Structural and Mechanical Characteristics of Double-Hoop Unbonded Annular Anchor Lining

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Structural and Mechanical Characteristics of Double-Hoop Unbonded Annular Anchor Lining

Author(s): Ruilang Cao, Yufei Zhao, Yujie Wang, and Jin Pi

Publication: Structural Journal

Volume: 118

Issue: 3

Appears on pages(s): 61-70

Keywords: annular anchors; mechanical characteristics; pressure tunnel; prestressed structure; structural design

DOI: 10.14359/51729352

Date: 5/1/2021

Abstract:
A new type of prestressed reinforced concrete lining with doublehoop unbonded annular anchors (hereinafter referred to as “DUAA lining”) can resist high internal pressure. It provides an approach to solving the problem of supporting large-section pressure tunnels with thin cover layers, unsatisfied stability, and high internal water pressure. However, its extensive application was hindered by its uncertain mechanical properties caused by its complexity. A large in-place test of the mechanical properties of the DUAA lining was carried out in a 6.8 m diameter water conveyance tunnel in Jilin, China. The study reveals the superposition effect of the annular anchor tension, the spatial distribution patterns of the prestress, and the potential failure mode of the structure by closely considering the mechanical properties and the prestress increasing together. The annular anchors are closed at the free anchor head, which not only helps decrease the prestress loss but also improves its uniform distribution. Although the annular anchor in different positions generates different prestress effects for the DUAA lining, the total prestress value by adding all the annular anchors is close. For the active restriction of the annular anchor, the relatively uniform circular and longitudinal prestress generated from the DUAA lining can effectively resist high internal water pressure even without the support of the surrounding rocks.

Related References:

Abbas, S.; Soliman, A. M.; and Nehdi, M. L., 2014, “Mechanical Performance of RC and SFRC Precast Tunnel Lining Segments: A Case Study,” ACI Materials Journal, V. 111, No. 5, Sept.-Oct., pp. 501-510. doi: 10.14359/51687101

Ahn, J. H.; Jung, C. Y.; and Kim, S. H., 2010, “Evaluation on Structural Behaviors of Prestressed Composite Beams Using External Prestressing Member,” Structural Engineering and Mechanics, V. 34, No. 2, pp. 247-275. doi: 10.12989/sem.2010.34.2.247

Bai, W., and Wang, Q. F., 2014, “Stress–Strain Characteristics and Elastic–Plastic Damage Constitutive Equation of Steel Fiber Reinforced Concrete under Cyclic Compression at Medium Strain Rate,” Journal of Testing and Evaluation, V. 42, No. 6, p. JTE20130150. doi: 10.1520/JTE20130150

Burningham, C. A.; Pantelides, C. P.; and Reaveley, L. D., 2014, “Repair of Prestressed Concrete Beams with Damaged Steel Tendons Using Post-Tensioned Carbon Fiber-Reinforced Polymer Rods,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 387-395.

Cao, R.; Wang, Y.; Zhao, Y.; Pi, J.; and Yao, W., 2016, “Study on Numerical Modelling Method of the Prestressed Tunnel Lining with Unbonded Curve Anchored Tendons,” Journal of China Institute Water Resource and Hydropower Research, V. 14, No. 6, pp. 471-477.

Dadashi, E.; Noorzad, A.; Shahriar, K.; and Goshtasbi, K., 2017, “Hydro-Mechanical Interaction Analysis of Reinforced Concrete Lining in Pressure Tunnels,” Tunnelling and Underground Space Technology, V. 69, No. 10, pp. 125-132. doi: 10.1016/j.tust.2017.06.006

Fahimifar, A., and Soroush, H., 2005, “A Theoretical Approach for Analysis of the Interaction between Grouted Rockbolts and Rock Masses,” Tunnelling and Underground Space Technology, V. 20, No. 4, pp. 333-343. doi: 10.1016/j.tust.2004.12.005

Hajali, M.; Alavinasab, A.; and Shdid, C. A., 2016, “Structural Performance of Buried Prestressed Concrete Cylinder Pipes with Harnessed Joints Interaction Using Numerical Modeling,” Tunnelling and Underground Space Technology, V. 51, No. 1, pp. 11-19. doi: 10.1016/j.tust.2015.10.016

Kang, J. F.; Liang, Y. H.; and Zhang, Q. C., 2006, “3-D Finite Element Analysis of Post-Prestressed Concrete Lining,” Journal of Tianjin University Science and Technology, V. 39, No. 8, pp. 968-972.

Kang, J. F.; Sui, C. E.; and Wang, X. Z., 2014, “Structure Optimization of the Prestressed Tunnel Lining with Unbonded Circular Anchored Tendons,” Journal of Hydraulic Engineering, V. 45, No. 1, pp. 103-108.

