Behavior of Square Columns with Interlocking Pattern Ties under Axial Compression

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Behavior of Square Columns with Interlocking Pattern Ties under Axial Compression

Author(s): Vemuri V. Rangarao, Kolluru V. L. Subramaniam, and S. Suriya Prakash

Publication: Structural Journal

Volume: 118

Issue: 3

Appears on pages(s): 209-222

Keywords: columns; confinement; ductility; interlocked; ties; uniaxial compression

DOI: 10.14359/51730528

Date: 5/1/2021

Abstract:
An innovative transverse reinforcement (TR) system for square reinforced concrete (RC) columns is proposed in this study. It consists of an interlocking pattern (SIP) formed by inclined ties for improving the confinement of the concrete core in the column. Specific improvements of the SIP system over the conventional ties (SC) include more uniform confinement along the axis of the column and better lateral restraint to longitudinal bars. The development and assembly of the SIP system are presented. The performance of short RC columns with an identical volumetric ratio of SC and SIP ties is investigated experimentally. Columns with the SIP tie system exhibit improvements in load capacity and ductility. In comparison with SC ties, higher deformations and larger strain energy are measured from the columns reinforced with SIP ties. The columns with SIP ties had significantly smaller visible damage when compared to the columns with SC ties. Experimentally measured axial strains in concrete and longitudinal reinforcing bars are also lower in the columns with SIP ties. A numerical evaluation indicates a higher average effective confinement pressure on concrete and lower damage in the cover for columns with the SIP system.

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 519 pp.

2. IS 13920-2016, “Ductile Designing and Detailing of Reinforced Concrete Structures Subject to Seismic Forces—Code of Practice,” first revision, Bureau of Indian Standards, New Delhi, India, 2016, 20 pp.

3. Anthony, J. C.; Dawn, E. L.; and Jack, P. M., “Behavior of Reinforced Concrete Bridge Columns Having Varying Aspect Ratios and Varying Lengths of Confinement,” Pacific Earthquake Engineering Research Center (PEER), PEER Report 2000/08, 2001, 136 pp.

4. Ho, J. C. M.; Lam, J. Y. K.; and Kwan, A. K. H., “Effectiveness of Adding Confinement for Ductility Improvement of High-Strength Concrete Columns,” Engineering Structures, V. 32, No. 3, 2010, pp. 714-725. doi: 10.1016/j.engstruct.2009.11.017

5. Dong, C. K.; Kwan, A. K. H.; and Ho, J. C. M., “A Constitutive Model for Predicting the Lateral Strain of Confined Concrete,” Engineering Structures, V. 91, 2015, pp. 155-166. doi: 10.1016/j.engstruct.2015.02.014

6. Park, R., and Paulay, T., Reinforced Concrete Structures, John Wiley & Sons, New York, 1975, 768 pp.

7. Sheikh, A. S., and Uzmeri, S. M., “Strength and Ductility of Tied Concrete Columns,” Journal of the Structural Division, Proceedings of the ASCE, V. 10, May 1980, pp. 1079-1102.

8. Mander, J. B., Priestley, M. J. N., and Park, R., “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, ASCE, V. 1 14, No. 8, 1988, pp. 1804-1826.

9. Sheikh, S.A., and Yeh C., “Tied Concrete Columns under Axial Load and Flexure,” Journal of Structural Engineering, ASCE, V. 116, No. 10, Oct. 1990, pp. 2780-2800.

10. Wayne, A. B.; Dawn, E. L.; and John, F. S., “Bar Buckling in Reinforced Concrete Bridge Columns,” PEER Report 2007/11, 2007, 123 pp.

11. Wight, J. K., and MacGregor, J. G., Reinforced Concrete Structures—Mechanics and Design, sixth edition, Pearson Education Inc., New Jersey 2012, 1177 pp.

12. Bayrak, O., and Sheikh, S. A., “Confinement Steel Requirement for High Strength Columns,” Paper No. 463, 11th World Conference on Earthquake Engineering, Acapulco, Mexico, 8 pp.

13. Dhakal, P., and Maekawa, K., “Reinforcement Stability and Fracture of Cover Concrete in Reinforced Concrete Members,” Journal Structural Engineering, ASCE, V. 128, No. 10, 2002, pp. 1253-1262.

