Calculating Method for Ultimate Tendon Stress in Internally Unbonded Prestressed Concrete Members
Search

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Calculating Method for Ultimate Tendon Stress in Internally Unbonded Prestressed Concrete Members

Author(s): Fei Peng and Weichen Xue

Publication: Structural Journal

Volume: 116

Issue: 5

Appears on pages(s): 225-234

Keywords: analytical model; flexural capacity; prestressed concrete; simplified equation; tendon stress increase; ultimate stress; unbonded tendon

DOI: 10.14359/51716764

Date: 9/1/2019

Abstract:
A new simplified and yet rational method is proposed to calculate ultimate tendon stress in internally unbonded prestressed concrete (PC) members in this paper. Firstly, a beam-tendon structural deformation model, in which the unbonded tendon is approximated by a number of segments, is proposed to implement global deformation compatibility. Using a geometry analysis, the tendon elongation is expressed as a function of the displacements of the segments. Based on plastic collapse mechanism, a deflected shape is introduced to simplify the deformation curve of unbonded PC members at ultimate limit state. Then, an analytical model is proposed for ultimate stress increase in unbonded tendons. Finally, a straightforward equation is developed to predict the tendon stress increase based on a regression analysis of parametric analysis results. On this basis, a simplified method is proposed to determine the ultimate tendon stress and flexural capacity of simply supported and continuous members. It is found that the proposed method is more accurate than existing methods by comparing their predictions with available experimental results of 218 specimens.

Related References:

Aalami, B., 1994, “Unbonded and Bonded Post-Tensioning Systems in Building Construction: A Design and Performance Review,” PTI Technical Notes, No. 5, Post-Tensioning Institute, Farmington Hills, MI, 10 pp.

AASHTO, 2017, LRFD Bridge Design Specifications, eighth edition, American Association of State Highway and Transportation Officials, Washington, DC, 1781 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 519 pp.

ACI Committee 440, 2004, “Prestressing Concrete Structures with FRP Tendons (ACI 440.4R-04),” American Concrete Institute, Farmington Hills, MI, 35 pp.

Alkhairi, F. M., and Naaman, A. E., 1993, “Analysis of Beams Prestressed with Unbonded Internal or External Tendons,” Journal of Structural Engineering, ASCE, V. 119, No. 9, Sept., pp. 2680-2700. doi: 10.1061/(ASCE)0733-9445(1993)119:9(2680)

Au, F. T. K., and Du, J. S., 2008, “Deformability of Concrete Beams with Unbonded FRP Tendons,” Engineering Structures, V. 30, No. 12, pp. 3764-3770. doi: 10.1016/j.engstruct.2008.07.003

Baker, A. L. L., 1949, “A Plastic Theory of Design for Ordinary Reinforced and Prestressed Concrete Including Moment Redistribution in Continuous Members,” Magazine of Concrete Research, V. 1, No. 2, June, pp. 57-66. doi: 10.1680/macr.1949.1.2.57

British Standards Institution (BSI), 1997, “Structural Use of Concrete – Part 1: Code of Practice for Design and Construction (BS 8110),” London, UK, 152 pp.

Burns, N. H.; Charney, F. A.; and Vines, W. R., 1978, “Tests of One-Way Post-Tensioned Slabs with Unbonded Tendons,” PCI Journal, V. 23, No. 5, Sept-Oct., pp. 66-83. doi: 10.15554/pcij.09011978.66.83

Burns, N. H.; Helwig, T.; and Tsujimoto, T., 1991, “Effective Prestress Force in Continuous Post-Tensioned Beams with Unbonded Tendons,” ACI Structural Journal, V. 88, No. 1, Jan.-Feb., pp. 84-90.

Campbell, T. I., and Chouinard, K. L., 1991, “Influence of Nonprestressed Reinforcement on the Strength of Unbonded Partially Prestressed Concrete Members,” ACI Structural Journal, V. 88, No. 5, Sept.-Oct., pp. 546-551.

Chakrabarti, P. R., 1995, “Ultimate Stress for Unbonded Post-Tensioning Tendons in Partially Prestressed Beams,” ACI Structural Journal, V. 92, No. 6, Nov.-Dec., pp. 689-697.

Cooke, N.; Park, R.; and Yong, P., 1981, “Flexural Strength of Prestressed Concrete Members with Unbonded Tendons,” PCI Journal, V. 26, No. 6, Nov.-Dec., pp. 52-81. doi: 10.15554/pcij.11011981.52.81

Dall’Asta, A.; Ragni, L.; and Zona, A., 2007, “Simplified Method for Failure Analysis of Concrete Beams Prestressed with External Tendons,” Journal of Structural Engineering, ASCE, V. 133, No. 1, Jan., pp. 121-131. doi: 10.1061/(ASCE)0733-9445(2007)133:1(121)

Ghallab, A., 2013, “Calculating Ultimate Tendon Stress in Externally Prestressed Continuous Concrete Beams Using Simplified Formulas,” Engineering Structures, V. 46, pp. 417-430. doi: 10.1016/j.engstruct.2012.07.018

Grace, N. F.; Singh, S. B.; and Puravankara, S., 2006, “Behavior of Prestressed Concrete Box-Beam Bridges Using CFRP Tendons,” PCI Journal, V. 51, No. 2, pp. 26-41. doi: 10.15554/pcij.03012006.26.41

Guiglia, M.; Taliano, M.; and Debernardi, P. G., 2013, “Calculation of the Ultimate Stress of Unbonded Tendons in Prestressed Concrete Members Considering the Rotation Capacity,” Magazine of Concrete Research, V. 65, No. 1, Jan., pp. 14-26. doi: 10.1680/macr.11.00197

Haldar, A., and Mahadevan, S., 2000, Probability, Reliability and Statistical Method in Engineering Design, John Wiley & Sons, Inc., New York, 304 pp.

Harajli, M. H., 1990, “Effect of Span-Depth Ratio on the Ultimate Steel Stress in Unbonded Prestressed Concrete Members,” ACI Structural Journal, V. 87, No. 3, May-June, pp. 305-312.

Harajli, M. H., 2006, “On the Stress in Unbonded Tendons at Ultimate: Critical Assessment and Proposed Changes,” ACI Structural Journal, V. 103, No. 6, Nov.-Dec., pp. 803-812.

Harajli, M. H., 2011, “Proposed Modification of AASHTO LRFD for Computing Stress in Unbonded Tendons at Ultimate,” Journal of Bridge Engineering, ASCE, V. 16, No. 6, pp. 828-838. doi: 10.1061/(ASCE)BE.1943-5592.0000183

Harajli, M. H., 2012, “Tendon Stress at Ultimate in Continuous Unbonded Post-Tensioned Members: Proposed Modification of ACI Eq. (18-4) and (18-5),” ACI Structural Journal, V. 109, No. 2, Mar.-Apr., pp. 183-192.

Harajli, M. H., and Kanj, M., 1991, “Ultimate Flexural Strength of Concrete Members Prestressed with Unbonded Tendons,” ACI Structural Journal, V. 88, No. 6, Nov.-Dec., pp. 663-673.

He, Z. Q., and Liu, Z., 2010, “Stresses in External and Internal Unbonded Tendons: Unified Methodology and Design Equations,” Journal of Structural Engineering, ASCE, V. 136, No. 9, pp. 1055-1065. doi: 10.1061/(ASCE)ST.1943-541X.0000202

Heo, S.; Shin, S.; and Lee, C., 2013, “Flexural Behavior of Concrete Beams Internally Prestressed with Unbonded Carbon-Fiber-Reinforced Polymer Tendons,” Journal of Composites for Construction, ASCE, V. 17, No. 2, Apr., pp. 167-175. doi: 10.1061/(ASCE)CC.1943-5614.0000306

Huang, Y., and Kang, T. H. K., 2018, “Modeling of Sliding Behavior of Unbonded Tendons in Post-Tensioned Concrete Members,” ACI Structural Journal, V. 115, No. 4, July-Aug., pp. 1153-1164. doi: 10.14359/51702066

JGJ 92, 2016, “Technical Specification for Concrete Structures Prestressed with Unbonded Tendons (JGJ92-2016),” China Architecture & Building Press, Beijing, China, 132 pp.

Lee, C.; Shin, S.; and Lee, H., 2017, “Balanced Ratio of Concrete Beams Internally Prestressed with Unbonded CFRP Tendons,” International Journal of Concrete Structures and Materials, V. 11, No. 1, pp. 1-16. doi: 10.1007/s40069-016-0171-6

Lee, L. H.; Moon, J. H.; and Lim, J. H., 1999, “Proposed Methodology for Computing of Unbonded Tendon Stress at Flexural Failure,” ACI Structural Journal, V. 96, No. 6, Nov.-Dec., pp. 1040-1048.

Lim, J.; Moon, J.; and Lee, L., 2003, “Ultimate Stress of Unbonded Tendon in Continuous Members,” Magazine of Concrete Research, V. 55, No. 5, pp. 461-470. doi: 10.1680/macr.2003.55.5.461

Lin, T. Y., and Burns, N. H., 1981, Design of Prestressed Concrete Structures, third edition, John Wiley & Sons, Inc., New York, 646 pp.

MacGregor, R. J. G., 1989, “Strength and Ductility of Externally Post-Tensioned Segmental Box Girders,” PhD dissertation, University of Texas at Austin, Austin, TX, 368 pp.

Maguire, M.; Chang, M.; Collins, W.; and Sun, Y., 2017, “Stress Increase of Unbonded Tendons in Continuous Posttensioned Members,” Journal of Bridge Engineering, ASCE, V. 22, No. 2, Feb., p. 04016115 doi: 10.1061/(ASCE)BE.1943-5592.0000991

Maguire, M.; Collins, W. M.; Halbe, K. R.; and Roberts-Wollmann, C. L., 2016, “Multi-span Members with Unbonded Tendons: Ultimate Strength Behavior,” ACI Structural Journal, V. 113, No. 2, Mar.-Apr., pp. 195-204.

Mattock, A. H.; Yamazaki, J.; and Kattula, B., 1971, “Comparative Study of Prestressed Concrete Beams, with and without Bond,” ACI Journal Proceedings, V. 68, No. 2, Feb., pp. 116-125.

Meng, L. X.; Tao, X. K.; Guan, J. G.; and Xu, F. Q., 2006, “Experimental Study on Flexural Behavior of Partially Prestressed Concrete Beams with Unbonded CFRP Tendons,” Building Structure, V. 36, No. 3, Mar., pp. 31-37. (in Chinese) doi: 10.19701/j.jzjg.2006.03.01010.19701/j.jzjg.2006.03.010

Meski, F. E., and Harajli, M., 2014, “Flexural Capacity of Fiber-Reinforced Polymer Strengthened Unbonded Post-Tensioned Members,” ACI Structural Journal, V. 111, No. 2, Mar.-Apr., pp. 407-418.

Mojtahedi, S., and Gamble, W., 1978, “Ultimate Steel Stress in Unbonded Prestressed Concrete,” Journal of the Structural Division, ASCE, V. 104, pp. 1159-1165.

Moreira, L. S.; Sousa, J. B. M. Jr.; and Parente, E., Jr., 2018, “Nonlinear Finite Element Simulation of Unbonded Prestressed Concrete Beams,” Engineering Structures, V. 170, Sept., pp. 167-177. doi: 10.1016/j.engstruct.2018.05.077

Naaman, A. E., and Alkhairi, F. M., 1991, “Stress at Ultimate in Unbonded Post-Tensioning Tendons: Part 2—Proposed Methodology,” ACI Structural Journal, V. 88, No. 6, Nov.-Dec., pp. 683-692.

Naaman, A. E.; Burns, N. H.; French, C.; Gamble, W. L.; and Mattock, A. H., 2002, “Stresses in Unbonded Prestressing Tendons at Ultimate: Recommendation,” ACI Structural Journal, V. 99, No. 4, July-Aug., pp. 518-529.

Ozkul, O.; Nassif, H.; Tanchan, P.; and Harajli, M. H., 2008, “Rational Approach for Predicting Stress in Beams with Unbonded Tendons,” ACI Structural Journal, V. 105, No. 3, May-June, pp. 338-347.

Pannell, F. N., 1969, “Ultimate Moment of Resistance of Unbonded Prestressed Concrete Beams,” Magazine of Concrete Research, V. 21, No. 66, pp. 43-54. doi: 10.1680/macr.1969.21.66.43

Peng, F., and Xue, W., 2018, “Analytical Approach for Flexural Capacity of FRP Prestressed Concrete T-Beams with Non-Prestressed Steel Bars,” Journal of Composites for Construction, ASCE, V. 22, No. 6, p. 04018063 doi: 10.1061/(ASCE)CC.1943-5614.0000903

Peng, F.; Xue, W.; and Tan, Y., 2018, “Design Approach for Flexural Capacity of Prestressed Concrete Beams with External Tendons,” Journal of Structural Engineering, ASCE, V. 144, No. 12, p. 04018215 doi: 10.1061/(ASCE)ST.1943-541X.0002208

Rizkalla, N. S., 2000, “Partial Bonding and Partial Prestressing Using Stainless Steel Reinforcement for Members Prestressed with FRP,” master’s dissertation, Queen’s University, Kingston, ON, Canada, 212 pp.

Roberts-Wollmann, C. R.; Kreger, M. E.; Rogowsky, D. M.; and Breen, J. E., 2005, “Stresses in External Tendons at Ultimate,” ACI Structural Journal, V. 102, No. 2, Mar.-Apr., pp. 206-213.

Six, P. D., 2015, “Continuous Unbonded Post-Tensioned Members: Quantifying Strand Stress Increase,” master’s dissertation, Utah State University, Logan, UT, 147 pp.

Tam, A., and Pannel, F. N., 1976, “The Ultimate Moment of Resistance of Unbonded Partially Prestressed Reinforced Concrete Beams,” Magazine of Concrete Research, V. 28, No. 97, pp. 203-208. doi: 10.1680/macr.1976.28.97.203

Tao, X., and Du, G., 1985, “Ultimate Stress of Unbonded Tendons in Partially Prestressed Concrete Beams,” PCI Journal, V. 30, No. 6, pp. 72-91. doi: 10.15554/pcij.11011985.72.91

Turmo, J.; Ramos, G.; and Aparicio, A. C., 2005, “FEM Study on the Structural Behaviour of Segmental Concrete Bridges with Unbonded Prestressing and Dry Joints: Simply Supported Bridges,” Engineering Structures, V. 27, No. 11, pp. 1652-1661. doi: 10.1016/j.engstruct.2005.04.011

Wang, J. Q.; Liu, Z.; and Lu, Z. T., 2005, “Stress Increment of Prestressing Tendons Based on Deflection for Unbonded or External Prestressed Beams,” Journal of Southeast University, V. 35, No. 6, pp. 915-919. (in Chinese) doi: 10.3321/j.issn:1001-0505.2005.06.019.10.3321/j.issn:1001-0505.2005.06.019

Warwaruk, J.; Sozen, M. A.; and Siess, C. P., 1962, “Investigation of Prestressed Reinforced Concrete for Highway Bridges, Part III: Strength and Behavior in Flexure of Prestressed Concrete Beams,” Bulletin No. 464, University of Illinois Engineering Experiment Station, Urbana, IL, Aug., 105 pp.

Xue, W.; Peng, F.; and Zheng, Q., 2016, “Design Equations for Flexural Capacity of Concrete Beams Reinforced with Glass Fiber–Reinforced Polymer Bars,” Journal of Composites for Construction, ASCE, V. 20, No. 3, June, p. 04015069. doi: 10.1061/(ASCE)CC.1943-5614.0000630, 04015069.10.1061/(ASCE)CC.1943-5614.0000630

Yang, K., and Kang, T. H., 2011, “Equivalent Strain Distribution Factor for Unbonded Tendon Stress at Ultimate,” ACI Structural Journal, V. 108, No. 2, Mar.-Apr., pp. 217-226.

Zhou, W., and Zheng, W., 2014, “Unbonded Tendon Stresses in Continuous Post-tensioned Beams,” ACI Structural Journal, V. 111, No. 3, May-June, pp. 525-536. doi: 10.14359/51686569


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer