Continuous Characterization of Pore Structure in Cement Paste

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Continuous Characterization of Pore Structure in Cement Paste

Author(s): Zhiyong Liu, Sen Gao, Weiwei Chen, Yunsheng Zhang, and Cheng Liu

Publication: Materials Journal

Volume: 116

Issue: 6

Appears on pages(s): 117-129

Keywords: cement paste; hydration; pore structure; simulation

DOI: 10.14359/51716978

Date: 11/1/2019

Abstract:
Unlike traditional experimental testing, some procedures have been developed for the characterization of microstructures of cement-based materials. Based on the microstructure of the cement hydration model obtained from a digital image-based model, the parameters of pore structure were in-place continuously determined by CEMHYD3D. The characteristic parameters of pore include total porosity, the continuous pore, isolated pore, dead-end pore, connectivity, pore size distribution, specific surface area, and tortuosity. According to the combustion algorithm, the three-dimensional (3-D) voxel-erosion method, the mercury intrusion porosimetry simulation, the continuous PSD algorithm, and the random walk algorithm, the physical models are developed into program to obtain the characteristic parameters of pore structure evolution. The results show that the dead-end pores and the isolated pores begin to decrease after the continuous pores disappear. The pore size distribution of the pore structure is calculated with finer resolution. The water-cement ratio (w/c) and hydration degree have a significant effect on the specific surface area of the pores. With the increase of the degree of hydration, the tortuosity of the pore structure increases gradually. Finally, the simulation results are compared to the experimental values and the literature data that have a good agreement.

Related References:

1. Zhang, W. H., and Zhang, Y. S., “Research on the Static and Dynamic Compressive Properties of High Performance Cementitious Composite (HPCC) Containing Coarse Aggregate,” Archives of Civil and Mechanical Engineering, V. 15, No. 3, 2015, pp. 711-720. doi: 10.1016/j.acme.2014.12.006

2. Liu, Z.; Zhang, Y.; and Jiang, Q., “Continuous Tracking of the Relationship between Resistivity and Pore Structure of Cement Pastes,” Construction and Building Materials, V. 53, No. 53, 2014, pp. 26-31. doi: 10.1016/j.conbuildmat.2013.11.067

3. Hou, D.; Zhao, T.; Ma, H.; and Li, Z., “Reactive Molecular Simulation on Water Confined in the Nanopores of the Calcium Silicate Hydrate Gel: Structure, Reactivity, and Mechanical Properties,” The Journal of Physical Chemistry C, V. 119, No. 3, 2015, pp. 1346-1358. doi: 10.1021/jp509292q

4. Mobili, A.; Belli, A.; Giosuè, C.; Bellezze, T.; and Tittarelli, F., “Metakaolin and Fly Ash Alkali-Activated Mortars Compared with Cementitious Mortars at the Same Strength Class,” Cement and Concrete Research, V. 88, 2016, pp. 198-210. doi: 10.1016/j.cemconres.2016.07.004

5. Dong, H.; Gao, P.; and Ye, G., “Characterization and Comparison of Capillary Pore Structures of Digital Cement Pastes,” Materials and Structures, V. 50, No. 2, 2017, pp. 154 doi: 10.1617/s11527-017-1023-9

6. Yang, C. C.; Cho, S. W.; and Wang, L. C., “The Relationship between Pore Structure and Chloride Diffusivity from Ponding Test in Cement-Based Materials,” Materials Chemistry and Physics, V. 100, No. 2, 2006, pp. 203-210. doi: 10.1016/j.matchemphys.2005.12.032

7. Luping, T., and Nilsson, L.-O., “A Study of the Quantitative Relationship between Permeability and Pore Size Distribution of Hardened Cement Pastes,” Cement and Concrete Research, V. 22, No. 4, 1992, pp. 541-550. doi: 10.1016/0008-8846(92)90004-F

8. Ulm, F. J.; Constantinides, G.; and Heukamp, F. H., “Is Concrete a Poromechanics Materials?—A Multiscale Investigation of Poroelastic Properties,” Materials and Structures, V. 37, No. 1, 2004, pp. 43-58. doi: 10.1007/BF02481626