14. Mau, S. T., and El-Mabsout, M., “Inelastic Buckling of Longitudinal Bars,” Journal of Engineering Mechanics, V. 115, No. 1, 1989, pp. 1-17.

15. Bae, S.; Mieses, A. M.; and Bayrak, O., “Inelastic Buckling of Reinforcing Bars,” Journal of Structural Engineering, ASCE, V. 131, No. 2, 2005, pp. 314-321. doi: 10.1061/(ASCE)0733-9445(2005)131:2(314)

16. Su, J.; Wang, J.; Bai, Z.; Wang, W.; and Zhao, D., “Influence of Reinforcement Buckling on the Seismic Performance of Reinforced Concrete Columns,” Engineering Structures, V. 103, 2015, pp. 174-188. doi: 10.1016/j.engstruct.2015.09.007

17. Salim, R. R., and Saatcioglu, M., “Confinement of Reinforced Concrete Columns with Welded Wire Fabric,” ACI Structural Journal, V. 86, No. 5, Sept.-Oct. 1989, pp. 615-623.

18. Saatcioglu, M., and Giera, M., “Confinement of Reinforced Concrete Columns with Welded Reinforcement Grids,” ACI Structural Journal, V. 96, No. 1, Jan.-Feb. 1999, pp. 29-39.

19. Matusumoto, T.; Okstad, E.; Kawashima, K.; and Mahin, S. A., “Seismic Performance of Rectangular Columns And Interlocking Spiral Columns,” 14th World Congress on Earthquake Engineering, Beijing, China, 2008, Oct. 12-17, 8 pp.

20. Yin, S. Y.-L.; Wang, J.-C.; and Wang, P.-H., “Development of Multi-Spiral Confinements in Rectangular Columns for Construction Automation,” Zhongguo Gongcheng Xuekan, V. 35, No. 3, 2012, pp. 309-320. doi: 10.1080/02533839.2012.655528

21. Liang, C. Y.; Chen, C. C.; Weng, C. C.; Yin, S. Y. L.; and Wang, J. C., “Axial Compressive Behaviour of Square Composite Columns Confined by Multiple Spirals,” Journal of Constructional Steel Research, V. 103, 2014, pp. 230-240. doi: 10.1016/j.jcsr.2014.09.006

22. Karayannis, C. G.; Chalioris, C. E.; and Mavroeidis, P. D., “Shear Capacity of RC Rectangular Beams with Continuous Spiral Transversal Reinforcement,” Computational Methods and Experimental Measurements XII, V. 41, 2005, pp. 379-386.

23. Bill, H. L.; Miller, M. L.; Doellman, A. M.; and Shahrooz, B. M., “Evaluation of Continuous Transverse Reinforcement - Applicability of Current Design Provisions and Detailing Practices,” Concrete International, V. 35, No. 11, Nov. 2013, pp. 49-55.

24. Azimi, M; Adnan, A. B.; Md Sam, A. R. B.; Md Tahir, M.; Faridmehr, I.; and RezaHodjati, “Seismic Performance of RC Beam-Column Connections with Continuous Rectangular Spiral Transverse Reinforcements for Low Ductility Classes,” The Scientific World Journal, Hindawi Publishing Corporation, 2014, pp. 1-12.

25. Vemuri, V. R. R; Subramaniam, K.V.L.; and Prakash, S. S., “Lateral Reinforcement System and Method for Concrete Structures,” US Patent Pub No 2017/0218629 A1, 2017, 40 pp.

26. ACI Committee 549, “State of the Art Report on Ferrocement (ACI 549R-97),” American Concrete Institute, Farmington Hills, MI, 1997, 26 pp.

27. Paul, B. K., and Pama, R. P., “Ferrocement,” International Ferrocement Information Center, Asian Institute of Technology, Bangkok, IFIC Publication Number 5/78, 1978, 149 pp.

28. IS 516-1959, “Method of Test for Strength of Concrete,” Bureau of Indian Standards, New Delhi, India, Re-affirmed in 2013, 24 pp.

29. IS 10262-2009, “Concrete Mix Proportioning – Guidelines (First revision) Plain & Reinforced Concrete – Code of Practice,” Bureau of Indian Standards, New Delhi, India, 2009, 40 pp.