Landau, Y. A., 1991, “New Design of Reinforced Concrete Penstock Compensator,” Hydrotechnical Construction, V. 25, No. 3, pp. 172-174. doi: 10.1007/BF01423982

Lee, Y., and Lee, E. T., 2015, “Analysis of Prestressed Concrete Cylinder Pipes with Fiber Reinforced Polymer,” KSCE Journal of Civil Engineering, V. 19, No. 3, pp. 682-688. doi: 10.1007/s12205-013-0006-9

Lou, T.; Lopes, S. M. R.; and Lopes, A. V., 2013, “Nonlinear and Time-Dependent Analysis of Continuous Unbonded Prestressed Concrete Beams,” Computers & Structures, V. 119, No. 4, pp. 166-176. doi: 10.1016/j.compstruc.2012.12.014

Lv, L.; Yang, Y.; and Tang, W., 2009, “Treatment for Oil and Water Penetration in Anchorage Channel of San Discharge Tunnel, Xiaolangdi Key Water Control Project,” Chinese Building Waterproofing, V. 2009, No. 2, pp. 36-38.

Mander, J. A. B., and Priestley, M. J. N., 1988, “Theoretical Stress-Strain Model for Confined Concrete,” Journal of Structural Engineering, V. 114, No. 8, pp. 1026-1804.

Nagamoto, T.; Yoneda, T.; Tanaka, D.; and Irita, K., 2008, “Large P & PC Segment Works: Construction Works for Rainwater Storage under Osaka International Airport,” Tunnels and Underground, V. 39, No. 8, pp. 581-589.

Nishikawa, K., 2003, “Development of a Prestressed and Precast Concrete Segmental Lining,” Tunnelling and Underground Space Technology, V. 18, No. 2-3, pp. 243-251. doi: 10.1016/S0886-7798(03)00033-6

Park, H. G.; Kang, S.; and Choi, K. K., 2013, “Analytical Model for Shear Strength of Ordinary and Prestressed Concrete Beams,” Engineering Structures, V. 46, No. 1, pp. 94-103. doi: 10.1016/j.engstruct.2012.07.015

Qayssar, S. M.; Mohammad, T.; and Prabhat, K. S., 2014, “Analysis of a Thin and Thick Walled Pressure Vessel for Different Materials,” International Journal of Mechanical Engineering and Technology, V. 10, No. 5, pp. 9-19.

Schleiss, A. J., and Manso, P. A., 2012, “Design of Pressure Relief Valves for Protection of Steel-Lined Pressure Shafts and Tunnels against Buckling during Emptying,” Rock Mechanics and Rock Engineering, V. 45, No. 1, pp. 11-20. doi: 10.1007/s00603-011-0187-9

Showkati, A.; Maarefvand, P.; and Hassani, H., 2016, “An Analytical Solution for Stresses Induced by a Post-Tensioned Anchor in Rocks Containing Two Perpendicular Joint Sets,” Acta Geotechnica, V. 11, No. 2, pp. 415-432. doi: 10.1007/s11440-015-0371-2

Simanjuntak, T. D. Y. F.; Marence, M.; Mynett, A. E.; and Schleiss, A. J., 2013, “Mechanical-Hydraulic Interaction in the Lining Cracking Process of Pressure Tunnels,” International Journal on Hydropower & Dams, V. 20, No. 3, pp. 48-54.

Simanjuntak, T. D. Y. F.; Marence, M.; Schleiss, A. J.; and Mynett, A. E., 2016, “The Interplay of in situ Stress Ratio and Transverse Isotropy in the Rock Mass on Prestressed Concrete-Lined Pressure Tunnels,” Rock Mechanics and Rock Engineering, V. 49, No. 11, pp. 4371-4392. doi: 10.1007/s00603-016-1035-8

Sousa, H.; Bento, J.; and Figueiras, J., 2013, “Construction Assessment and Long-Term Prediction of Prestressed Concrete Bridges Based on Monitoring Data,” Engineering Structures, V. 52, No. 9, pp. 26-37. doi: 10.1016/j.engstruct.2013.02.003

Trucco, G., and Zeltner, O., 1978, “Grimsel-Oberrar Pumped Storage System,” Water Power & Dam Construction, V. 1978, No. 2, pp. 351-357.

Wan, B.; Harries, K. A.; and Petrou, M. F., 2002, “Transfer Length of Strands in Prestressed Concrete Piles,” ACI Structural Journal, V. 99, No. 5, Sept.-Oct., pp. 577-585.

Zareifard, M. R., and Fahimifar, A., 2016, “A Simplified Solution for Stresses around Lined Pressure Tunnels Considering Non-Radial Symmetrical Seepage Flow,” KSCE Journal of Civil Engineering, V. 20, No. 7, pp. 2640-2654. doi: 10.1007/s12205-016-0105-5

Zhang, Y.; Yan, Z.; Zhu, H.; and Ju, J., 2018, “Experimental Study on the Structural Behaviors of Jacking Prestressed Concrete Cylinder Pipe,” Tunnelling and Underground Space Technology, V. 73, No. 3, pp. 60-70. doi: 10.1016/j.tust.2017.11.033


ALSO AVAILABLE IN:

Electronic Structural Journal