9. Jiang, L., and Guan, Y., “Pore Structure and Its Effect on Strength of High-Volume Fly Ash Paste,” Cement and Concrete Research, V. 29, No. 4, 1999, pp. 631-633. doi: 10.1016/S0008-8846(99)00034-4

10. Ma, H., “Mercury Intrusion Porosimetry in Concrete Technology: Tips in Measurement, Pore Structure Parameter Acquisition and Application,” Journal of Porous Materials, V. 21, No. 2, 2014, pp. 207-215. doi: 10.1007/s10934-013-9765-4

11. Yang, L.; Zhang, Y.; Liu, Z.; Zhao, P.; and Liu, C., “In-Situ Tracking of Water Transport in Cement Paste Using X-Ray Computed Tomography Combined with CsCl Enhancing,” Materials Letters, V. 160, 2015, pp. 381-383. doi: 10.1016/j.matlet.2015.08.011

12. Bortolotti, V.; Brizi, L.; Brown, R. J. S.; Fantazzini, P.; and Mariani, M., “Nano and Sub-Nano Multiscale Porosity Formation and Other Features Revealed by 1H NMR Relaxometry During Cement Hydration,” Langmuir, V. 30, No. 36, 2014, pp. 10871-10877. doi: 10.1021/la501677k

13. Pujari, P. K.; Sen, D.; Amarendra, G.; Abhaya, S.; Pandey, A. K.; Dutta, D.; and Mazumder, S., “Study of Pore Structure in Grafted Polymer Membranes using Slow Positron Beam and Small-Angle X-Ray Scattering Techniques,” Nuclear Instruments and Methods in Physics Research, V. 254, No. 2, 2007, pp. 278-282. doi: 10.1016/j.nimb.2006.11.052

14. Ouellet, S.; Bussière, B.; Aubertin, M.; and Benzaazoua, M., “Microstructural Evolution of Cemented Paste Backfill: Mercury Intrusion Porosimetry Test Results,” Cement and Concrete Research, V. 37, No. 12, 2007, pp. 1654-1665. doi: 10.1016/j.cemconres.2007.08.016

15. Diamond, S., and Landis, E., “Microstructural Features of a Mortar as Seen by Computed Microtomography,” Materials and Structures, V. 40, No. 9, 2007, pp. 989-993. doi: 10.1617/s11527-006-9194-9

16. Korb, J. P., “NMR and Nuclear Spin Relaxation of Cement and Concrete Materials,” Current Opinion in Colloid & Interface Science, V. 14, No. 3, 2009, pp. 192-202. doi: 10.1016/j.cocis.2008.10.004

17. Ye, G., “Experimental Study and Numerical Simulation of the Development of the Microstructure and Permeability of Cementitious Materials,” Journal of Colloid and Interface Science, V. 262, No. 1, 2003, pp. 149-161.

18. Zhang, H.; Šavija, B.; Chaves Figueiredo, S.; Lukovic, M.; and Schlangen, E., “Microscale Testing and Modelling of Cement Paste as Basis for Multi-Scale Modelling,” Materials (Basel), V. 9, No. 11, 2016, pp. 907-921. doi: 10.3390/ma9110907

19. Bishnoi, S., and Scrivener, K. L., “µic: A New Platform for Modelling the Hydration of Cements,” Cement and Concrete Research, V. 39, No. 4, 2009, pp. 266-274. doi: 10.1016/j.cemconres.2008.12.002

20. Liu, Z.; Chen, W.; Zhang, Y.; and Lv, H., “A Three-Dimensional Multi-Scale Method to Simulate the ion Transport Behavior of Cement-Based Materials,” Construction and Building Materials, V. 120, 2016, pp. 494-503. doi: 10.1016/j.conbuildmat.2016.05.121

21. Bentz, D. P., and Garboczi, E. J., “Percolation of Phases in a Three-Dimensional Cement Paste Microstructural Model,” Cement and Concrete Research, V. 21, No. 2, 1991, pp. 325-344. doi: 10.1016/0008-8846(91)90014-9

22. Bentz, D. P., “Three‐Dimensional Computer Simulation of Portland Cement Hydration and Microstructure Development,” Journal of the American Ceramic Society, V. 80, No. 1, 1997, pp. 3-21. doi: 10.1111/j.1151-2916.1997.tb02785.x

23. Ma, H., and Li, Z., “Realistic Pore Structure of Portland Cement Paste: Experimental Study and Numerical Simulation,” Computers and Concrete, V. 11, No. 4, 2013, pp. 317-336. doi: 10.12989/cac.2013.11.4.317

24. Aligizaki, K. K., Pore Structure of Cement-Based Materials: Testing, Interpretation and Requirements, CRC Press, Boca Raton, FL, 2014.

25. Baroghel-Bouny, V.; Dierkens, M.; Wang, X.; Soive, A.; Saillio, M.; Thiery, M.; and Thauvin, B., “Ageing and Durability of Concrete in Lab and in Field Conditions: Investigation of Chloride Penetration,” Journal of Sustainable Cement-Based Materials, V. 2, No. 2, 2013, pp. 67-110. doi: 10.1080/21650373.2013.797938

26. Turcotte, D. L., and Brown, S. R., “Fractals and Chaos in Geology and Geophysics,” Physics Today, V. 46, No. 5, 1993, pp. 68. doi: 10.1063/1.2808908

27. Hedenblad, G., “The Use of Mercury Intrusion Porosimetry or Helium Porosity to Predict the Moisture Transport Properties of Hardened Cement Paste,” Advanced Cement Based Materials, V. 6, No. 3, 1997, pp. 123-129. doi: 10.1016/S1065-7355(97)90019-5

28. Pratt, W. K., Digital Image Processing, Wiley, New York, NY, 1978.

29. Münch, B., and Holzer, L., “Contradicting Geometrical Concepts in Pore Size Analysis Attained with Electron Microscopy and Mercury Intrusion,” Journal of the American Ceramic Society, V. 91, No. 12, 2008, pp. 4059-4067. doi: 10.1111/j.1551-2916.2008.02736.x

30. Nakashima, Y., and Kamiya, S., “Mathematica Programs for the Analysis of Three-Dimensional Pore Connectivity and Anisotropic Tortuosity of Porous Rocks Using X-ray Computed Tomography Image Data,” Journal of Nuclear Science and Technology, V. 44, No. 9, 2007, pp. 1233-1247. doi: 10.1080/18811248.2007.9711367

31. Carman, P. C., “Fluid Flow Through a Granular Bed,” Chemical Engineering Research and Design, V. 97, 1937, pp. 32-48.

32. Childs, E. C., “Dynamics of Fluids in Porous Media,” Engineering Geology, V. 7, No. 2, 1973, pp. 174-175. doi: 10.1016/0013-7952(73)90047-1

33. Ghanbarian, B.; Hunt, A. G.; Ewing, R. P.; and Sahimi, M., “Tortuosity in Porous Media: A Critical Review,” Soil Science Society of America Journal, V. 77, No. 5, 2013, p. 1461-1477 doi: 10.2136/sssaj2012.0435

34. Liu, L.; Sun, W.; Ye, G.; Chen, H.; and Qian, Z., “Estimation of the Ionic Diffusivity of Virtual Cement Paste by Random Walk Algorithm,” Construction and Building Materials, V. 28, No. 1, 2012, pp. 405-413. doi: 10.1016/j.conbuildmat.2011.08.077

35. Nakashima, Y., and Watanabe, Y., “Estimate of Transport Properties of Porous Media by Microfocus X-Ray Computed Tomography and Random Walk Simulation,” Water Resources Research, V. 38, No. 12, 2002. doi: 10.1029/2001WR000937

36. Archie, G. E., “The Electrical Resistivity Log as an Aid in Determining Some Reservoir Characteristics,” Transactions of the AIME, V. 146, No. 1, 1942, pp.54-62.


ALSO AVAILABLE IN:

Electronic Materials Journal