Deflections Considering Twist Angles for Curved Concrete Girders

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Deflections Considering Twist Angles for Curved Concrete Girders

Author(s): Yin Shen, Taiyu Song, Guoping Li, CS Walter Yang, and David W. Scott

Publication: Structural Journal

Volume: 116

Issue: 4

Appears on pages(s): 155-168

Keywords: curved girders; effective stiffness; post-cracking deformation; prestressed concrete; torsional stiffness; twist angle

DOI: 10.14359/51715566

Date: 7/1/2019

Abstract:
Horizontally curved concrete girder bridges have been widely used in urban viaducts and overpasses across the world. When designing these structures, it is necessary to estimate the maximum deflections under service loads to satisfy requirements of the serviceability limit state. Because of twist due to torsion in curved concrete girders, the maximum deflection needs to take into account the effect of torsional twist, which has not been considered in previous research. Based on the concept of effective torsional stiffness, a new method is proposed for calculating post-cracking twist angles in curved concrete girders. The proposed method in combination with the effective moment of inertia method can accurately predict maximum deflections in curved concrete girders. The simplicity of the proposed method is illustrated in an example. The calculated central deflections and twist angles are compared with experimental data obtained from previous tests that cover curved box-section and solid-section non-prestressed and prestressed concrete beams. The proposed method provides satisfactory predictions in terms of twist angles until the first yielding of reinforcement. The variations between the calculated and measured twist angles and maximum deflections are within ±10% and ±20%, respectively. The results of this study indicate that deflection formulas from the ACI 318-14 Code and the AASHTO LRFD Bridge Design Specifications may produce non-conservative results for curved concrete girders under certain loading conditions.

Related References:

1. National Cooperative Highway Research Program, “Development of Design Specifications and Commentary for Horizontally Curved Concrete Box Girder Bridges,” NCHRP Report No. 620, Transportation Research Board, Washington, DC, 2008.

2. Comite Euro-International du Beton, “CEB-FIP Model Code 2010—Final Draft,” International Federation for Structural Concrete, Lausanne, Switzerland, 2011.

3. Chen, W. F., and Duan, L., Bridge Engineering Handbook, Second Edition: Fundamentals, CRC Press, Boca Raton, FL, 2014.

4. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.

5. AASHTO LRFD, “Bridge Design Specifications,” American Association of State Highway and Transportation Officials, Washington, DC, 2012.

6. GB 50010-2010, “Code for Design of Concrete Structures,” Ministry of Housing and Urban-Rural Development of the People’s Republic of China, Beijing, China, 2010. (in Chinese)

7. Song, T. Y.; Shen, Y.; and Li, G. P., “Moment Redistribution in EPC Continuous Curved Box Beams,” Journal of Bridge Engineering, ASCE, V. 22, No. 8, 2017, pp. 1-20. doi: 10.1061/(ASCE)BE.1943-5592.0001055

8. Branson, D. E., “Instantaneous and Time-Dependent Deflections on Simple and Continuous Reinforced Concrete Beams,” HRP Report, No. 7, Part 1, Alabama Highway Department, U.S. Bureau of Public Roads, Montgomery, AL, Aug. 1965, pp. 1-78.

9. Branson, D. E., Deformation of Concrete Structures, McGraw-Hill, New York, 1977, 546 pp.

10. Shaikh, A. F., and Branson, D. E., “Nontensioned Steel in Prestressed Concrete Beams,” PCI Journal, V. 15, No. 1, 1970, pp. 14-36. doi: 10.15554/pcij.02011970.14.36

11. Zuraski, P. D.; Salmon, C. G.; and Shaikh, A. F., “Calculation of Instantaneous Deflections for Continuous Reinforced Concrete Beams,” Deflections of Concrete Structures, SP-43, American Concrete Institute, Farmington Hills, MI, 1974, pp. 315-332.

12. Branson, D. E., and Trost, H., “Unified Procedures for Predicting the Deflection and Centroidal Axis Location of Partially Cracked Non-Prestressed and Prestressed Concrete Members,” ACI Journal Proceedings, V. 79, No. 2, Feb. 1982, pp. 119-130.

13. Branson, D. E., and Trost, H., “Application of the I-Effective Method in Calculating Deflections of Partially Prestressed Members,” PCI Journal, V. 27, No. 5, 1982, pp. 62-77. doi: 10.15554/pcij.09011982.62.77

14. Rao, S. V. K. M., and Dilger, W. H., “Evaluation of Short-Term Deflections of Partially Prestressed Concrete Members,” ACI Structural Journal, V. 89, No. 1, Jan.-Feb. 1992, pp. 71-78.

