A State-of-the-Art Review of Bending and Shear Behaviors of Corrosion-Damaged Reinforced Concrete Beams

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: A State-of-the-Art Review of Bending and Shear Behaviors of Corrosion-Damaged Reinforced Concrete Beams

Author(s): Mahmoodreza Soltani, Amir Safiey, and Almarie Brennan

Publication: Structural Journal

Volume: 116

Issue: 3

Appears on pages(s): 53-64

Keywords: bond (concrete-to-reinforcement); deterioration; flexural capacity; residual strength; shear capacity

DOI: 10.14359/51714481

Date: 5/1/2019

Abstract:
Steel corrosion is mainly at fault for the trend of deterioration among U.S. infrastructure—namely, bridges, pipelines, and wharves. Reinforced concrete (RC) is used as the primary construction material worldwide. Reinforcement corrosion can significantly impair mechanical properties of RC members, including shear and bending capacities. In the past decades, several attempts have been made to investigate the impacts of corrosion on the mechanical behavior of RC members. It can be observed that the number of research programs conducted on this topic has rapidly increased in recent years. Therefore, there is a need in the body of knowledge to encapsulate the relevant findings in the form of a state-of-the-art review. This paper presents a chronological literature review of investigations on different components of mechanical behavior of RC beams (including shear and flexural strengths) under corrosion. The most significant contributions of these studies are identified and presented. This study presents simple relationships that rely on the current literature to be used by practitioners and designers for quick evaluation of RC beams in corrosion distress.

Related References:

AASHTO, 1996, “Standard Specifications for Highway Bridges,” 16th edition, American Association of State Highway and Transportation, Washington, DC.

AASHTO, 2002, “Standard Specifications for Highway Bridges,” 17th edition, American Association of State Highway and Transportation, Washington, DC.

ACI Committee 318, 2002, “Building Code Requirements for Structural Concrete (ACI 318-02) and Commentary (ACI 318R-02),” American Concrete Institute, Farmington Hills, MI, 443 pp.

ACI Committee 318, 2014, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 520 pp.

Aïtcin, P.-C., 2000, “Cements of Yesterday and Today: Concrete of Tomorrow,” Cement and Concrete Research, V. 30, No. 9, pp. 1349-1359. doi: 10.1016/S0008-8846(00)00365-3

Al-Sulaimani, G. J.; Kaleemullah, M.; and Basunbul, I. A., Rasheeduzzafar, 1990, “Influence of Corrosion and Cracking on Bond Behavior and Strength of Reinforced Concrete Members,” ACI Structural Journal, V. 87, No. 2, Mar.-Apr., pp. 220-231.

Ali, M. S.; Ji, C.; and Mirza, M. S., 2015, “Durable Design of Reinforced Concrete Elements against Corrosion,” Construction and Building Materials, V. 93, pp. 317-325. doi: 10.1016/j.conbuildmat.2015.05.011

Almusallam, A. A.; Al-Gahtani, A. S.; Aziz, A. R.; Dakhil, F. H.; and Rasheeduzzafar, 1996, “Effect of Reinforcement Corrosion on Flexural Behavior of Concrete Slabs,” Journal of Materials in Civil Engineering, ASCE, V. 8, No. 3, pp. 123-127. doi: 10.1061/(ASCE)0899-1561(1996)8:3(123)

Alonso, C.; Andrade, C.; Rodriguez, J.; and Diez, J. M., 1998, “Factors Controlling Cracking of Concrete Affected by Reinforcement Corrosion,” Materials and Structures, V. 31, No. 7, pp. 435-441. doi: 10.1007/BF02480466

ASCE’s 2017 Infrastructure Report Card | GPA: D+, 2017, http://www.infrastructurereportcard.org. (last accessed Sept. 15, 2017)

Azad, A. K.; Ahmad, S.; and Azher, S. A., 2007, “Residual Strength of Corrosion-Damaged Reinforced Concrete Beams,” ACI Materials Journal, V. 104, No. 1, Jan.-Feb., pp. 40-47.

Azad, K.; Ahmad, S.; and Al-Gohi, B. H. A., 2010, “Flexural Strength of Corroded Reinforced Concrete Beams,” Magazine of Concrete Research, V. 62, No. 6, pp. 405-414. doi: 10.1680/macr.2010.62.6.405

Bentz, E. C., 2000, “Sectional Analysis of Reinforced Concrete Members,” University of Toronto, Toronto, ON, Canada.

