High-Temperature Behavior of Lightweight Aggregate Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: High-Temperature Behavior of Lightweight Aggregate Reinforced Concrete Beams

Author(s): F. Dabbaghi, A. Tanhadoust, M. L. Nehdi, M. Dehestani, H. Yousefpour, and H.-T. Thai

Publication: Materials Journal

Volume: 119

Issue: 5

Appears on pages(s): 199-212

Keywords: finite element analysis; flexural capacity; lightweight aggregate; post-fire response; reinforced concrete; residual strength; stress-strain relationship

DOI: 10.14359/51736093

Date: 9/1/2022

Abstract:
Structural lightweight-aggregate concrete (LWAC) has gained a broad range of applications in the construction industry owing to its reduced dead load and enhanced fire resistance. In this study, the potential of using lightweight expanded clay aggregates as a partial replacement for fine and coarse natural aggregates was experimentally and numerically examined. Testing was performed on cylindrical specimens made of normalweight and lightweight concrete incorporating microsilica as a partial replacement for cement to determine the associated stress-strain behavior. Subsequently, three-point bending testing was conducted on reinforced concrete beams to evaluate their structural behavior. Four levels of temperature were considered: 25°C (ambient temperature), and 250, 500, and 750°C (elevated temperatures). The finite element method through Abaqus software was deployed to numerically investigate the behavior at elevated temperatures through a comprehensive parametric study. The experimental and numerical results indicate that under high-temperature exposure, LWAC outperforms its normal counterpart in terms of strength, stiffness, and Young’s modulus. It is also noticeable that LWAC beams retained their load-bearing capacity better than normal weight aggregate concrete (NWAC) after reaching the peak load.

Related References:

1. Dabbaghi, F.; Tanhadoust, A.; Nehdi, M. L.; Nasrollahpour, S.; Dehestani, M.; and Yousefpour, H., “Life Cycle Assessment Multi-Objective Optimization and Deep Belief Network Model for Sustainable Lightweight Aggregate Concrete,” Journal of Cleaner Production, V. 318, Oct. 2021, Article No. 128554. doi: 10.1016/j.jclepro.2021.128554

2. Karimaei, M.; Dabbaghi, F.; Dehestani, M.; and Rashidi, M., “Estimating Compressive Strength of Concrete Containing Untreated Coal Waste Aggregates Using Ultrasonic Pulse Velocity,” Materials (Basel), V. 14, No. 3, Feb. 2021, Article No. 647. doi: 10.3390/ma14030647

3. Othuman, M. A., and Wang, Y. C., “Elevated-Temperature Thermal Properties of Lightweight Foamed Concrete,” Construction and Building Materials, V. 25, No. 2, Feb. 2011, pp. 705-716. doi: 10.1016/j.conbuildmat.2010.07.016

4. Karimaei, M.; Dabbaghi, F.; Sadeghi-Nik, A.; and Dehestani, M., “Mechanical Performance of Green Concrete Produced with Untreated Coal Waste Aggregates,” Construction and Building Materials, V. 233, Feb. 2020, Article No. 117264. doi: 10.1016/j.conbuildmat.2019.117264

5. ACI Committee 213, “Guide for Structural Lightweight-Aggregate Concrete (ACI 213R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 53 pp.

6. Deifalla, A.; Awad, A.; Seleem, H.; and Abdelrahman, A., “Investigating the Behavior of Lightweight Foamed Concrete T-Beams under Torsion, Shear, and Flexure,” Engineering Structures, V. 219, Sept. 2020, Article No. 110741. doi: 10.1016/j.engstruct.2020.110741

7. Dabbaghi, F.; Fallahnejad, H.; Nasrollahpour, S.; Dehestani, M.; and Yousefpour, H., “Evaluation of Fracture Energy, Toughness, Brittleness, and Fracture Process Zone Properties for Lightweight Concrete Exposed to High Temperatures,” Theoretical and Applied Fracture Mechanics, V. 116, Dec. 2021, Article No. 103088. doi: 10.1016/j.tafmec.2021.103088

8. Dabbaghi, F.; Nasrollahpour, S.; Dehestani, M.; and Yousefpour, H., “Optimization of Concrete Mixtures Containing Lightweight Expanded Clay Aggregates Based on Mechanical, Economical, Fire-Resistance, and Environmental Considerations,” Journal of Materials in Civil Engineering, ASCE, V. 34, No. 2, Feb. 2022, p. 04021445.

9. Dabbaghi, F.; Dehestani, M.; and Yousefpour, H., “Residual Mechanical Properties of Concrete Containing Lightweight Expanded Clay Aggregate (LECA) after Exposure to Elevated Temperatures,” Structural Concrete, 2021. doi: 10.1002/suco.202000821

10. Callister Jr., W. D., Materials Science and Engineering: An Introduction, fifth edition, John Wiley & Sons, Inc., New York, 2003.

11. Leet, K.; Uang, C.-M.; and Lanning, J., Fundamentals of Structural Analysis, sixth edition, McGraw Hill Education, New York, 2021.

12. ASTM C39/C39M-21, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2021, 8 pp.

13. ASTM C873/C873M-15, “Standard Test Method for Compressive Strength of Concrete Cylinders Cast in Place in Cylindrical Molds,” ASTM International, West Conshohocken, PA, 2015, 4 pp.

14. ASTM C78/C78M-18, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2018, 5 pp.

15. Dabbaghi, F.; Rashidi, M.; Nehdi, M. L.; Sadeghi, H.; Karimaei, M.; Rasekh, H.; and Qaderi, F., “Experimental and Informational Modeling Study on Flexural Strength of Eco-Friendly Concrete Incorporating Coal Waste,” Sustainability, V. 13, No. 13, July 2021, Article No. 7506. doi: 10.3390/su13137506

16. ASTM C1161-18, “Standard Test Method for Flexural Strength of Advanced Ceramics at Ambient Temperature,” ASTM International, West Conshohocken, PA, 2018, 19 pp.

17. Aluko, O. G.; Yatim, J. M.; Kadir, M. A. A.; and Yahya, K., “A Review of Properties of Bio-Fibrous Concrete Exposed to Elevated Temperatures,” Construction and Building Materials, V. 260, Nov. 2020, Article No. 119671. doi: 10.1016/j.conbuildmat.2020.119671

18. Saridemir, M.; Severcan, M. H.; Ciflikli, M.; Celikten, S.; Ozcan, F.; and Atis, C. D., “The Influence of Elevated Temperature on Strength and Microstructure of High Strength Concrete Containing Ground Pumice and Metakaolin,” Construction and Building Materials, V. 124, Oct. 2016, pp. 244-257. doi: 10.1016/j.conbuildmat.2016.07.109

19. Sukontasukkul, P.; Pomchiengpin, W.; and Songpiriyakij, S., “Post-Crack (or Post-Peak) Flexural Response and Toughness of Fiber Reinforced Concrete after Exposure to High Temperature,” Construction and Building Materials, V. 24, No. 10, Oct. 2010, pp. 1967-1974. doi: 10.1016/j.conbuildmat.2010.04.003

20. Real, S.; Gomes, M. G.; Moret Rodrigues, A.; and Bogas, J. A., “Contribution of Structural Lightweight Aggregate Concrete to the Reduction of Thermal Bridging Effect in Buildings,” Construction and Building Materials, V. 121, Sept. 2016, pp. 460-470. doi: 10.1016/j.conbuildmat.2016.06.018

21. Ahmad, M. R.; Chen, B.; and Shah, S. F. A., “Investigate the Influence of Expanded Clay Aggregate and Silica Fume on the Properties of Lightweight Concrete,” Construction and Building Materials, V. 220, Sept. 2019, pp. 253-266. doi: 10.1016/j.conbuildmat.2019.05.171

22. Dabbaghi, F.; Sadeghi-Nik, A.; Libre, N. A.; and Nasrollahpour, S., “Characterizing Fiber Reinforced Concrete Incorporating Zeolite and Metakaolin as Natural Pozzolans,” Structures, V. 34, Dec. 2021, pp. 2617-2627. doi: 10.1016/j.istruc.2021.09.02510.1016/j.istruc.2021.09.025

23. Amiri, H.; Azadi, S.; Karimaei, M.; Sadeghi, H.; and Dabbaghi, F., “Multi-Objective Optimization of Coal Waste Recycling in Concrete Using Response Surface Methodology,” Journal of Building Engineering, V. 45, Jan. 2022, Article No. 103472. doi: 10.1016/j.jobe.2021.103472

24. Lo, T. Y.; Tang, W. C.; and Nadeem, A., “Comparison of Carbonation of Lightweight Concrete with Normal Weight Concrete at Similar Strength Levels,” Construction and Building Materials, V. 22, No. 8, Aug. 2008, pp. 1648-1655. doi: 10.1016/j.conbuildmat.2007.06.006

25. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

26. Park, R., and Paulay, T., Reinforced Concrete Structures, John Wiley & Sons, Inc., New York, 1975.

27. Xu, L.; Ma, M.; Li, L.; Xiong, Y.; and Liu, W., “Continuum-Based Approach for Modelling the Flexural Behaviour of Plain Concrete Beam under High-Cycle Fatigue Loads,” Engineering Structures, V. 241, Aug. 2021, Article No. 112442. doi: 10.1016/j.engstruct.2021.112442

28. Nicolaides, D., and Markou, G., “Modelling the Flexural Behaviour of Fibre Reinforced Concrete Beams with FEM,” Engineering Structures, V. 99, Sept. 2015, pp. 653-665. doi: 10.1016/j.engstruct.2015.05.028

29. Esfahani, M.; Hoseinzade, M.; Shakiba, M.; Arbab, F.; Yekrangnia, M.; and Pachideh, G., “Experimental Investigation of Residual Flexural Capacity of Damaged Reinforced Concrete Beams Exposed to Elevated Temperatures,” Engineering Structures, V. 240, Aug. 2021, Article No. 112388. doi: 10.1016/j.engstruct.2021.112388

30. Khodabakhshian, A.; de Brito, J.; Ghalehnovi, M.; and Asadi Shamsabadi, E., “Mechanical, Environmental and Economic Performance of Structural Concrete Containing Silica Fume and Marble Industry Waste Powder,” Construction and Building Materials, V. 169, Apr. 2018, pp. 237-251. doi: 10.1016/j.conbuildmat.2018.02.192

31. Siddique, R., “Utilization of Silica Fume in Concrete: Review of Hardened Properties,” Resources, Conservation and Recycling, V. 55, No. 11, Sept. 2011, pp. 923-932.

32. Dabbaghi, F.; Dehestani, M.; Yousefpour, H.; Rasekh, H.; and Navaratnam, S., “Residual Compressive Stress–Strain Relationship of Lightweight Aggregate Concrete after Exposure to Elevated Temperatures,” Construction and Building Materials, V. 298, Sept. 2021, Article No. 123890. doi: 10.1016/j.conbuildmat.2021.123890

33. Zheng, W.; Li, H.; and Wang, Y., “Compressive Stress–Strain Relationship of Steel Fiber-Reinforced Reactive Powder Concrete after Exposure to Elevated Temperatures,” Construction and Building Materials, V. 35, Oct. 2012, pp. 931-940. doi: 10.1016/j.conbuildmat.2012.05.031

34. ASTM C150/C150M-12, “Standard Specification for Portland Cement,” ASTM International, West Conshohocken, PA, 2012, 9 pp.

35. ASTM C33-03, “Standard Specification for Concrete Aggregates,” ASTM International, West Conshohocken, PA, 2003, 11 pp.

36. ASTM C127-04, “Standard Test Method for Density, Relative Density (Specific Gravity), and Absorption of Coarse Aggregate,” ASTM International, West Conshohocken, PA, 2004, 6 pp.

37. ASTM C192/C192M-02, “Standard Practice for Making and Curing Concrete Test Specimens in the Laboratory,” ASTM International, West Conshohocken, PA, 2002, 8 pp.

38. Arel, H. Ş., and Shaikh, F. U. A., “Effects of Silica Fume Fineness on Mechanical Properties of Steel Fiber Reinforced Lightweight Concretes Subjected to Ambient and Elevated Temperatures Exposure,” Structural Concrete, V. 19, No. 6, Dec. 2018, pp. 1829-1837. doi: 10.1002/suco.201700281

39. Bingöl, A. F., and Gül, R., “Compressive Strength of Lightweight Aggregate Concrete Exposed to High Temperatures,” Indian Journal of Engineering and Materials Sciences, V. 11, Feb. 2004, pp. 68-72.

40. Nematzadeh, M.; Tayebi, M.; and Samadvand, H., “Prediction of Ultrasonic Pulse Velocity in Steel Fiber-Reinforced Concrete Containing Nylon Granule and Natural Zeolite after Exposure to Elevated Temperatures,” Construction and Building Materials, V. 273, Mar. 2021, Article No. 121958. doi: 10.1016/j.conbuildmat.2020.121958

41. Dehghani, A.; Mozafari, A. R.; and Aslani, F., “Evaluation of the Efficacy of Using Engineered Cementitious Composites in RC Beam-Column Joints,” Structures, V. 27, Oct. 2020, pp. 151-162.

42. Yapar, O.; Basu, P. K.; and Nordendale, N., “Accurate Finite Element Modeling of Pretensioned Prestressed Concrete Beams,” Engineering Structures, V. 101, Oct. 2015, pp. 163-178. doi: 10.1016/j.engstruct.2015.07.018

43. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

44. Fédération internationale du béton, “Lightweight Aggregate Concrete (fib Bulletin No. 8),” fib, Lausanne, Switzerland, 2000, 118 pp.


ALSO AVAILABLE IN:

Electronic Materials Journal