Title: Factorial Design and Optimization of Ultra-High-Performance Concrete with Lightweight Sand

Author(s): Weina Meng, V. A. Samaranayake, and Kamal H. Khayat

Publication: Materials Journal

Volume: 115

Issue: 1

Appears on pages(s): 129-138

Keywords: autogenous shrinkage; compressive strength; factorial design; internal curing; lightweight sand; rheological properties; ultra-highperformance concrete (UHPC)

DOI: 10.14359/51700995

Date: 1/1/2018

Abstract:
In this study, lightweight sand is used as an internal curing agent in ultra-high-performance concrete (UHPC). A factorial design approach was employed to evaluate the effects of multiple mixture proportioning parameters that are important for mixture optimization of UHPC. The investigated mixture design parameters included the substitution volume ratio of lightweight sand for river sand (LWS/NS: 0 to 25%), the cementitious materials-to-sand volume ratio (cm/s: 0.8 to 1.2), and the water-cementitious materials ratio (w/cm: 0.17 to 0.23). The evaluated properties included fresh properties, compressive strengths at up to 91 days, and autogenous shrinkage at up to 28 days. Statistical models that take into account the coupling effects of mixture proportioning parameters were formulated to predict the UHPC properties. The w/cm and LWS/NS were the most significant parameters influencing the compressive strength and autogenous shrinkage, respectively. By replacing the river sand with 25% lightweight sand, the compressive strength at 91 days increased from 150 to 170 MPa (22.5 to 25.5 ksi) and the autogenous shrinkage at 28 days decreased from 410 to 70 μm/m (410 × 10–6 to 70 × 10–6 in./in.). The mixture with w/cm of 0.23, LWS/NS of 0.25, and cm/s of 1.2 is determined as the optimum UHPC mixture. The material properties of the mixture: the HRWR demand was 0.6%, the 28-day autogenous shrinkage was 260 μm/m (260 × 10–6 in./in.), and the 91-day compressive strength was 147 MPa (22.1 ksi).

Related References:

1. Graybeal, B., “Material Property Characterization of Ultra-High Performance Concrete,” FHWA-HRT-06-103, Federal Highway Administration, U.S. Department of Transportation, Washington, DC, 2006.

2. Habert, G.; Denarié, E.; Šajna, A.; and Rossi, P., “Lowering the Global Warming Impact of Bridge Rehabilitations by Using Ultra High Performance Fibre Reinforced Concretes,” Cement and Concrete Composites, V. 38, 2013, pp. 1-11. doi: 10.1016/j.cemconcomp.2012.11.008

3. Meng, W.; Valipour, M.; and Khayat, K., “Optimization and Performance of Cost-Effective Ultra-High Performance Concrete,” Materials and Structures, V. 50, No. 1, 2017. doi: 10.1617/s11527-016-0896-3

4. Meng, W., and Khayat, K. H., “Improving Flexural Performance of Ultra-High-Performance Concrete by Rheology Control of Suspending Mortar,” Composites. Part B, Engineering, V. 117, 2017, pp. 26-34. doi: 10.1016/j.compositesb.2017.02.019

5. Meng, W., and Khayat, K. H., “Mechanical Properties of Ultra-High-Performance Concrete Enhanced with Graphite Nanoplatelets and Carbon Nanofibers,” Composites. Part B, Engineering, V. 107, 2016, pp. 113-122. doi: 10.1016/j.compositesb.2016.09.069

6. Justs, J.; Wyrzykowski, M.; Bajare, D.; and Lura, P., “Internal Curing by Superabsorbent Polymers in Ultra-High Performance Concrete,” Cement and Concrete Research, V. 76, 2015, pp. 82-90. doi: 10.1016/j.cemconres.2015.05.005

7. Justs, J.; Wyrzykoski, M.; Winnefeld, F.; Bajare, D.; and Lura, P., “Influence of Superabsorbent Polymers on Hydration of Cement Pastes with Low Water-to-Binder Ratio,” Journal of Thermal Analysis and Calorimetry, V. 115, No. 1, 2014, pp. 425-432. doi: 10.1007/s10973-013-3359-x

8. Bao, Y.; Meng, W.; Chen, Y.; Chen, G.; and Khayat, K. H., “Measuring Mortar Shrinkage and Cracking by Pulse Pre-Pump Brillouin Optical Time Domain Analysis with a Single Optical Fiber,” Materials Letters, V. 145, 2015, pp. 344-346. doi: 10.1016/j.matlet.2015.01.140

9. Bentz, D., and Weiss, J., “Internal Curing: A 2010 State-of-the-Art Review,” NISTIR 7765, U.S. Department of Commerce, Washington, DC, 2011, 82 pp.

