Shear Strength of Reinforced Concrete Beams Using Recycled Coarse Aggregates without Stirrups

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Shear Strength of Reinforced Concrete Beams Using Recycled Coarse Aggregates without Stirrups

Author(s): Woosuk Kim, Thomas H.-K. Kang, Deuckhang Lee, Hajin Choi, and Yoon-Keun Kwak

Publication: Structural Journal

Volume: 117

Issue: 6

Appears on pages(s): 281-295

Keywords: construction waste; design; failure mode; recycled coarse aggregate; shear; strength

DOI: 10.14359/51728079

Date: 11/1/2020

Abstract:
Given current environmental concerns, attention has been directed toward the use of recycled coarse aggregates (RCAs) as a substitute for natural raw materials commonly consumed in construction. In regard to shear performance, limited studies currently exist. To this end, a total of 56 reinforced concrete beams without stirrups were tested to identify the effect of using RCA on shear strength. Failure governed primarily by shear span-depth ratios and partially by tension reinforcement ratios can significantly affect shear behavior of RCA concrete members. Test results obtained for this study were evaluated using current ACI 318 shear design equations. Overall, crack patterns and failure modes for the RCA concrete test specimens were similar to those of natural coarse aggregates (NCAs). On this basis, it was established that RCA concrete beams can be used in practice with confidence in satisfactory shear performance.

Related References:

1. Ministry of Environment of Korea, “Comprehensive Plan to Promote of the Recycling of Construction Waste,” Sejong City, South Korea, 2002, 16 pp. (in Korean)

2. Shon, C.; Mukashev, T.; Lee, D. H.; Zhang, D.; and Kim, J., “Can Common Reed Fiber Become an Effective Construction Material? Physical, Mechanical, and Thermal Properties of Mortar Mixture Containing Common Reed Fiber,” Sustainability, V. 11, No. 3, 2019, pp. 1-19. doi: 10.3390/su11030903

3. Frondistou-Yannas, S., “Waste Concrete as Aggregate for New Concrete,” ACI Journal Proceedings, V. 74, No. 8, Aug. 1977, pp. 373-376.

4. Fathifazl, G.; Razaqpur, A.; Isgor, B.; Abbas, A.; Fournier, B.; and Foo, S., “Flexural Performance of Steel-Reinforced Recycled Concrete Beams,” ACI Structural Journal, V. 106, No. 6, Nov.-Dec. 2009, pp. 858-867.

5. Fathifazl, G.; Razaqpur, A.; Isgor, B.; Abbas, A.; Fournier, B.; and Foo, S., “Proportioning Concrete Mixtures with Recycled Concrete Aggregate, a Novel Method,” Concrete International, V. 32, No. 3, Mar. 2010, pp. 37-43.

6. Kang, T. H.-K.; Kim, W. S.; Kwak, Y. K.; and Hong, S. G., “Flexural Testing of Reinforced Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 111, No. 3, Mar.-Apr. 2014, pp. 607-616. doi: 10.14359/51686622

7. McNeil, K., and Kang, T. H.-K., “Recycled Concrete Aggregates: A Review,” International Journal of Concrete Structures and Materials, V. 7, No. 1, 2013, pp. 61-69. doi: 10.1007/s40069-013-0032-5

8. Yehia, S.; Helal, K.; Abusharkh, A.; Zaher, A.; and Istaitiyeh, H., “Strength and Durability Evaluation of Recycled Aggregate Concrete,” International Journal of Concrete Structures and Materials, V. 9, No. 2, 2015, pp. 219-239. doi: 10.1007/s40069-015-0100-0

9. Lee, W. S.; Yun, H. D.; Kim, S. W.; Choi, K. S.; You, Y. C.; and Kim, K. H., “The Effect of Replacement Ratio of Recycled Coarse Aggregate on Shear Strength of Reinforced Concrete Beams without Shear Reinforcement,” Journal of the Architectural Institute of Korea, V. 23, No. 10, 2007, pp. 3-10. (in Korean)

10. Lee, Y. O.; Yun, H. D.; You, Y. C.; and Kim, K. H., “Shear Performance of Reinforced Concrete Beams Utilized Mixed Recycled Coarse Aggregates,” Journal of the Architectural Institute of Korea, V. 26, No. 4, 2010, pp. 39-46. (in Korean)

11. Kim, J. H.; Sung, J. H.; Jeon, C. S.; Lee, S. H.; and Kim, H. S., “A Study on the Properties of Recycled Aggregate Concrete and Its Production Facilities,” Applied Sciences (Basel, Switzerland), V. 9, No. 9, 2019, pp. 1-21. doi: 10.3390/app9091935

12. Brandes, M. R., and Kurama, Y. C., “Ultimate Behavior of Flexure-Critical Prestressed Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 116, No. 2, Mar. 2019, pp. 15-28. doi: 10.14359/51713287

13. Knaack, A. M., and Kurama, Y. C., “Modeling Time-Dependent Deformations: Application for Reinforced Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 115, No. 1, Jan. 2018, pp. 175-190. doi: 10.14359/51701153

14. Knaack, A. M., and Kurama, Y. C., “Sustained Service Load Behavior of Concrete Beams with Recycled Concrete Aggregates,” ACI Structural Journal, V. 112, No. 5, Sept.-Oct. 2015, pp. 565-578. doi: 10.14359/51687799

15. Sadati, S.; Arezoumandi, M.; Khayat, K. H.; and Volz, J. S., “Shear Performance of Reinforced Concrete Beams Incorporating Recycled Concrete Aggregate and High-Volume Fly Ash,” Journal of Cleaner Production, V. 115, No. 1, 2016, pp. 284-293. doi: 10.1016/j.jclepro.2015.12.017

16. Fathifazl, G.; Razaqpur, A.; Isgor, B.; Abbas, A.; Fournier, B.; and Foo, S., “Shear Strength of Reinforced Recycled Concrete Beams without Stirrups,” Magazine of Concrete Research, V. 61, No. 7, 2009, pp. 477-490. doi: 10.1680/macr.2008.61.7.477

17. Fathifazl, G.; Razaqpur, A. G.; Isgor, B.; Abbas, A.; Fournier, B.; and Foo, S., “Shear Capacity Evaluation of Steel Reinforced Recycled Concrete (RRC) Beams,” Engineering Structures, V. 33, No. 3, 2011, pp. 1025-1033. doi: 10.1016/j.engstruct.2010.12.025

18. Rahal, K. N., and Alrefaei, Y. T., “Shear Strength of Recycled Aggregate Concrete Beams Containing Stirrups,” Construction and Building Materials, V. 191, No. 1, 2018, pp. 866-876. doi: 10.1016/j.conbuildmat.2018.10.023

19. Han, B. C.; Yun, H. D.; and Chung, S. Y., “Shear Capacity of Reinforced Concrete Beams Made with Recycled-Aggregate,” Recent Advances in Concrete Technology, SP-200, American Concrete Institute, Farmington Hills, MI, 2001, pp. 503-516.

20. Knaack, A. M., and Kurama, Y. C., “Behavior of Reinforced Concrete Beams with Recycled Concrete Coarse Aggregates,” Journal of Structural Engineering, ASCE, V. 141, No. 3, 2015, pp. 1-12. doi: 10.1061/(ASCE)ST.1943-541X.0001118

21. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-19) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2019, 624 pp.

22. Reineck, K.-H.; Bentz, E. C.; Fitik, B.; Kuchma, D. A.; and Bayrak, O., “ACI-DAfStb Database of Shear Tests on Slender Reinforced Concrete Beams without Stirrups,” ACI Structural Journal, V. 110, No. 5, Sept.-Oct. 2013, pp. 867-875.

23. ASTM C127-04, “Standard Test Method for Density, Relative Density (Specific Gravity), and Absorption of Coarse Aggregate,” ASTM International, West Conshohocken, PA, 2004, 6 pp.

24. ASTM C39/C39M-18, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2018, 8 pp.

25. ASTM C496/C496M-17, “Standard Test Method for Splitting Tensile Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2017, 5 pp.

26. ASTM C78/C78M-18, “Standard Test Method for Flexural Strength of Concrete (Using Simple Beam with Third-Point Loading),” ASTM International, West Conshohocken, PA, 2018, 5 pp.

27. Collins, M. P.; Bentz, E. C.; and Sherwood, E. G., “Where Is Shear Reinforcement Required? Review of Research Results and Design Procedures,” ACI Structural Journal, V. 105, No. 5, Sept.-Oct. 2008, pp. 590-600.

28. Sherwood, E. G.; Bentz, E. C.; and Collins, M. P., “Effect of Aggregate Size on Beam-Shear Strength of Thick Slabs,” ACI Structural Journal, V. 104, No. 2, Mar.-Apr. 2007, pp. 180-191.

29. Janaka Perera, S. J., and Mutsuyoshi, H., “Shear Behavior of Reinforced High-Strength Concrete Beams,” ACI Structural Journal, V. 110, No. 1, Jan.-Feb. 2013, pp. 43-52.

30. Lee, D. H.; Han, S. J.; and Kim, K. S., “Dual Potential Capacity Model for Reinforced Concrete Beams Subjected to Shear,” Structural Concrete, V. 17, No. 3, 2016, pp. 443-456. doi: 10.1002/suco.201500165

31. Lee, D. H.; Han, S. J.; Kim, K. S.; and LaFave, J. M., “Shear Strength of Reinforced Concrete Beams Strengthened in Shear Using Externally-­Bonded FRP Composites,” Composite Structures, V. 173, No. 1, 2017, pp. 177-187. doi: 10.1016/j.compstruct.2017.04.025

32. Lee, D. H.; Kim, K. S.; Han, S. J.; Zhang, D.; and Kim, J., “Dual Potential Capacity Model for Reinforced Concrete Short and Deep Beams Subjected to Shear,” Structural Concrete, V. 19, No. 1, 2018, pp. 76-85. doi: 10.1002/suco.201700202

33. Wight, J. K., Reinforced Concrete: Mechanics and Design, seventh edition, Pearson, Upper Saddle River, NJ, 2016.

34. Collins, M. P., and Mitchell, D., Prestressed Concrete Structures, Prentice Hall, Upper Saddle River, NJ, 1991.

35. Collins, M. P., and Kuchma, D., “How Safe Are Our Large, Lightly Reinforced Concrete Beams, Slabs, and Footings?” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 482-490.

36. Kani, G. N. J., “How Safe Are Our Large Reinforced Concrete Beams?” ACI Journal Proceedings, V. 64, No. 3, Mar. 1967, pp. 128-141.

37. Kim, W., and White, R. N., “Initiation of Shear Cracking in Reinforced Concrete Beams with No Web Reinforcement,” ACI Structural Journal, V. 88, No. 3, May-June 1991, pp. 301-308.

38. Kim, D.; Kim, W.; and White, R. N., “Arch Action in Reinforced Concrete Beams—A Rational Prediction of Shear Strength,” ACI Structural Journal, V. 96, No. 4, July-Aug. 1999, pp. 586-595.

39. Kuchma, D. A.; Wei, S.; Sanders, D. H.; Belarbi, A.; and Novak, L. C., “Development of the One-Way Shear Design Provisions of ACI 318-19 for Reinforced Concrete,” ACI Structural Journal, V. 116, No. 4, July-Aug. 2019, pp. 285-295.

40. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary,” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

41. Yerzhanov, M.; Ju, H.; Zhang, D.; Moon, S. W.; Kim, J.; and Lee, D. H., “Shear Strength Model of Reinforced Concrete Beams without Stirrup Used in the CIS Countries,” Journal of Structural Integrity and Maintenance, V. 4, No. 1, 2019, pp. 15-25. doi: 10.1080/24705314.2019.1565056

42. Ibrahim Ary, M., and Kang, T. H.-K., “Shear-Strengthening of Reinforced & Prestressed Concrete Beams Using FRP: Part I – Review of Previous Research,” International Journal of Concrete Structures and Materials, V. 6, No. 1, 2012, pp. 41-48.

43. Kang, T. H.-K., and Ibrahim Ary, M., “Shear-Strengthening of Reinforced & Prestressed Concrete Beams Using FRP: Part II – Experimental Investigation,” International Journal of Concrete Structures and Materials, V. 6, No. 1, 2012, pp. 49-57.


ALSO AVAILABLE IN: