Effectiveness of Hybrid Fibers on Flexural Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effectiveness of Hybrid Fibers on Flexural Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars

Author(s): Ganapati M. Patil, M. Chellapandian, and S. Suriya Prakash

Publication: Structural Journal

Volume: 117

Issue: 5

Appears on pages(s): 269-282

Keywords: flexure; glass fiber-reinforced polymer (GFRP) reinforcement; hybrid fibers; polyolefin fiber; serviceability; steel fiber

DOI: 10.14359/51725844

Date: 9/1/2020

Abstract:
The effectiveness of structural macro-synthetic polyolefin (PO) and a hybrid combination of steel and synthetic fibers on the flexural performance of glass fiber-reinforced polymer (GFRP) reinforced concrete beams is studied. Improvement in post-cracking stiffness, deformation factor, and change in failure modes due to fiber addition is investigated. In total, 14 full-scale RC beams are cast and tested under four-point bending configuration. The test series includes: 1) control specimen with GFRP reinforcement; 2) GFRP-reinforced members with 0.35, 0.70, and 1.0% volume of PO fibers; and 3) GFRP-reinforced members with 0.35, 0.70, and 1.0% volume of hybrid steel and PO fibers in equal ratio. Experimental results revealed that the addition of synthetic and hybrid fibers significantly improved the post-cracking stiffness, peak strength, and energy dissipation capacity of GFRP-reinforced members. The deflection levels at service loads reduced with increase in fiber dosage. Deflection of GFRP-reinforced members with and without fibers was calculated using the models proposed by different researchers and compared with test results at the serviceability levels. Also, a proposed model is introduced for consideration of the effect of fiber contribution in the predictions of deflection.

Related References:

1. Abdalla, H. A., “Evaluation of Deflection in Concrete Members Reinforced with Fibre Reinforced Polymer (FRP) Bars,” Composite Structures, V. 56, No. 1, 2002, pp. 63-71. doi: 10.1016/S0263-8223(01)00188-X

2. Kassem, C.; Farghaly, A. S.; and Benmokrane, B., “Evaluation of Flexural Behavior and Serviceability Performance of Concrete Beams Reinforced with FRP Bars,” Journal of Composites for Construction, V. 15, No. 5, 2011, pp. 682-695. doi: 10.1061/(ASCE)CC.1943-5614.0000216

3. Miàs, C.; Torres, L.; Turon, A.; and Barris, C., “Experimental Study of Immediate and Time Dependent Deflections of GFRP Reinforced Concrete Beams,” Composite Structures, V. 96, 2013, pp. 279-285. doi: 10.1016/j.compstruct.2012.08.052

4. Toutanji, H., and Deng, Y., “Deflection and Crack-Width Prediction of Concrete Beams Reinforced with Glass FRP Rods,” Construction & Building Materials, V. 17, No. 1, 2003, pp. 69-74. doi: 10.1016/S0950-0618(02)00094-6

5. Bencardino, F.; Condello, A.; and Ombres, L., “Numerical and Analytical Modeling of Concrete Beams with Steel, FRP and Hybrid FRP-Steel Reinforcements,” Composite Structures, V. 140, 2016, pp. 53-65. doi: 10.1016/j.compstruct.2015.12.045

6. Mousa, S.; Mohamed, H. M.; and Benmokrane, B., “Cracking and Crack Control in Circular Concrete Bridge Members Reinforced with Fiber-Reinforced Polymer Bars,” Journal of Bridge Engineering, V. 24, No. 1, 2019, p. 04018108 doi: 10.1061/(ASCE)BE.1943-5592.0001335

7. El-Nemr, A.; Ahmed, E. A.; and Benmokrane, B., “Flexural Behavior and Serviceability of Normal- and High-Strength Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 110, No. 6, Nov.-Dec. 2013, pp. 1077-1090.

8. El-Nemr, A.; Ahmed, E. A.; El-Safty, A.; and Benmokrane, B., “Evaluation of the Flexural Strength and Serviceability of Concrete Beams Reinforced with Different Types of GFRP Bars,” Engineering Structures, V. 173, 2018, pp. 606-619. doi: 10.1016/j.engstruct.2018.06.089

9. Mousa, S.; Mohamed, H. M.; and Benmokrane, B., “Flexural Strength and Design Analysis of Circular Reinforced Concrete Members with Glass Fiber-Reinforced Polymer Bars and Spirals,” ACI Structural Journal, V. 115, No. 5, Sept. 2018, pp. 1353-1364. doi: 10.14359/51702282

10. Rimkus, A.; Barros, J. A. O.; Gribniak, V.; and Rezazadeh, M., “Mechanical Behavior of Concrete Prisms Reinforced with Steel and GFRP Bar Systems,” Composite Structures, V. 220, 2019, pp. 273-288. doi: 10.1016/j.compstruct.2019.03.088

11. Jakubovskis, R.; Kaklauskas, G.; Gribniak, V.; Weber, A.; and Juknys, M., “Serviceability Analysis of Concrete Beams with Different Arrangements of GFRP Bars in the Tensile Zone,” Journal of Composites for Construction, V. 18, No. 5, 2014, p. 04014005 doi: 10.1061/(ASCE)CC.1943-5614.0000465

12. Sheikh, S. A., and Kharal, Z., “Replacement of Steel with GFRP for Sustainable Reinforced Concrete,” Construction & Building Materials, V. 160, 2018, pp. 767-774. doi: 10.1016/j.conbuildmat.2017.12.141

13. Mousa, S.; Mohamed, H. M.; Benmokrane, B.; and Ferrier, E., “Flexural Behavior of Full-Scale Circular Concrete Members Reinforced with Basalt FRP Bars and Spirals: Tests and Theoretical Studies,” Composite Structures, V. 203, 2018, pp. 217-232. doi: 10.1016/j.compstruct.2018.06.107

14. Ovitigala, T.; Ibrahim, M. A.; and Issa, M. A., “Serviceability and Ultimate Load Behavior of Concrete Beams Reinforced with Basalt Fiber-Reinforced Polymer Bars,” ACI Structural Journal, V. 113, No. 4, July-Aug. 2016, pp. 757-768. doi: 10.14359/51688752

15. Bischoff, P. H., and Gross, S., “Design Approach for Calculating the Deflection of FRP Reinforced Concrete,” Journal of Composites for Construction, V. 15, No. 4, 2011, pp. 490-499. doi: 10.1061/(ASCE)CC.1943-5614.0000195

16. Mota, C.; Alminar, S.; and Svecova, D., “Critical Review of Deflection Formulas for FRP-RC Members,” Journal of Composites for Construction, V. 10, No. 3, 2006, pp. 183-194. doi: 10.1061/(ASCE)1090-0268(2006)10:3(183)

17. Bernard, E. S., “Effect of Synthetic Fibers and Aggregate Size on Flexural Crack Widths,” ACI Structural Journal, V. 116, No. 3, May 2019, pp. 677-686. doi: 10.14359/51713286

18. Amin, A., and Gilbert, R. I., “Steel Fiber-Reinforced Concrete Beams—Part I: Material Characterization and In-Service Behavior,” ACI Structural Journal, V. 116, No. 2, 2019, pp. 19-26. doi: 10.14359/51713288

19. Buratti, N.; Mazzotti, C.; and Savoia, M., “Post-Cracking Behavior of Steel and Macro-Synthetic Fibre-Reinforced Concretes,” Construction & Building Materials, V. 25, No. 5, 2011, pp. 2713-2722. doi: 10.1016/j.conbuildmat.2010.12.022

20. Rasheed, M. A., and Prakash, S. S., “Experimental Study on Compression Behaviour of Fibre Reinforced Cellular Concrete Stack Bonded Masonry Prisms,” ACI Materials Journal, V. 115, No. 1, Jan. 2018, pp. 149-160.

21. Joshi, S.; Thammishetti, N.; and Prakash, S. S., “Efficiency of Steel and Macro- Synthetic Structural Fibers on the Flexure-Shear Behaviour of Prestressed Concrete Beams,” Engineering Structures, V. 171, 2018, pp. 47-55. doi: 10.1016/j.engstruct.2018.05.067

22. Alberti, M.; Enfedaque, A.; and Gálvez, J., “Improving the Reinforce­ment of Polyolefin Fiber Reinforced Concrete for Infrastructure Applications,” Fibers (Basel, Switzerland), V. 3, No. 4, 2015, pp. 504-522. doi: 10.3390/fib3040504

23. Wang, H., and Belarbi, A., “Ductility Characteristics of Fiber-Reinforced-Concrete Beams Reinforced with FRP Rebars,” Construction & Building Materials, V. 25, No. 5, 2011, pp. 2391-2401. doi: 10.1016/j.conbuildmat.2010.11.040

24. Yang, J. M.; Min, K.; Shin, H. O.; and Yoon, Y. S., “Effect of steel and synthetic fibers on flexural behavior of high-strength concrete beams reinforced with FRP bars,” Composites. Part B, Engineering, V. 43, No. 3, 2012, pp. 1077-1086. doi: 10.1016/j.compositesb.2012.01.044

25. Marcos-Meson, V.; Michel, A.; Solgaard, A.; Fischer, G.; Edvardsen, C.; and Skovhus, T. L., “Corrosion Resistance of Steel Fibre Reinforced Concrete - A Literature Review,” Cement and Concrete Composites, V. 103, 2018, pp. 1-20. doi: 10.1016/j.cemconres.2017.05.016

26. Spagnuolo, S.; Meda, A.; Rinaldi, Z.; and Nanni, A., “Precast Concrete Tunnel Segments with GFRP Reinforcement,” Journal of Composites for Construction, V. 21, No. 5, 2017, p. 04017020 doi: 10.1061/(ASCE)CC.1943-5614.0000803

27. Meda, A.; Rinaldi, Z.; Spagnuolo, S.; De Rivaz, B.; and Giamundo, N., “2019, “Hybrid Precast Tunnel Segments in Fiber Reinforced Concrete with Glass Fiber Reinforced Bars,” Tunnelling and Underground Space Technology, V. 86, Apr, 2019, pp. 100-112. doi: 10.1016/j.tust.2019.01.016

28. ASTM D7205/D7205M-06(2011), “Standard Test Method for Tensile Properties of Fiber Reinforced Polymer Matrix Composite Bars,” ASTM International, West Conshohocken, PA, 2011, 13 pp.

29. EN 14651, “Test Method for Metallic Fibered Concrete—Measuring the Flexural Tensile Strength,” European Committee for Standardization, Brussels, Belgium, 2005.

30. fib, “Model Code for Concrete Structures,” International Federation for Structural Concrete, Lausanne, Switzerland, 2010.

31. ACI Committee 440, “Guide for the Design and Construction of Structural Concrete Reinforced with Fiber-Reinforced Polymer Bars (ACI 440.1R-15),” American Concrete Institute, Farmington Hills, MI, 2015, 88 pp.

32. CAN/CSA S806-12, “Design and Construction of Building Components with Fiber Reinforced Polymers,” Canadian Standards Association, Mississauga, ON, Canada, 2012.

33. ISIS Canada Research Network, “Reinforced Concrete Structures with Fibre Reinforced Polymers,” ISIS Manual No. 3, University of Manitoba, Winnipeg, MB, Canada, 2007.

34. Benmokrane, B.; Chaallal, O.; and Masmoudi, R., “Flexural Response of Concrete Beams Reinforced with FRP Reinforcing Bars,” ACI Structural Journal, V. 93, No. 1, Jan.-Feb. 1996, pp. 46-55.

35. Toutanji, H. A., and Saafi, M., “Flexural Behavior of Concrete Beams Reinforced with Glass Fiber-Reinforced Polymer (GFRP) Bars,” ACI Structural Journal, V. 97, No. 5, Sept.-Oct. 2000, pp. 712-719.

36. Zhu, H.; Cheng, S.; Gao, D.; Neaz, S. M.; and Li, C., “Flexural Behavior of Partially Fiber-Reinforced High-Strength Concrete Beams Reinforced with FRP Bars,” Construction & Building Materials, V. 161, 2018, pp. 587-597. doi: 10.1016/j.conbuildmat.2017.12.003

37. Alberti, M. G.; Enfedaque, A.; Gálvez, J. C.; and Agrawal, V., “Fibre Distribution and Orientation of Macro-Synthetic Polyolefin Fiber Reinforced Concrete Elements,” Construction & Building Materials, V. 122, 2016, pp. 505-517. doi: 10.1016/j.conbuildmat.2016.06.083

38. Alberti, M. G.; Enfedaque, A.; and Gálvez, J. C., “On the Prediction of the Orientation Factor and Fibre Distribution of Steel and Macro-Synthetic Fibres for Fiber-Reinforced Concrete,” Cement and Concrete Composites, V. 77, 2017, pp. 29-48. doi: 10.1016/j.cemconcomp.2016.11.008

39. RILEM TC 162-TDF. “Test and Design Methods for Steel Fibre Reinforced Concrete, σ-ε-Design Method,” Materials and Structures, V. 36, No. 262, 2003, pp. 560-567. doi: 10.1617/14007

40. di Prisco, M.; Colombo, M.; and Dozio, D., “Fibre‐Reinforced Concrete in fib Model Code 2010: Principles, Models and Test Validation,” Structural Concrete, V. 14, No. 4, 2013, pp. 342-361. doi: 10.1002/suco.201300021

41. EN 14651, “Test Method for Metallic Fibre Concrete-Measuring the Flexural Tensile Strength (Limit of Proportionality (LOP), Residual),” European Committee for Standardization, Brussels, Belgium, 2005.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer