Size Effect of Squat Shear Walls Extrapolated by Microplane Model M7

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Size Effect of Squat Shear Walls Extrapolated by Microplane Model M7

Author(s): Mohammad Rasoolinejad and Zdenek P. Bažant

Publication: Structural Journal

Volume: 116

Issue: 3

Appears on pages(s): 75-84

Keywords: crack band model; cracking; failure mechanism; finite element analysis; fracture; microplane model; shear wall; size effect

DOI: 10.14359/51714478

Date: 5/1/2019

Abstract:
Recent earthquakes revealed poor performance of very tall shear walls. This is no surprise because the design for size effect has long been hampered by the lack of large-size tests and by mingling of different concretes and different test parameters among the existing test data. Fortunately, recent progress in material modeling and computer power permits overcoming this obstacle by extending the data to large sizes computationally. Herein, a large classical set of reduced-scale shear wall tests performed (at ETH) are selected and used to verify and calibrate the finite element simulations with the crack band model, in which a powerful constitutive damage model—microplane model M7—is implemented. Then the calibrated computer code is used to predict the strength and ductility of much larger shear walls. As expected, the size effect is found to occur if the shear in concrete controls the failure load but not if the steel bar yielding does. Increasing the reinforcement ratio may compromise ductility; it may cause the shear in concrete to control the peak load and the failure to occur before the steel bars begin to yield. Increasing the height-to-width aspect ratio of the wall is shown to lead to flexural failure, which does not show size effect on the shear wall strength. Increasing the wall size may change the failure mechanism, cause the concrete to fail at a lower stress, and shorten or remove the yield plateau. Adding horizontal reinforcing bars to vertical ones tends to prevent inclined shear cracks in the web, although it has little effect on sliding shear. Computer simulations of the present type are helpful for checking the design of large shear walls.

Related References:

1. Barda, F.; Hanson, J. M.; and Corley, W. G., “Shear Strength of Low-Rise Walls with Boundary Elements,” Reinforced Concrete Structures in Seismic Zones, SP-53, N. M. Hawkins and D. Mitchell, eds., American Concrete Institute, Farmington Hills, MI, 1977, pp. 149-202.

2. Cardenas, A.; Russell, H.; and Corley, W., “Strength of Low-Rise Structural Walls,” Reinforced Concrete Structures Subjected to Wind and Earthquake Forces, SP-63, American Concrete Institute, Farmington Hills, MI, 1980, pp. 221-242.

3. Dabbagh, H., “Strength and Ductility of High-Strength Concrete Shear Walls under Reversed Cyclic Loading,” PhD thesis, University of New South Wales, Sydney, NSW, Australia.

4. Farvashany, F. E.; Foster, S. J.; and Rangan, B. V., “Strength and Deformation of High-Strength Concrete Shearwalls,” ACI Structural Journal, V. 105, No. 1, Jan.-Feb. 2008, pp. 21-29.

5. Gulec, C. K.; Whittaker, A. S.; and Stojadinovic, B., “Shear Strength of Squat Rectangular Reinforced Concrete Walls,” ACI Structural Journal, V. 105, No. 4, July-Aug. 2008, pp. 488-497.

6. Gupta, A., and Rangan, B. V., “High-Strength Concrete (HSC) Structural Walls,” ACI Structural Journal, V. 95, No. 2, Mar.-Apr. 1998, pp. 194-204.

7. Hidalgo, P.; Jordan, R.; and Martinez, M., “An Analytical Model to Predict the Inelastic Seismic Behavior of Shear-Wall, Reinforced Concrete Structures,” Engineering Structures, V. 24, No. 1, 2002, pp. 85-98. doi: 10.1016/S0141-0296(01)00061-X

8. Hidalgo, P. A.; Ledezma, C. A.; and Jordan, R. M., “Seismic Behavior of Squat Reinforced Concrete Shear Walls,” Earthquake Spectra, V. 18, No. 2, 2002, pp. 287-308. doi: 10.1193/1.1490353

9. Lefas, I. D., and Kotsovos, M. D., “Strength and Deformation Characteristics of Reinforced Concrete Walls under Load Reversals,” ACI Structural Journal, V. 87, No. 6, Nov.-Dec. 1990, pp. 716-726.

10. Lefas, I. D.; Kotsovos, M. D.; and Ambraseys, N. N., “Behavior of Reinforced Concrete Structural Walls: Strength, Deformation Characteristics, and Failure Mechanism,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 23-31.

11. Maier, J., and Thürlimann, B., “Bruchversuche an Stahlbetonscheiben,” Bericht/Institut für Baustatik und Konstruktion, ETH Zürich, Zürich, Switzerland, V. 8003, No. 1, 1985.

12. Wood, S. L., “Shear Strength of Low-Rise Reinforced Concrete Walls,” ACI Structural Journal, V. 87, No. 1, Jan.-Feb. 1990, pp. 99-107.

13. Bažant, Z. P., “Size Effect in Shear Failure of Longitudinally Reinforced Beams,” ACI Journal Proceedings, V. 81, No. 5, Sept-.Oct. 1984, pp. 456-468.

14. Yu, Q.; Le, J.-L.; Hubler, M. H.; Wendner, R.; Cusatis, G.; and Bažant, Z. P., “Comparison of Main Models for Size Effect on Shear Strength of Reinforced and Prestressed Concrete Beams,” Structural Concrete, V. 17, No. 5, 2016, pp. 778-789. doi: 10.1002/suco.201500126

15. Bažant, Z. P., and Cao, Z., “Size Effect in Punching Shear Failure of Slabs,” ACI Structural Journal, V. 84, No. 1, Jan.-Feb. 1987, pp. 44-53.

16. Dönmez, A., and Bažant, Z. P., “Size Effect on Punching Strength of Reinforced Concrete Slabs with and without Shear Reinforcement,” ACI Structural Journal, V. 114, No. 4, July-Aug. 2017, p. 875. doi: 10.14359/51689719

17. Vorel, J., and Bažant, Z. P., “Size Effect in Flexure of Prestressed Concrete Beams Failing by Compression Softening.” Journal of Structural Engineering, ASCE, V. 140, No. 10, 2004, pp. 04014068-1-04014068.

18. Paulay, T., and Priestley, M. N., Seismic Design of Reinforced Concrete and Masonry Buildings, Wiley, New York, 1992.

19. Bažant, Z. P., and Planas, J., Fracture and Size Effect in Concrete and Other Quasibrittle Materials, CRC Press, Boca Raton, FL, 1997.

20. Oesterle, R. G.; Fiorato, A. E.; Johal, L. S.; Carpenter, J. E.; Russell, H. G.; and Corley, W. G., 1976, “Earthquake Resistant Structural Walls—Test of Isolated Walls,” Report No. GI-43880/RA-760815, National Science Foundation, Arlington, VA, 315 pp.

21. Ghorbani-Renani, I.; Velev, N.; Tremblay, R.; Palermo, D.; Massicotte, B.; and Léger, P., “Modeling and Testing Influence of Scaling Effects on Inelastic Response of Shear Walls,” ACI Structural Journal, V. 106, No. 3, May-June 2009, pp. 358-367.

22. Bažant, Z. P., “Size Effect In Blunt Fracture: Concrete, Rock, Metal,” Journal of Engineering Mechanics, ASCE, V. 110, No. 4, 1984, pp. 518-535. doi: 10.1061/(ASCE)0733-9399(1984)110:4(518)

23. Bažant, Z. P., “Crack Band Model for Fracture of Geomaterials,” Proceedings of the 4th International Conference on Num. Meth. in Geomechanics, Z. Eisenstein, ed., University of Alberta, Edmonton, AB, Canada, V. 3, 1982, 1137-1152.

24. Bažant, Z. P., and Oh, B. H., “Crack Band Theory for Fracture of Concrete,” Materiales de Construcción, V. 16, No. 3, 1983, pp. 155-177. doi: 10.1007/BF02486267

25. Bažant, Z. P., “Microplane Model for Strain-Controlled Inelastic Behavior,” Chapter 3, Mechanics of Engineering Materials, C. S. Desai and R. H. Gallagher, eds., John Wiley, London, UK, 1984, pp. 45-59

26. Bažant, Z. P., and Oh, B.-H., “Microplane Model for Progressive Fracture of Concrete and Rock,” Journal of Engineering Mechanics, ASCE, V. 111, No. 4, 1985, pp. 559-582. doi: 10.1061/(ASCE)0733-9399(1985)111:4(559)

27. Caner, F. C., and Bažant, Z. P., “Microplane Model M7 for Plain Concrete. I: Formulation,” Journal of Engineering Mechanics, ASCE, V. 139, No. 12, 2012, pp. 1714-1723. doi: 10.1061/(ASCE)EM.1943-7889.0000570

28. Caner, F. C., and Bažant, Z. P., “Microplane Model M7 for Plain Concrete. II: Calibration and Verification,” Journal of Engineering Mechanics, ASCE, V. 139, No. 12, 2013, pp. 1724-35.

29. Taylor, G. I., “Plastic Strain in Metals,” Our Inst Metals, V. 62, 1938, pp. 307-324.

30. Karsan, I. D., and Jirsa, J. O., “Behavior of Concrete under Compressive Loadings,” Journal of the Structural Division, ASCE, V. 95, No. 12, 1969, pp. 2543-2564.

31. Yankelevsky, D. Z., and Reinhardt, H. W., “Response of Plain Concrete to Cyclic Tension,” ACI Materials Journal, V. 84, No. 5, Sept.-Oct. 1987, pp. 365-373.

32. Yankelevsky, D. Z., and Reinhardt, H. W., “Uniaxial Behavior of Concrete in Cyclic Tension,” Journal of Structural Engineering, ASCE, V. 115, No. 1, 1989, pp. 166-182. doi: 10.1061/(ASCE)0733-9445(1989)115:1(166)

33. Bažant, Z. P.; Şener, S.; and Prat, P. C., “Size Effect Tests of Torsional Failure of Plain and Reinforced Concrete Beams,” Materials and Structures, V. 21, No. 6, 1988, pp. 425-430. doi: 10.1007/BF02472322

34. Kirane, K.; Singh, K. D.; and Bažant, Z. P., “Size Effect in Torsional Strength of Plain and Reinforced Concrete,” ACI Structural Journal, V. 113, No. 6, Nov.-Dec. 2016, pp. 1253-1262. doi: 10.14359/51689149

35. Bažant, Z., and Kwon, Y., “Failure of Slender and Stocky Reinforced Concrete Columns: Tests of Size Effect,” Materials and Structures, V. 27, No. 2, 1994, pp. 79-90. doi: 10.1007/BF02472825

36. Brocca, M., and Bažant, Z., P., “Size Effect in Concrete Columns: Finite-Element Analysis with Microplane Model,” Journal of Structural Engineering, ASCE, V. 127, No. 12, 2001, pp. 1382-1390. doi: 10.1061/(ASCE)0733-9445(2001)127:12(1382)

37. Bažant, Z. P., and Cao, Z., “Size Effect of Shear Failure in Prestressed Concrete Beams,” ACI Journal Proceedings, V. 83, No. 2, Mar.-Apr. 1986, pp. 260-268.

38. Bažant, Z. P., and Kazemi, M. T., “Size Effect on Diagonal Shear Failure of Beams without Stirrups,” ACI Structural Journal, V. 88, No. 3, Mar.-Apr. 1991, pp. 268-276.

39. Bažant, Z. P., and Le, J.-L., “Probabilistic Mechanics of Quasibrittle Structures: Strength, Lifetime, and Size Effect,” Cambridge University Press, London, UK, 2017.


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer