Seismic Performance of Flexural Reinforced Concrete Columns with Corroded Reinforcement

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Seismic Performance of Flexural Reinforced Concrete Columns with Corroded Reinforcement

Author(s): Ngoc Son Vu and Bing Li

Publication: Structural Journal

Volume: 115

Issue: 5

Appears on pages(s): 1253-1266

Keywords: corrosion; flexural strength; reinforced concrete column; reinforcement; shear strength

DOI: 10.14359/51702372

Date: 9/1/2018

Abstract:
This paper presents an experimental study carried out on eight full-scale uncorroded and corroded reinforced concrete columns that were subjected to simulated seismic loading to investigate the effects of reinforcement corrosion on the seismic behavior of columns that failed in flexure. The main variables are the corrosion levels of reinforcement and applied axial force ratios. The seismic performance of test specimens was assessed in terms of crack pattern, hysteretic response, yield displacement, lateral load resistance, drift capacity, displacement ductility, and energy dissipation capacity. The results highlighted that the corroded columns suffered a significant degradation of strength and lateral drift capacity as compared to uncorroded columns. In addition, it is noteworthy to observe that the failure mode of corroded columns switched from flexural failure to flexural-shear failure and sudden axial failure when they are highly corroded and subjected to high axial force. An empirical equation based on the maximum pit depth of corroded longitudinal reinforcing bars was proposed to predict the residual flexural strength of corroded columns. Furthermore, based on the shear strength model proposed in ASCE/SEI 41-13, methods were proposed to estimate the shear strength of corroded columns failed in flexural-shear failure and axial failure, which consider the contribution reductions to shear strength of transverse reinforcement and concrete due to corrosion. Among these methods, the shear strength of corroded columns estimated based on the corrosion mass loss and average residual cross-sectional area was not conservative as compared to the test results. In contrast, the shear strength of corroded columns predicted using the minimum residual cross-sectional area of transverse reinforcing bars showed good and reliable correlation with the experimental results.

Related References:

1. Meda, A.; Mostosi, S.; Rinaldi, Z.; and Riva, P., “Experimental Evaluation of the Corrosion Influence on the Cyclic Behaviour of RC Columns,” Engineering Structures, V. 76, 2014, pp. 112-123. doi: 10.1016/j.engstruct.2014.06.043

2. Goksu, C., and Ilki, A., “Seismic Behavior of Reinforced Concrete Columns with Corroded Deformed Reinforcing Bars,” ACI Structural Journal, V. 113, No. 5, Sept.-Oct. 2016, pp. 1053-1064.

3. Bousias, S. N.; Triantafillou, T. C.; Fardis, M. N.; Spathis, L. A.; and O’Regan, B. A., “Fiber-Reinforced Polymer Retrofitting of Rectangular Reinforced Concrete Columns with or without Corrosion,” ACI Structural Journal, V. 101, No. 4, July-Aug. 2004, pp. 512-520.

4. Li, J.; Gong, J.; and Wang, L., “Seismic Behavior of Corrosion-Damaged Reinforced Concrete Columns Strengthened Using Combined Carbon Fiber-Reinforced Polymer and Steel Jacket,” Construction and Building Materials, V. 23, No. 7, 2009, pp. 2653-2663. doi: 10.1016/j.conbuildmat.2009.01.003

5. Meda, A.; Mostosi, S.; Rinaldi, Z.; and Riva, P., “Corroded RC Columns Repair and Strengthening with High Performance Fiber Reinforced Concrete Jacket,” Materials and Structures, V. 49, No. 5, 2016, pp. 1967-1978. doi: 10.1617/s11527-015-0627-1

6. ASCE/SEI 41-13, “Seismic Evaluation and Retrofit of Existing Buildings,” American Society of Civil Engineers, Reston, VA, 2014, 518 pp.

7. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, 2014, 520 pp.

8. ASTM G1-03, “Standard Practice for Preparing, Cleaning, and Evaluating Corrosion Test Specimens,” ASTM International, West Conshohocken, PA, 2003, 9 pp.

9. Ou, Y. C., and Chen, H. H., “Cyclic Behavior of Reinforced Concrete Beams with Corroded Transverse Steel Reinforcement,” Journal of Structural Engineering, ASCE, V. 140, No. 9, 2014, pp. 1-10. doi: 10.1061/(ASCE)ST.1943-541X.0000932

10. Ou, Y. C., and Nguyen, N. D., “Influences of Location of Reinforcement Corrosion on Seismic Performance of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 126, 2016, pp. 210-223. doi: 10.1016/j.engstruct.2016.07.048

11. Sezen, H., and Moehle, J. P., “Shear Strength Model for Lightly Reinforced Concrete Columns,” Journal of Structural Engineering, ASCE, V. 130, No. 11, 2004, pp. 1692-1703. doi: 10.1061/(ASCE)0733-9445(2004)130:11(1692)

12. Sezen, H., “Seismic Behavior and Modeling of Reinforced Concrete Building Columns,” PhD thesis, Department of Civil and Environmental Engineering, University of California, Berkeley, Berkeley, CA, 2002, 336 pp.

13. Torres-Acosta, A. A.; Navarro-Gutierrez, S.; and Teran-Guillen, J., “Residual Flexure Capacity of Corroded Reinforced Concrete Beams,” Engineering Structures, V. 29, No. 6, 2007, pp. 1145-1152. doi: 10.1016/j.engstruct.2006.07.018

14. Ou, Y. C.; Tsai, L. L.; and Chen, H. H., “Cyclic Performance of Large-Scale Corroded Reinforced Concrete Beams,” Earthquake Engineering & Structural Dynamics, V. 41, No. 4, 2012, pp. 593-604. doi: 10.1002/eqe.1145

15. El-Sayed, A. K.; Hussain, R. R.; and Shuraim, A. B., “Influence of Stirrup Corrosion on Shear Strength of Reinforced Concrete Slender Beams,” ACI Structural Journal, V. 113, No. 6, Nov.-Dec. 2016, pp. 1223-1232.

16. Du, Y. G.; Clark, L. A.; and Chan, A. H. C., “Residual Capacity of Corroded Reinforcing Bars,” Magazine of Concrete Research, V. 57, No. 3, 2005, pp. 135-147. doi: 10.1680/macr.2005.57.3.135

17. Hsu, T. T. C., and Mo, Y. L., Unified Theory of Concrete Structures, Wiley, West Sussex, UK, 2010, 518 pp.


ALSO AVAILABLE IN:

Electronic Structural Journal