30. IS 12269-2013, “Specification for 53 Grade Ordinary Portland Cement,” Bureau of Indian Standards, New Delhi, India, 2013, 10 pp.

31. IS 383-1970, “Specification for Coarse and Fine Aggregates from Natural Sources for Concrete,” Bureau of Indian Standards, New Delhi, India, (Re-affirmed in 2002), 19 pp.

32. IS 9103-1999, “Concrete Admixtures-Specification,” Bureau of Indian Standards, New Delhi, India, 1999, 14 pp.

33. IS 1786-2008, “High Strength Deformed Bars and Wires for Concrete Reinforcement – Specification (Fourth Revision)” Bureau of Indian Standards, New Delhi, India, 2008, 12 pp.

34. Applied Technology Council (ATC), “NEHRP Guidelines for the Seismic Guidelines for the Rehabilitation of Buildings (ATC-33 FEMA-273),” 1997, 444 pp.

35. Jankowiak, T., and Lodygowski, T., “Identiðcation of Parameters of Concrete Damage Plasticity Constitutive Model,” Found Civil Environmental Enginerring, V. 6, 2005, pp. 53-69.

36. Kmiecik, P., and Kamiński, M., “Modeling of Reinforced Concrete Structures and Composite Structures with Concrete Strength Degradation Taken into Consideration,” Archives of Civil and Mechanical Engineering, V. 11, No. 3, 2011, pp. 623-636. doi: 10.1016/S1644-9665(12)60105-8

37. ABAQUS 6.14., Dassault Systèms Simulia Corp., Providence, RI, 2014, 1489 pp.

38. Fink, J.; Petraschek, T.; and Ondris, L., “Push-Out Test Parametric Simulation Study of a New Sheet-Type Shear Connector,” Projekte an den zentralen Applikationsservern, Berichte 2006, Zentraler Informatikdienst (ZID) der Technischen Univ., Wien, Wien, Austria, 2007, pp. 131-153.

39. Chellapandian, M.; Prakash, S. S.; and Rajagopal, A., “Analytical and ðnite Element Studies on Hybrid FRP Strengthened RC Column Elements under Axial and Eccentric Compression,” Composite Structures, V. 184, 2018, pp. 234-248. doi: 10.1016/j.compstruct.2017.09.109

40. Kupfer, H.; Hisdorf, H. K.; and Rusch, H., “Behaviour of Concrete Under Biaxial Stress,” ACI Journal Proceedings, V. 66, No. 8, Aug. 1969, pp. 656-666.

41. Hognestad, E., “Ultimate Strength of Reinforced Concrete in American Design Practice,” Bulletin D12, Portland Cement Association, Research, and Development Laboratories, Chicago, IL, 1961, 19 pp.

42. Greene, G. G., “Behavior of Reinforced Concrete Girders under Cyclic Torsion and Torsion Combined with Shear: Experimental Investigation and Analytical Models,” PhD dissertation, Department of Civil, Architectural, and Environmental Engineering, University of Missouri Rolla, Rolla, MO, 2006.

43. Lai, M. H.; Liang, Y. W.; Wang, Q.; Ren, F. M.; Chen, M. T.; and Ho, J. C. M., “A Stress-Path Dependent Stress-Strain Model for FRP-Confined Concrete,” Engineering Structures, V. 203, 2020, 17 pp.

44. Ho, J. C. M.; Ou, X. L.; Chen, M. T.; Wang, Q.; and Lai, M. H., “A Path Dependent Constitutive Model for CFFT Column,” Engineering Structures, V. 210, 2020, 19 pp.

45. Lai, M. H.; Song, W.; Ou, X. L.; Chen, M. T.; Wang, Q.; and Ho, J. C. M., “A Path Dependent Stress-Strain Model for Concrete-Filled-Steel-Tube Column,” Engineering Structures, V. 210, 2020, 19 pp.

46. Pantazopoulou, S. J., “Detailing for Reinforcement Stability in RC Members,” Journal of Structural Engineering, ASCE, V. 124, No. 6, 1998, pp. 623-632. doi: 10.1061/(ASCE)0733-9445(1998)124:6(623)


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer