria, VA, 2021, 37 pp.