10. Bentz, D. P.; Lura, P.; and Roberts, J. W., “Mixture Proportioning for Internal Curing,” Concrete International, V. 27, No. 2, Feb. 2005, pp. 35-40.

11. De la Varga, I., and Graybeal, B., “Dimensional Stability of Grout-Type Materials used as Connections between Prefabricated Concrete Elements,” Journal of Materials in Civil Engineering, ASCE, V. 27, No. 9, 2015, p. 04014246. doi: 10.1061/(ASCE)MT.1943-5533.0001212

12. Weiss, J.; Bentz, D.; Schindler, A.; and Lura, P., “Internal Curing,” STRUCTURE, Jan. 2012, pp. 10-14.

13. Meng, W., and Khayat, K., “Effects of Saturated Lightweight Sand Content on Key Characteristics of Ultra-High-Performance Concrete,” Cement and Concrete Research, V. 101, 2017, pp. 46-54.

14. ASTM C1761/C1761M, “Standard Specification for Lightweight Aggregate for Internal Curing of Concrete,” ASTM International, West Conshohocken, PA, 2017, 8 pp.

15. Henkensiefken, R., “Internal Curing in Cementitious Systems Made Using Saturated Lightweight Aggregate,” PhD dissertation, Purdue University, West Lafayette, IN, 2008, 187 pp.

16. ACI Committee 239, “Committee on Ultra-High Performance Concrete,” Minutes of Committee Meeting Oct. 2012, ACI Convention 2012, Toronto, ON, Canada.

17. EFNARC, “Specification and Guidelines for Self-Compacting Concrete,” European Federation for Specialist Construction Chemicals and Concrete Systems, Norfolk, UK, English ed., 2002, 32 pp.

18. Tattersall, G. H., and Banfill, P. F. G., The Rheology of Fresh Concrete, Pitman, London, UK, 1983, 356 pp.

19. Vaughn, N. A., and Polnaszek, C., Design-Expert® software. Stat-Ease, Inc., Minneapolis, MN, 2007.

20. Lura, P.; van Breugel, K.; and Maruyama, I., “Effect of Curing Temperature and Type of Cement on Early-Age Shrinkage of High-Performance Concrete,” Cement and Concrete Research, V. 31, No. 12, 2001, pp. 1867-1872. doi: 10.1016/S0008-8846(01)00601-9

21. Lura, P.; Jensen, O. M.; and van Breugel, K., “Autogenous Shrinkage in High-Performance Cement Paste: An Evaluation of Basic Mechanism,” Cement and Concrete Research, V. 33, No. 2, 2003, pp. 223-232. doi: 10.1016/S0008-8846(02)00890-6

22. Jensen, O. M., and Hansen, P. F., “Water-Entrained Cement-Based Materials: I. Principles and Theoretical Background,” Cement and Concrete Research, V. 31, No. 4, 2001, pp. 647-654. doi: 10.1016/S0008-8846(01)00463-X

23. Duran-Herrera, A.; Aitcin, P. C.; and Petrov, N., “Effect of Saturated Lightweight Sand Substitution on Shrinkage in 0.35 w/b Concrete,” ACI Materials Journal, V. 104, No. 1, Jan.-Feb. 2007, pp. 48-52.

24. Montgomery, D., Design and Analysis of Experiments, John Wiley & Sons, Inc., New York, 2012.

25. Lotfy, A.; Hossain, K. M.; and Lachemi, M., “Application of Statistical Models in Proportioning Lightweight Self-Consolidating Concrete with Expanded Clay Aggregates,” Construction and Building Materials, V. 65, 2014, pp. 450-469. doi: 10.1016/j.conbuildmat.2014.05.027

26. User’s Manual of Design-Expert Software, Stat-Ease Inc., Minneapolis, MN, 2013.


ALSO AVAILABLE IN:

Electronic Materials Journal