15. Au, F. T. K.; Du, J. S.; and Cheung, Y. K., “Service Load Analysis of Unbonded Partially Prestressed Concrete Members,” Magazine of Concrete Research, V. 57, No. 4, 2005, pp. 199-209. doi: 10.1680/macr.2005.57.4.199

16. Du, J. S.; Au, F. T.; Chan, E. K.; and Liu, L., “Deflection of Unbonded Partially Prestressed Concrete Continuous Beams,” Engineering Structures, V. 118, 2016, pp. 89-96. doi: 10.1016/j.engstruct.2016.03.040

17. Rahal, K. N., and Collins, M. P., “Analysis of Sections Subjected to Combined Shear and Torsion—A Theoretical Model,” ACI Structural Journal, V. 92, No. 4, July-Aug. 1995, pp. 459-469.

18. Rahal, K. N., and Collins, M. P., “Combined Torsion and Bending in Reinforced and Prestressed Concrete Beams,” ACI Structural Journal, V. 100, No. 2, Mar.-Apr. 2003, pp. 157-165.

19. Bairan Garcia, J. M., and Mari Bernat, A. R., “Shear-Bending-Torsion Interaction in Structural Concrete Members: A Nonlinear Coupled Sectional Approach,” Archives of Computational Methods in Engineering, V. 14, No. 3, 2007, pp. 249-278. doi: 10.1007/s11831-007-9007-5

20. Robinson, J. R., “Torsion of Concrete Cylinders of Circular Cross Section Reinforced with Hoops and Longitudinal Ties,” International Association for Bridge and Structural Engineering, Zurich, Switzerland, 1966, pp. 390-419. (in French)

21. Lampert, P., “Postcracking Stiffnesses of Reinforced Concrete Beams in Torsion and Bending,” Analysis of Structural Systems for Torsion, SP-35, American Concrete Institute, Farmington Hills, MI, 1973, pp. 385-433.

22. Hsu, T. T. C., “Torsion of Structural Concrete-Behavior of Reinforced Concrete Rectangular Members. Torsion of Structural Concrete,” Torsion of Structural Concrete, SP-18, American Concrete Institute, Farmington Hills, MI, 1968, pp. 261-306.

23. Hsu, T. T. C., “Post-Cracking Torsional Rigidity of Reinforced Concrete Sections,” ACI Journal Proceedings, V. 70, No. 5, May 1973, pp. 352-360.

24. Hsu, T. T. C.; Ivan, M.; and Fonticiella, L., “Behavior of Reinforced Concrete Horizontally Curved Beams,” ACI Journal Proceedings, V. 75, No. 4, Apr. 1978, pp. 112-123.

25. Campbell, T. I.; Lee, E. Y. K.; and Chan, K. S., “Strength of Continuous Horizontally Curved Post-Tensioned Beams,” PCI Journal, V. 25, No. 4, 1980, pp. 118-145. doi: 10.15554/pcij.07011980.118.145

26. Darwin, D.; Dolan, C. W.; and Nilson, A. H., Design of Concrete Structures, McGraw-Hill, New York, 2016, 255 pp.

27. Timoshenko, S., and Goodier, J. N., Theory of Elasticity, second edition, third edition, McGraw-Hill, New York, 1951, pp. 283-286.

28. Huang, Z., and Liu, X. L., “Modified Skew Bending Model for Segmental Bridge with Unbonded Tendons,” Journal of Bridge Engineering, ASCE, V. 11, No. 1, 2006, pp. 59-63. doi: 10.1061/(ASCE)1084-0702(2006)11:1(59)

29. JTG D62-2004, “Code for Design of Highway Reinforced Concrete and Prestressed Concrete Bridges and Culverts.” Ministry of Transport of the People’s Republic of China, China Communications Press, Beijing, China, 2004, 42 pp. (in Chinese)

30. Karlsson, I.; Elfgren, L.; and Losberg, A., “Long-Time Behavior of Reinforced Concrete Beams Subjected to Pure Torsion,” ACI Journal Proceedings, V. 71, No. 6, June 1974, pp. 280-283.

31. Pandit, G. S., “Long-Time Torsion Tests,” ACI Journal Proceedings, V. 65, No. 8, Aug. 1968, pp. 659-661.

32. Au, F. T. K., and Du, J. S., “Partially Prestressed Concrete,” Progress in Structural Engineering and Materials, V. 6, No. 2, 2004, pp. 127-135. doi: 10.1002/pse.168


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer