Title: 
            End-Region Behavior of Pretensioned I-Girders Employing 0.7 in. (17.8 mm) Strands
        
        
            Author(s): 
            J. Salazar, H. Yousefpour, R. Alirezaei Abyaneh, H. Kim, A. Katz, T. Hrynyk, and O. Bayrak
        
        
            
                Publication: 
                Structural Journal
            
            
                Volume: 
                115
            
            
                Issue: 
                1
            
            
                Appears on pages(s): 
                91-102
            
            
                Keywords: 
                0.7 in. strands; bursting stresses; end-region cracking; pretensioned; spalling stresses; splitting resistance; transfer length
            
            
                DOI: 
                10.14359/51700783
            
        
        
            Date: 
            1/1/2018
        
        
            Abstract:
            This paper presents an experimental study on transfer length, end-region cracking, and transverse end-region stresses in pretensioned concrete I-girders fabricated using 0.7 in. (17.8 mm) diameter strands on a 2 x 2 in. (51 x 51 mm) grid. The full-scale specimens consisted of two Tx46 and two Tx70 girders that were fabricated in a controlled laboratory environment using different strand patterns and concrete release strengths. The detailing for mild-steel reinforcement was done according to the current practice in Texas for girders with smaller-diameter strands. The measured 24-hour transfer lengths from the specimens exceeded estimates by both AASHTO LRFD and ACI 318-14 provisions. The observed crack widths in the specimens within 28 days after prestress transfer were generally limited to 0.007 in. (0.18 mm), indicating satisfactory performance for exposure to deicing chemicals according to ACI 224R guidelines. However, noticeably greater transverse forces were observed in the end regions of the specimens compared to the resistance required by AASHTO LRFD specifications.
        
     
    
    
    
            Related References:
                
                        1. Tadros, M. K., and Morcous, G., “Impact of 0.7 Inch Diameter Strands on NU I-Girders,” Technical Report, Nebraska Department of Roads, Lincoln, NE, 2011, 203 pp.
                    
                        2. Salazar, J.; Yousefpour, H.; Katz, A.; Alirezaei Abyaneh, R.; Kim, H.; Garber, D.; Hrynyk, T.; and Bayrak, O., “Benefits of Using 0.7 in. (18 mm) Diameter Strands in Precast, Pretensioned Girders: A Parametric Investigation,” PCI Journal, V. 62, No. 6, Nov-Dec. 2017, pp. 59-75. 
                    
                        3. Katz, A.; Yousefpour, H.; Kim, H.; Alirezaei Abyaneh, R.; Salazar, J.; Hrynyk, T.; and Bayrak, O., “Shear Performance of Pretensioned Concrete I-Girders Employing 0.7 in. (17.8 mm) Strands,” ACI Structural Journal, V. 114, No. 5, Sept.-Oct. 2017, pp. 1273-1284.
                    
                        4. American Association of State Highway and Transportation Officials (AASHTO), “AASHTO LRFD Bridge Design Specifications,” seventh edition with 2015 and 2016 Interim Revisions, Washington, DC, 2016, 2150 pp.
                    
                        5. ACI Committee 318, “Building Code Requirements for Structural Concrete (ACI 318R-14) and Commentary (ACI 318R-14),” American Concrete Institute, Farmington Hills, MI, 2014, 520 pp.
                    
                        6. Russell, B. W., and Burns, N. H., “Measured Transfer Lengths of 0.5 and 0.6 in. Strands in Pretensioned Concrete,” PCI Journal, V. 41, No. 5, 1996, pp. 44-65. doi: 10.15554/pcij.09011996.44.65
                    
                        7. Comité Euro-International Du Beton (CEB), “Anchorage Zones of Prestressed Concrete Members,” CEB Bulletin No. 181, 1987, 137 pp.
                    
                        8. Hoyer, E., and Friedrich, E., “Beitrag zur Frage der Haftspannung in Eisenbetonbauteilen [Contribution to the Question of Bond in Concrete Elements],” Beton und Eisen, V. 30, No. 6, 1939, pp. 107-110.
                    
                        9. Dang, C. N.; Floyd, R. W.; Hale, M.; and Marti-Vargas, J. R., “Measured Transfer Lengths of 0.7 in. (17.8 mm) Strands for Pretensioned Beams,” ACI Structural Journal, V. 113, No. 3, May-June 2016, pp. 85-94.
                    
                        10. Vadivelu, J., “Impact of Larger Diameter Strands on AASHTO/PCI Bulb-Tees,” master’s thesis, University of Tennessee, Knoxville, TN, 2009, 114 pp.
                    
                        11. Morcous, G.; Hanna, K.; and Tadros, M. K., “Use of 0.7-in. Diameter Strands in Pretensioned Bridge Girders,” PCI Journal, V. 56, No. 4, 2011, pp. 65-82. doi: 10.15554/pcij.09012011.65.82
                    
                        12. Morcous, G.; Assad, S.; Hatami, A.; and Tadros, M. K., “Implementation of 0.7 in. Diameter Strands at 2.0 x 2.0 in. Spacing in Pretensioned Bridge Girders,” PCI Journal, V. 59, No. 3, 2014, pp. 145-158. doi: 10.15554/pcij.06012014.145.158
                    
                        13. Texas Department of Transportation (TxDOT), “Concrete I-Girder Details, Standard Drawings by the Bridge Division, Austin, Texas,” Austin, TX, 2015, 2 pp.
                    
                        14. ASTM C39/C39M-14, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2014, 7 pp.
                    
                        15. ASTM C469/C469M-14, “Standard Test Method for Static Modulus of Elasticity and Poisson’s Ratio of Concrete in Compression,” ASTM International, West Conshohocken, PA, 2014, 5 pp.
                    
                        16. ASTM A370-16, “Standard Test Methods and Definitions for Mechanical Testing of Steel Products,” ASTM International, West Conshohocken, PA, 2016, 49 pp.
                    
                        17. ASTM A1061/A1061M-16, “Standard Test Methods for Testing Multi-Wire Steel Prestressing Strand,” ASTM International, West Conshohocken, PA, 2016, 4 pp.
                    
                        18. O’Callaghan, M. R., “Tensile Stresses in the End Regions of Pretensioned I-Beams at Release,” master’s thesis, University of Texas at Austin, Austin, TX, 2007, 265 pp.
                    
                        19. Barnes, R.; Grove, J.; and Burns, N., “Experimental Assessment of Factors Affecting Transfer Length,” ACI Structural Journal, V. 100, No. 6, Nov.-Dec. 2003, pp. 740-748.
                    
                        20. ACI Committee 224, “Control of Cracking in Concrete Structures (ACI 224R-01),” American Concrete Institute, Farmington Hills, MI, 2001, 46 pp.
                    
                        21. Tadros, M. K.; Badie, S. S.; and Tuan, C. Y., “Evaluation and Repair Procedures for Precast/Prestressed Concrete Girders with Longitudinal Cracking in the Web,” NCHRP Report 654, Transportation Research Board, Washington, DC, 2010, 66 pp.
                    
                        22. Texas Department of Transportation (TxDOT), “Standard Specifications for Construction and Maintenance of Highways, Streets, and Bridges,” Austin, TX, 2014, 919 pp.
                    
                        23. Hovell, C.; Avedano, A.; Moore, A.; Dunkman, D.; Bayrak, O.; and Jirsa, J., “Structural Performance of Texas U-Beams at Prestressed Transfer and under Shear-Critical Loads,” Technical Report, Center for Transportation Research, Austin, TX, 2011, 355 pp.
                    
                        24. Dunkman, D., “Bursting and Spalling in Pretensioned U-Beams,” master’s thesis, University of Texas at Austin, Austin, TX, 2009, 242 pp.
                    
                        25. Alirezaei Abyaneh, R., “Computational Modeling of Prestress Transfer, End-Region Cracks, and Shear Behavior in Prestressed Concrete I-Girders Employing Large-Diameter Strands,” master’s thesis, University of Texas at Austin, Austin, TX, 2016, 95 pp.