Concrete Q & A: Design and Construction of Slabs-on-Ground

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Concrete Q & A: Design and Construction of Slabs-on-Ground

Author(s):

Publication: Concrete International

Volume: 42

Issue: 11

Appears on pages(s): 87-88

Keywords:

DOI: 10.14359/51729313

Date: 11/1/2020

Abstract:
Applying ACI 318: Can I use ACI 318 to design slabs-on-ground? Minimum Reinforcement: What is the minimum reinforcement required for slabs-on-ground? Hard Troweling and Air Content: Can concrete with a total air content exceeding 3% be hard troweled successfully? Exposure Conditions: What can be done to protect slabs-on-ground that will be subject to various exposure conditions as defined in ACI 318?

Related References:

1. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary (ACI 318R-19),” American Concrete Institute, Farmington Hills, MI, 2019, 623 pp.

2. ACI Committee 360, “Guide to Design of Slabs-on-Ground (ACI 360R-10),” American Concrete Institute, Farmington Hills, MI, 2010, 72 pp.

3. Tarr, S.M.; Sheehan, M.J.; and Van Duyne, E.J., “Considerations for Precast Concrete Panels Tied to Slabs-on-Ground,” Concrete International, V. 42, No. 1, Jan. 2020, pp. 31-35.

4. ACI Committee 301, “Specifications for Concrete Construction (ACI 301-20),” American Concrete Institute, Farmington Hills, MI, 2020, 69 pp.




  