Cairns, J.; Du, Y.; and Law, D., 2008, “Structural Performance of Corrosion-Damaged Concrete Beams,” Magazine of Concrete Research, V. 60, No. 5, pp. 359-370. doi: 10.1680/macr.2007.00102

Cairns, J., and Zhao, M. A., 1993, “Behavior of Concrete Beams with Exposed Reinforcement,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 99, No. 2, pp. 141-154. doi: 10.1680/istbu.1993.23373

Campione, G.; Cannella, F.; and Cavaleri, L., 2017, “Shear and Flexural Strength Prediction of Corroded RC Beams,” Construction and Building Materials, V. 149, pp. 395-405. doi: 10.1016/j.conbuildmat.2017.05.125

Capozucca, R., and Cerri, M. N., 2003, “Influence of Reinforcement Corrosion—in the Compressive Zone—on the Behaviour of RC Beams,” Engineering Structures, V. 25, No. 13, pp. 1575-1583. doi: 10.1016/S0141-0296(03)00119-6

Castel, A.; François, R.; and Arliguie, G., 2000, “Mechanical Behaviour of Corroded Reinforced Concrete Beams—Part 1: Experimental Study of Corroded Beams,” Materials and Structures, V. 33, No. 9, pp. 539-544. doi: 10.1007/BF02480533

Chen, Y.; Gao, J.; Tang, L.; and Shen, D., 2017, “Performance of Concrete Subjected to Severe Multiple Actions of Composite Salts Solution under Wet-Dry Cycles and Flexural Loading in Lab,,” Journal of Wuhan University of Technology: Materials Science Edition, V. 32, No. 4, pp. 830-837. doi: 10.1007/s11595-017-1676-9

Coronelli, D., and Gambarova, P., 2004, “Structural Assessment of Corroded Reinforced Concrete Beams: Modeling Guidelines,” Journal of Structural Engineering, ASCE, V. 130, No. 8, pp. 1214-1224. doi: 10.1061/(ASCE)0733-9445(2004)130:8(1214)

Coronelli, D., and Mulas, M. G., 2001, “Local-Global Approach in the Seismic Analysis of R/C Frames Including Bond Slip Effects,” Engineering Structures, V. 23, No. 8, pp. 911-925. doi: 10.1016/S0141-0296(00)00116-4

Coronelli, D., and Mulas, M. G., 2006, “Modeling of Shear Behavior in Reinforced Concrete Beams,” ACI Structural Journal, V. 103, No. 3, May-June, pp. 372-382.

Dekoster, M.; Buyle-Bodin, F.; Maurel, O.; and Delmas, Y., 2003, “Modelling of the Flexural Behaviour of RC Beams Subjected to Localized and Uniform Corrosion,” Engineering Structures, V. 25, No. 10, pp. 1333-1341. doi: 10.1016/S0141-0296(03)00108-1

Dong, W.; Ye, J.; Murakami, Y.; Oshita, H.; Suzuki, S.; and Tsutsumi, T., 2016, “Residual Load Capacity of Corroded Reinforced Concrete Beam undergoing Bond Failure,” Engineering Structures, V. 127, pp. 159-171. doi: 10.1016/j.engstruct.2016.08.044

El Maaddawy, T.; Soudki, K.; and Topper, T., 2005, “Long-Term Performance of Corrosion-Damaged Reinforced Concrete Beams,” ACI Structural Journal, V. 102, No. 5, Sept.-Oct., pp. 649-656.

El-Sayed, A. K., 2017, “Shear Capacity Assessment of Reinforced Concrete Beams with Corroded Stirrups,” Construction and Building Materials, V. 134, pp. 176-184. doi: 10.1016/j.conbuildmat.2016.12.118

El-Sayed, A. K.; Hussain, R. R.; and Shuraim, A. B., 2016, “Influence of Stirrup Corrosion on Shear Strength of Reinforced Concrete Slender Beams,” ACI Structural Journal, V. 113, No. 6, Nov.-Dec., pp. 1223-1232. doi: 10.14359/51689147

Eyre, J. R., and Nokhasteh, Z., 1992, “Strength Assessment of Corrosion-Damaged Reinforced Concrete Slabs and Beams,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 94, No. 2, pp. 197-203. doi: 10.1680/istbu.1992.18788

Federal Highway Administration (FHWA), 2011, “Bridge Preservation Guide,” Report No. FHWA-HIF-11042, U.S. Department of Transportation, Washington, DC.

