Can We Design Concrete to Survive Nuclear Environments?

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Can We Design Concrete to Survive Nuclear Environments?

Author(s): Kimberly E. Kurtis, Yunping Xi, Michał A. Glinicki, John L. Provis, Eric R. Giannini, and Tengfei Fu

Publication: Concrete International

Volume: 39

Issue: 11

Appears on pages(s): 29-35

Keywords: reactor, aging, durability, waste

DOI: 10.14359/51701248

Date: 11/1/2017

Abstract:
This article is a summary of a panel discussion that took place during the 123 Forum session at The Fall 2016 ACI Concrete Convention and Exposition in Philadelphia, PA. The panelists and one of the moderators have been actively involved in research efforts to improve understanding of the effects of nuclear environments on concrete and cementitious grouts as well as the ability to monitor degradation of nuclear structures.

Related References:

1. “Power Reactor Information System (PRIS),” International Atomic Energy Agency, Vienna, Austria, www.iaea.org/pris.

2. Le Pape, Y.; Giorla, A.; and Sanahuja, J., “Combined Effects of Temperature and Irradiation on Concrete Damage,” Journal of Advanced Concrete Technology, V. 14, No. 3, Mar. 2016, pp. 70-86.

3. Hilsdorf, H.K.; Kropp, J.; and Koch, H.J., “The Effects of Nuclear Radiation on the Mechanical Properties of Concrete,” Douglas McHenry International Symposium on Concrete and Concrete Structures, SP-55, American Concrete Institute, Farmington Hills, MI, 1978, pp. 223-254.

4. Field, K.G.; Remec, I.; and LePape, Y., “Radiation Effects in Concrete for Nuclear Power Plants—Part I: Quantification of Radiation Exposure and Radiation Effects,” Nuclear Engineering and Design, V. 282, Feb. 2015, pp. 126-143.

5. Rosseel, T.M.; Maruyama, I.; Le Pape, Y.; Kontani, O.; Giorla, A.; Wall, J.J.; Sircar, M.; Andrade, C.; Ordonez, M.; and Remec, I., “Review of the Current State of Knowledge on the Effects of Radiation on Concrete,” Journal of Advanced Concrete Technology, V. 14, No. 7, July 2016, pp. 368-383.

6. “International Energy Statistics,” U.S. Energy Information Administration (EIA), Washington, DC, www.eia.gov/beta/international/data/browser.

7. “Total Energy,” U.S. Energy Information Administration (EIA), Washington, DC, www.eia.gov/totalenergy/data/browser.

8. “Energy Policy Act of 2005,” www.gpo.gov/fdsys/pkg/PLAW-109publ58/html/PLAW-109publ58.htm.

9. “NRC Datasets,” United States Nuclear Regulatory Commission (U.S.NRC), www.nrc.gov/reading-rm/doc-collections/datasets. (last accessed Feb. 21, 2017)

10. “Vermont Yankee Nuclear Plant Closure in 2014 Will Challenge New England Energy Markets,” U.S. Energy Information Administration (EIA), Washington, DC, www.eia.gov/todayinenergy/detail.php?id=12851.

11. “Fort Calhoun Becomes Fifth U.S. Nuclear Plant to Retire in Past Five Years,” U.S. Energy Information Administration (EIA), Washington, DC, www.eia.gov/todayinenergy/detail.php?id=28572.

12. Dolphyn, B.P., “Laminar Cracking in Post-Tensioned Concrete Nuclear Containment Buildings,” PhD thesis, Georgia Institute of Technology, Atlanta, GA, 2016, pp. 522, https://smartech.gatech.edu/bitstream/handle/.../DOLPHYN-DISSERTATION-2016.pdf.

13. Penn, I., “Duke Energy Announces Closing of Crystal River Nuclear Power Plant,” Tampa Bay Times, Feb. 5, 2013, www.tampabay.com/news/business/energy/duke-energy-announces-closing-of-crystal-rivernuclear-power-plant/1273794.

14. Krauss, P.D., “Repair Materials and Techniques for Concrete Structures in Nuclear Power Plants,” ORNL/NRC/LTR-93/28, Oak Ridge National Laboratory, Oak Ridge, TN, 1994, 205 pp.

15. Shah, V.N., and Hookham, C.J., “Long-term Aging of Light Water Reactor Concrete Containments,” Nuclear Engineering and Design, V. 185, No. 1, Sept. 1998, pp. 51-81.

16. Naus, D.J., “Primer on Durability of Nuclear Power Plant Reinforced Concrete Structures—A Review of Pertinent Factors,” NUREG/CR-6927, Oak Ridge National Laboratory, Oak Ridge, TN, 2007, 112 pp.

17. Ashar, H.; Naus, D.J.; and Tan, C.P., “Prestressed Concrete in U.S. Nuclear Power Plants (Part 1),” Concrete International, V. 16, No. 5, May 1994, pp. 30-34.

18. Ashar, H.; Naus, D.J.; and Tan, C.P., “Prestressed Concrete in U.S. Nuclear Power Plants (Part 2),” Concrete International, V. 16, No. 6, June 1994, pp. 58-61.

19. Naus, D.J., “Concrete Component Aging and its Significance Relative to Life Extension of Nuclear Power Plants,” NUREG/CR-4652, Oak Ridge National Laboratory, Oak Ridge, TN, 1986, 158 pp.

20. Naus, D.J.; Oland, C.B.; Ellingwood, B.; Norris, W.E.; and Graves, H.L. III, “Management of Aging of Nuclear Power Plant Containment Structures,” International Conference on Engineering Structural Integrity Assessment, Cambridge, UK, Sept. 12-14, 1998, 8 pp.

21. Graves, H.; LePape, Y; Naus, D.; Rashid, J.; Saouma, V.; Sheikh, A.; and Wall, J., “Expanded Materials Degradation Assessment (EMDA): Aging of Concrete and Civil Structures,” NUREG/CR-7153, V. 4, Oak Ridge National Laboratory, Oak Ridge, TN, 2014, 137 pp.

22. Bažant, Z.P., and Xi, Y., “Drying Creep of Concrete: Constitutive Model and New Experiments Separating its Mechanisms,” Materials and Structures, V. 27, No. 1, Jan. 1994, pp. 3-14.

23. Khoury, G.A.; Grainger, B.N.; and Sullivan, P.J.E., “Strain of Concrete during First Heating to 600°C under Load,” Magazine of Concrete Research, V. 37, No. 133, Dec. 1985, pp. 195-215.

24. Willam, K.; Xi, Y.; and Naus, D., “A Review of the Effects of Radiation on Microstructure and Properties of Concretes Used in Nuclear Power Plants,” NUREG/CR-7171, U.S. Nuclear Regulatory Commission, Washington, DC, Nov. 2013, 131 pp.

25. Pabalan, R.T.; Yang, L.; and Chiang, K.-T.K., “Boric Acid Degradation of Reinforced Concrete,” Center for Nuclear Waste Regulatory Analyses, San Antonio, TX, 2011, www.nrc.gov/docs/ML1210/ML12103A065.pdf.

26. Baran, T.; Glinicki, M.A.; and Jóźwiak-Niedźwiedzka, D., “The Properties of Special Cements for Shielding Constructions in Nuclear Power Plants, Cement-Wapno-Beton, V. 21, No. 4, July-Aug. 2016, pp. 207-216.

27. Zerger, B., and Noël, M., “Nuclear Power Plant Construction: What Can Be Learned from Past and On-going Projects?” Nuclear Engineering and Design, V. 241, No. 8, Aug. 2011, pp. 2916-2926.

28. Joyce, M.J.; Garnsey, R.; and Nickson, I., Nuclear Lessons Learned, Royal Academy of Engineering, London, UK, 2010, 80 pp., www.raeng.org.uk/nll.

29. Saouma, V.E., and Hariri-Ardebili, M.A., “A Proposed Aging Management Program for Alkali Silica Reactions in a Nuclear Power Plant,” Nuclear Engineering and Design, V. 277, Oct. 2014, pp. 248-264.

30. Jóźwiak-Niedźwiedzka, D.; Jaskulski, R.; and Glinicki, M.A., “Application of Image Analysis to Identify Quartz Grains in Heavy Aggregates Susceptible to ASR in Radiation Shielding Concrete,” Materials, V. 9, No. 4, Apr. 2016, 14 pp.

31. Kubissa, W., and Glinicki, M.A., “Influence of Internal Relative Humidity and Mix Design of Radiation Shielding Concrete on Air Permeability Index,” Construction and Building Materials, V. 147, Aug. 2017, pp. 352-361.

32. Glinicki, M.A.; Jaskulski, R.; Dąbrowski, M.; and Ranachowski, Z., “Determination of Thermal Properties of Hardening Concrete for Massive Nuclear Shielding Structures,” Fourth International Conference on Sustainable Construction Materials & Technologies, Las Vegas, NV, Aug. 7-11, 2016, 9 pp.

33. “The Behaviours of Cementitious Materials in Long Term Storage and Disposal of Radioactive Waste, Results of a Coordinated Research Project,” IAEA-TECDOC-1701, International Atomic Energy Agency (IAEA), Vienna, Austria, 2013, 61 pp., www-pub.iaea.org/MTCD/Publications/PDF/TE-1701_web.pdf.

34. Glasser, F.P., “Application of Inorganic Cements to the Conditioning and Immobilisation of Radioactive Wastes,” Handbook of Advanced Radioactive Waste Conditioning Technologies, Woodhead Publishing, Cambridge, UK, 2011, pp. 67-135.

35. Bouniol, P., and Bjergbakke, E., “A Comprehensive Model to Describe Radiolytic Processes in Cement Medium,” Journal of Nuclear Materials, V. 372, No. 1, Jan. 2008, pp. 1-15.

36. Angus, M.J.; Hayes, M.; Orr, R.; and Corkhill, C., “Behaviour of Alpha Emitters in Cement,” Paper No. 16139, Waste Management WM2016 Conference, Phoenix, AZ, Mar. 6-10, 2016.

37. Richardson, I.G.; Groves, G.W.; and Wilding, C.R., “Effect of γ-Radiation on the Microstructure and Microchemistry of GGBFS/OPC Cement Blends,” Materials Research Society Symposium Proceedings, V. 176, 1989, pp. 31-39.

38. Mobasher, N.; Bernal, S.A.; Kinoshita, H.; Sharrad, C.A.; and Provis, J.L., “Gamma Irradiation Resistance of an Early Age Slag-Blended Cement Matrix for Nuclear Waste Encapsulation,” Journal of Materials Research, V. 30, No. 9, May 2015, pp. 1563-1571.

39. Ojovan, M.I., and Lee, W.E., An Introduction to Nuclear Waste Immobilisation, second edition, Elsevier, 2013, 376 pp.

40. Provis, J.L., and Van Deventer, J.S.J., “Alkali-Activated Materials—State of the Art Report,” RILEM TC 224-AAM, RILEM/Springer, 2014, 388 pp.




  

Edit Module Settings to define Page Content Reviewer