Feng, Q.; Visintin, P.; and Oehlers, D. J., 2018, “Effect of Steel Bar Corrosion on Flexural Behaviour through Bond,” Proceedings of the Institution of Civil Engineers. Structures and Buildings, V. 171, No. 5, May, pp. 380-394. doi: 10.1680/jstbu.16.00168

Gewertz, M. W., 1958, “Causes and Repair of Deterioration to a California Bridge Due to Corrosion of Reinforcing Steel in a Marine Environment. Part I: Method of Repair,” Highway Research Board Bulletin 182.

Halstead, L. A., 1955, “The Deterioration of Reinforced Concrete Structures under Coastal Conditions,” Civil Engineering (New York, N.Y.), V. 5, No. 10, pp. 353-372.

Han, S.-J.; Lee, D. H.; Kim, K. S.; Seo, S.-Y.; Moon, J.; and Monteiro, P. J., 2014, “Degradation of Flexural Strength in Reinforced Concrete Members caused by Steel Corrosion,” Construction and Building Materials, V. 54, pp. 572-583. doi: 10.1016/j.conbuildmat.2013.12.101

Higgins, C., and Farrow, W. C. III, 2006, “Tests of Reinforced Concrete Beams with Corrosion-Damaged Stirrups,” ACI Structural Journal, V. 103, No. 1, Jan.-Feb., pp. 133-141.

Higgins, C.; Farrow, W. C. III; and Turan, O. T., 2012, “Analysis of Reinforced Concrete Beams with Corrosion Damaged Stirrups for Shear Capacity,” Structure and Infrastructure Engineering, V. 8, No. 11, pp. 1080-1092.

Imam, A.; Anifowose, F.; and Azad, A. K., 2015, “Residual Strength of Corroded Reinforced Concrete Beams Using an Adaptive Model Based on ANN,” International Journal of Concrete Structures and Materials, V. 9, No. 2, pp. 159-172. doi: 10.1007/s40069-015-0097-4

Imam, A., and Azad, A. K., 2016, “Prediction of Residual Shear Strength of Corroded Reinforced Concrete Beams,” International Journal of Advanced Structural Engineering, V. 8, No. 3, pp. 307-318. doi: 10.1007/s40091-016-0133-x

Imperatore, S.; Leonardi, A.; and Rinaldi, Z., 2016, “Strength Decay of RC Sections for Chloride Attack,” International Journal of Structural Integrity, V. 7, No. 2, pp. 194-212. doi: 10.1108/IJSI-09-2014-0043

Jnaid, F., and Aboutaha, R. S., 2014, “Residual Flexural Strength of Reinforced Concrete Beams with Unbonded Reinforcement,” ACI Structural Journal, V. 111, No. 6, Nov.-Dec., pp. 1419-1430. doi: 10.14359/51686975

Jnaid, F., and Aboutaha, R. S., 2016, “Residual Flexural Strength of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 119, pp. 198-216. doi: 10.1016/j.engstruct.2016.04.018

Johnson, P. M.; Couture, A.; and Nicolet, R., 2007, “Report of the Commission of Inquiry into the Collapse of a Portion of the de la Concorde Overpass,” Gouvernement Du Québec, 222 pp.

Juarez, C. A.; Guevara, B.; Fajardo, G.; and Castro-Borges, P., 2011, “Ultimate and Nominal Shear Strength in Reinforced Concrete Beams Deteriorated by Corrosion,” Engineering Structures, V. 33, No. 12, pp. 3189-3196. doi: 10.1016/j.engstruct.2011.08.014

Kallias, A. N., and Rafiq, M. I., 2010, “Finite Element Investigation of the Structural Response of Corroded RC Beams,” Engineering Structures, V. 32, No. 9, pp. 2984-2994. doi: 10.1016/j.engstruct.2010.05.017

Kearsley, E. P., and Joyce, A., 2014, “Effect of Corrosion Products on Bond Strength and Flexural Behaviour of Reinforced Concrete Slabs,” Journal of the South African Institution of Civil Engineering, V. 56, No. 2, pp. 21-29.

Khan, I.; François, R.; and Castel, A., 2014, “Experimental and Analytical Study of Corroded Shear-Critical Reinforced Concrete Beams,” Materials and Structures, V. 47, No. 9, pp. 1467-1481. doi: 10.1617/s11527-013-0129-y

Kim, S.-H., 2008, “NFEA Modeling of RC Beams Having Exposed Longitudinal Reinforcement: Effects of Debonding on Shear Behavior,” University of Illinois at Urbana-Champaign, Champaign, IL.

Lachemi, M.; Al-Bayati, N.; Sahmaran, M.; and Anil, O., 2014, “The Effect of Corrosion on Shear Behavior of Reinforced Self-Consolidating Concrete Beams,” Engineering Structures, V. 79, pp. 1-12. doi: 10.1016/j.engstruct.2014.07.044

Lewis, D. A., and Copenhagen, W. J., 1959, “Corrosion of Reinforcing Steel In Concrete in Marine Atmospheres,” Corrosion, V. 15, No. 7, pp. 60-66. doi: 10.5006/0010-9312-15.7.60

Mancini, G., and Tondolo, F., 2014, “Effect of Bond Degradation due to Corrosion—A Literature Survey,” Structural Concrete, V. 15, No. 3, pp. 408-418. doi: 10.1002/suco.201300009

Mangat, P. S., and Elgarf, M. S., 1999a, “Flexural Strength of Concrete Beams with Corroding Reinforcement,” ACI Structural Journal, V. 96, No. 1, Jan.-Feb., pp. 149-158.

Mangat, P. S., and Elgarf, M. S., 1999b, “Strength and Serviceability of Repaired Reinforced Concrete Beams undergoing Reinforcement Corrosion,” Magazine of Concrete Research, V. 51, No. 2, pp. 97-112. doi: 10.1680/macr.1999.51.2.97

McLeish, A., 1987, “Structural Assessment: Manual for Life Cycle Aspects of Concrete in Buildings and Structures,” V. 4, Taywood Engineering Ltd., pp. 1-4.

Michel, A.; Pease, B. J.; Geiker, M. R.; Stang, H.; and Olesen, J. F., 2011, “Monitoring Reinforcement Corrosion and Corrosion-Induced Cracking Using Non-Destructive X-Ray Attenuation Measurements,” Cement and Concrete Research, V. 41, No. 11, pp. 1085-1094. doi: 10.1016/j.cemconres.2011.06.006

Ou, Y.-C., and Nguyen, N. D., 2016, “Modified Axial-Shear-Flexure Interaction Approaches for Uncorroded and Corroded Reinforced Concrete Beams,” Engineering Structures, V. 128, pp. 44-54. doi: 10.1016/j.engstruct.2016.09.031

Oyado, M.; Kanakubo, T.; Sato, T.; and Yamamoto, Y., 2011, “Bending Performance of Reinforced Concrete Member Deteriorated by Corrosion,” Structure and Infrastructure Engineering, V. 7, No. 1-2, pp. 121-130. doi: 10.1080/15732471003588510

Palsson, R., and Mirza, M. S., 2002, “Mechanical Response of Corroded Steel Reinforcement of Abandoned Concrete Bridge,” ACI Structural Journal, V. 99, No. 2, Mar.-Apr., pp. 157-162.

Potisuk, T.; Higgins, C. C.; Miller, T. H.; and Yim, S. C., 2011, “Finite Element Analysis of Reinforced Concrete Beams with Corrosion Subjected to Shear,” Advances in Civil Engineering, V. 2011, pp. 1-14. doi: 10.1155/2011/706803

Rodriguez, J.; Ortega, L. M.; and Casal, J., 1994, “Corrosion of Reinforcing Bars and Service Life of Reinforced Concrete Structures: Corrosion and Bond Deterioration,” International Conference on Concrete across Borders, Odense, Denmark, pp. 315-326.

Rodriguez, J.; Ortega, L. M.; and Casal, J., 1997, “Load Carrying Capacity of Concrete Structures with Corroded Reinforcement,” Construction and Building Materials, V. 11, No. 4, pp. 239-248. doi: 10.1016/S0950-0618(97)00043-3

Sahmaran, M.; Anil, O.; Lachemi, M.; Yildirim, G.; Ashour, A. F.; and Acar, F., 2015, “Effect of Corrosion on Shear Behavior of Reinforced Engineered Cementitious Composite Beams,” ACI Structural Journal, V. 112, No. 6, Nov.-Dec., pp. 771-782. doi: 10.14359/51687749

Schmitt, G., 2009, “Global Needs for Knowledge Dissemination, Research, and Development in Materials Deterioration and Corrosion Control,” World Corrosion Organization, New York.

Shayanfar, M. A.; Ghalehnovi, M.; and Safiey, A., 2007, “Corrosion Effects on Tension Stiffening Behavior of Reinforced Concrete,” Computers and Concrete, V. 4, No. 5, Oct., pp. 403-424. doi: 10.12989/cac.2007.4.5.403

Shayanfar, M. A., and Safiey, A., 2008, “A New Approach for Nonlinear Finite Element Analysis of Reinforced Concrete Structures with Corroded Reinforcements,” Computers and Concrete, V. 5, No. 2, pp. 155-174. doi: 10.12989/cac.2008.5.2.155

Stratfull, R. F., 1957, “The Corrosion of Steel in a Reinforced Concrete Bridge,” Corrosion, V. 13, No. 3, pp. 43-48. doi: 10.5006/0010-9312-13.3.43

Tahershamsi, M., 2016, “Structural Effects of Reinforcement Corrosion in Concrete Structures,” Chalmers University of Technology, Gothenburg, Sweden.

Tahershamsi, M.; Zandi, K.; Lundgren, K.; and Plos, M., 2014, “Anchorage of Naturally Corroded Bars in Reinforced Concrete Structures,” Magazine of Concrete Research, V. 66, No. 14, pp. 729-744. doi: 10.1680/macr.13.00276

Tanaka, Y.; Kawano, H.; Watanabe, H.; and Kimura, T., 2001, “Chloride-Induced Deterioration and Its Influence on Load-Carrying Capacity of Post-Tensioned Concrete Bridges,” Third International Conference on Concrete under Severe Conditions—Environment and Loading, Citeseer, pp. 495-502.

Ting, S.-C., and Nowak, A. S., 1991, “Effect of Reinforcing Steel Area Loss on Flexural Behavior of Reinforced Concrete Beams,” ACI Structural Journal, V. 88, No. 3, May-June, pp. 309-314.

Toongoenthong, K., and Maekawa, K., 2005, “Multi-mechanical Approach to Structural Performance Assessment of Corroded RC Members in Shear,” Journal of Advanced Concrete Technology, V. 3, No. 1, pp. 107-122. doi: 10.3151/jact.3.107

Torres-Acosta, A. A.; Fabela-Gallegos, M. J.; Munoz-Noval, A.; Vázquez-Vega, D.; Hernandez-Jimenez, J. R.; and Martinez-Madrid, M., 2004, “Influence of Corrosion on the Structural Stiffness of Reinforced Concrete Beams,” Corrosion, V. 60, No. 9, pp. 862-872. doi: 10.5006/1.3287868

Torres-Acosta, A. A.; Navarro-Gutierrez, S.; and Terán-Guillén, J., 2007, “Residual Flexure Capacity of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 29, No. 6, pp. 1145-1152. doi: 10.1016/j.engstruct.2006.07.018

Tremper, B.; Beaton, J. L.; and Stratfull, R. F., 1958, “Causes and Repair of Deterioration to a California Bridge Due to Corrosion of Reinforcing Steel in a Marine Environment. Part II: Fundamental Factors Causing Corrosion,” Highway Research Board Bulletin 182.

Vidal, T.; Castel, A.; and François, R., 2007, “Corrosion Process and Structural Performance of a 17-Year-Old Reinforced Concrete Beam Stored in Chloride Environment,” Cement and Concrete Research, V. 37, No. 11, pp. 1551-1561. doi: 10.1016/j.cemconres.2007.08.004

Vu, H. H.; Vu, N. A.; and François, R., 2014, “Effect of Corrosion of Tensile Rebars and Stirrups on the Flexural Stiffness of Reinforced Concrete Members,” European Journal of Environmental and Civil Engineering, V. 18, No. 3, pp. 358-376. doi: 10.1080/19648189.2014.881759

Wakeman, C. M.; Dockweiler, E. V.; Stover, H. E.; and Whiteneck, L. L., 1958, “Use of Concrete in Marine Environments,” ACI Journal Proceedings, V. 54, pp. 841-856.

Wang, L.; Li, C.; and Yi, J., 2015a, “An Experiment Study on Behavior of Corrosion RC Beams with Different Concrete Strength,” Journal of Coastal Research, V. 73, pp. 259-264. doi: 10.2112/SI73-046.1

Wang, L.; Ma, Y.; Ding, W.; Zhang, J.; and Liu, Y., 2015b, “Comparative Study of Flexural Behavior of Corroded Beams with Different Types of Steel Bars,” Journal of Performance of Constructed Facilities, V. 29, No. 6, p. 04014163 doi: 10.1061/(ASCE)CF.1943-5509.0000661

Wang, X.-H.; Gao, X.-H.; Li, B.; and Deng, B.-R., 2011, “Effect of Bond and Corrosion within Partial Length on Shear Behaviour and Load Capacity of RC Beam,” Construction and Building Materials, V. 25, No. 4, pp. 1812-1823. doi: 10.1016/j.conbuildmat.2010.11.081

Wood, J. G. M., 2008, “Implications of the Collapse of the de la Concorde Overpass,” Structural Engineering, V. 86, No. 1, pp. 16-18.

Xia, J.; Jin, W.-L.; and Li, L.-Y., 2012, “Effect of Chloride-Induced Reinforcing Steel Corrosion on the Flexural Strength of Reinforced Concrete Beams,” Magazine of Concrete Research, V. 64, No. 6, pp. 471-485. doi: 10.1680/macr.10.00169

Xu, S.; Zhang, Z.; Li, R.; and Qiu, B., 2017, “Experimental Study on the Shear Behavior of RC Beams with Corroded Stirrups,” Journal of Advanced Concrete Technology, V. 15, No. 4, pp. 178-189. doi: 10.3151/jact.15.178

Xue, X.; Seki, H.; and Song, Y., 2014, “Shear Behavior of RC Beams Containing Corroded Stirrups,” Advances in Structural Engineering, V. 17, No. 2, pp. 165-177. doi: 10.1260/1369-4332.17.2.165

Yu, L.; François, R.; Dang, V. H.; L’Hostis, V.; and Gagné, R., 2015, “Development of Chloride-Induced Corrosion in Pre-cracked RC Beams under Sustained Loading: Effect of Load-Induced Cracks, Concrete Cover, and Exposure Conditions,” Cement and Concrete Research, V. 67, pp. 246-258. doi: 10.1016/j.cemconres.2014.10.007

Yuan, Y.; Ji, Y.; and Shah, S. P., 2007, “Comparison of Two Accelerated Corrosion Techniques for Concrete Structures,” ACI Structural Journal, V.  104, No. 3, May-June, pp. 344-347.

Zhang, W.; Ye, Z.; and Gu, X., 2017, “Effects of Stirrup Corrosion on Shear Behaviour of Reinforced Concrete Beams,” Structure and Infrastructure Engineering, V. 13, No. 8, pp. 1081-1092. doi: 10.1080/15732479.2016.1243563

Zhang, X.; Wang, L.; Zhang, J.; and Liu, Y., 2016, “Bond Degradation-Induced Incompatible Strain between Steel Bars and Concrete in Corroded RC Beams,” Journal of Performance of Constructed Facilities, V. 30, No. 6, p. 04016058 doi: 10.1061/(ASCE)CF.1943-5509.0000921

Zhou, Y.; Gencturk, B.; Willam, K.; and Attar, A., 2015, “Carbonation-Induced and Chloride-Induced Corrosion in Reinforced Concrete Structures,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 9, p. 04014245 doi: 10.1061/(ASCE)MT.1943-5533.0001209

Zhu, W., and François, R., 2014, “Corrosion of the Reinforcement and its Influence on the Residual Structural Performance of a 26-Year-Old Corroded RC Beam,” Construction and Building Materials, V. 51, pp. 461-472. doi: 10.1016/j.conbuildmat.2013.11.015

Zhu, W.; François, R.; Cleland, D.; and Coronelli, D., 2015, “Failure Mode Transitions of Corroded Deep Beams Exposed to Marine Environment for Long Period,” Engineering Structures, V. 96, pp. 66-77. doi: 10.1016/j.engstruct.2015.04.004

Zhu, W.; François, R.; Coronelli, D.; and Cleland, D., 2013, “Effect of Corrosion of Reinforcement on the Mechanical Behaviour of Highly Corroded RC Beams,” Engineering Structures, V. 56, pp. 544-554. doi: 10.1016/j.engstruct.2013.04.017

Zhu, W.; François, R.; Fang, Q.; and Zhang, D., 2016, “Influence of Long-Term Chloride Diffusion in Concrete and the Resulting Corrosion of Reinforcement on the Serviceability of RC Beams,” Cement and Concrete Composites, V. 71, pp. 144-152. doi: 10.1016/j.cemconcomp.2016.05.003


ALSO AVAILABLE IN:

Electronic Structural Journal