Effect of Embedment Length on Bond of 18 mm (0.7 in.) Strand by Pullout Test

International Concrete Abstracts Portal

The International Concrete Abstracts Portal is an ACI led collaboration with leading technical organizations from within the international concrete industry and offers the most comprehensive collection of published concrete abstracts.

  


Title: Effect of Embedment Length on Bond of 18 mm (0.7 in.) Strand by Pullout Test

Author(s): Xin Jiang, John Cabage, Yuan Jing, Zhongguo John Ma, and Edwin G. Burdette

Publication: Structural Journal

Volume: 114

Issue: 3

Appears on pages(s): 707-717

Keywords: 18 mm (0.7 in.) diameter strands; bond; development length; pullout; strand embedment length; transfer length

DOI: 10.14359/51689442

Date: 5/1/2017

Abstract:
A series of experimental tests were conducted to investigate the bond performance of untensioned 18 mm (0.7 in.) diameter strand in high-strength concrete. Eight pullout tests were conducted on prismatic specimens with four different strand embedment lengths. The relationship between strand slip and pullout force, along with the concrete surface strain distribution along the strand and its development with force, was investigated. Observed failure modes of the pullout tests varied, but seemed to be dependent on strand embedment length. Also, transfer length Lt and development length Ld were examined. The measured transfer length was 610 mm (24 in.) and the observed development length was from 910 to 1220 mm (36 to 48 in.) for the 18 mm (0.7 in.) diameter strand. A correlation is demonstrated between transfer and development lengths and strand embedment length in pullout tests in terms of strand stress development and strand slip in the end. Crack effect in flexural beam test was discussed. Pullout testing of specimens with different strand embedment lengths can determine transfer length and development length, and serve as a basis in predicting bond performance in prestressed concrete members.

Related References:

1. Schuler, G., “Producer’s Experience with 10,000 psi Concrete and 0.7-in. Diameter Strands,” HPC Bridge Views, No. 54, 2009, http://www.hpcbridgeviews.com/i54/Article4.asp (accessed Aug. 2013)

2. Song, W.; Ma, Z.; Vadivelu, J.; and Burdette, E., “Transfer Length and Splitting Force Calculation for Pretensioned Concrete Girders with High-capacity Strands,” Journal of Bridge Engineering, V. 19, No. 7, 2014, pp. 0401426/1-8.

3. Morcous, G.; Hatami, A.; Maguire, M.; Hanna, K.; and Tadros, M. K., “Mechanical and Bond Properties of 18-mm-(0.7-in.-) Diameter Prestressing Strands,” Journal of Materials in Civil Engineering, ASCE, V. 24, No. 6, 2012, pp. 735-744. doi: 10.1061/(ASCE)MT.1943-5533.0000424

4. Morcous, G.; Hanna, K.; and Tadros, M. K., “Use of 0.7-in.-Diameter Strands in Pretensioned Bridge Girders,” PCI Journal, V. 56, No. 4, 2011, pp. 65-82. doi: 10.15554/pcij.09012011.65.82

5. Maguire, M.; Morcous, G.; and Tadros, M. K., “Structural Performance of Precast/Prestressed Bridge Double-Tee Girders Made of High-Strength Concrete, Welded Wire Reinforcement, and 18-mm-Diameter Strands,” Journal of Bridge Engineering, ASCE, V. 18, No. 10, 2013, pp. 1053-1061. doi: 10.1061/(ASCE)BE.1943-5592.0000458

6. Morcous, G.; Assad, S.; Hatami, A.; and Tadros, M. K., “Implementation of 0.7 in. Diameter Strands at 2.0 x 2.0 in. Spacing in Pretensioned Bridge Girders,” PCI Journal, V. 59, No. 3, 2014, pp. 145-158. doi: 10.15554/pcij.06012014.145.158

7. Dang, C. N.; Floyd, R. W.; Hale, W. M.; and Marti-Vargas, J. R., “Measured Transfer Lengths of 0.7 in. (17.8 mm) Strands for Pretensioned Beams,” ACI Structural Journal, V. 113, No. 1, Jan.-Feb. 2016, pp. 85-94. doi: 10.14359/51687941

8. Dang, C. N.; Floyd, R. W.; Hale, W. M.; and Martí-Vargas, J. R., “Spacing Requirements of 0.7 in. (18 mm) Diameter Prestressing Strands,” PCI Journal, V. 61, No. 1, 2016, pp. 70-87. doi: 10.15554/pcij.01012016.70-87

9. Guyon. Y., Prestressed Concrete, Contractors Record and Municipal Engineering, London, UK, 1953.

10. Janney, J. R., “Nature of Bond in Pre-Tensioned Prestressed Concrete,” ACI Journal Proceedings, V. 51, No. 9, May, pp. 717-736.

11. Brearley, L. M. Jr., and Johnston, D. W., “Pull-Out Bond Tests of Epoxy-Coated Prestressing Strand,” Journal of Structural Engineering, ASCE, V. 116, No. 8, 1990, pp. 2236-2252. doi: 10.1061/(ASCE)0733-9445(1990)116:8(2236)

12. Logan, D. R., ��Acceptance Criteria for Bond Quality of Strands for Pretensioned Prestressed Concrete Application,” PCI Journal, V. 42, No. 2, 1997, pp. 52-90. doi: 10.15554/pcij.03011997.52.90

13. Rose, D. R., and Russell, B. W., “Investigation of Standardized Tests to Measure the Bond Performance of Prestressing Strand,” PCI Journal, V. 42, No. 4, 1997, pp. 56-80. doi: 10.15554/pcij.07011997.56.80

14. AASHTO LRFD, “Bridge Design Specifications,” sixth edition, American Association for State Highway and Transportation Officials, Washington, DC, 2012.

15. Russell, B. W., and Burns, N. H., “Design Guidelines for Transfer, Development and Debonding of Large Diameter Seven Wire Strands in Pretensioned Concrete Girders,” Report No. 1210-5F, Center for Transportation Research, University of Texas at Austin, Austin, TX, 1993, 464 pp.

16. Leonhardt, F., Prestressed Concrete: Design and Construction, Wilhelm Ernst &Sohn, Berlin, Germany, 1964.

17. fib, “Bond of Reinforcement in Concrete,” State-of-Art Report Bulletin 10, Lausanne, Switzerland, 2000, 427 pp.

18. ASTM A981/A981M-11, “Standard Test Method for Evaluating Bond Strength for 0.600-in. (15.24-mm) Diameter Prestressing Steel Strand, Grade 270 (1860), Uncoated, Used in Prestressed Ground Anchors,” ASTM International, West Conshohocken, PA, 2011, 3 pp.

19. Ramirez, J., and Russell, B., “Transfer, Development, and Splice Length for Strand/Reinforcement in High-Strength Concrete,” NCHRP Report 603, Washington, DC, 2008, 122 pp.

20. Moustafa, S., “Pull-Out Strength of Strand and Lifting Loops,” Concrete Technology Associates Technical Bulletin 74-B5, Precast/Prestressed Concrete Institute, Chicago, IL, 1974.

21. Stocker, M. T., and Sozen, M. A., “Investigation of Prestressed Reinforced Concrete for Highway Bridges, Part V: Bond Characteristics of Prestressing Strand,” Engineering Experiment Station Bulletin 503, University of Illinois, Urbana-Champaign, IL, 1970, 119 pp.

22. ASTM C39/C39M-12, “Standard Test Method for Compressive Strength of Cylindrical Concrete Specimens,” ASTM International, West Conshohocken, PA, 2012, 7 pp.

23. Morcous, G.; Hanna, K.; and Tadros, M., “Transfer and Development Length of 0.7 in. Diameter Strands in Pretensioned Concrete Bridge Girders,” HPC Bridge Views, No. 64, 2010, http://www.hpcbridgeviews.com/i64/Article3.asp. (accessed Aug. 2012)

24. Cabage, J.; Ma, Z.; Jiang, X.; and Burdette, E. G., “An Assessment of Development Length when Using High-Capacity Strands,” 2014 PCI Conference and National Bridge Convention, 2014.

25. ASTM A1081/A1081-12, “Standard Test Method for Evaluating Bond of Seven-Steel Prestressing Strand,” ASTM International, West Conshohocken, PA, 2012, 5 pp.

26. Morcous, G.; Hanna, K.; and Tadros, M. K., “Bottom Flange Reinforcement in NU I-Girders,” NDOR Project No. P331, University of Nebraska-Lincoln, Lincoln, NE, 2010, 60 pp.

27. Ma, Z.; Tadros, M. K.; and Baishya, M., “Shear Behavior of Pretensioned High-Strength Concrete Bridge I-Girders,” ACI Structural Journal, V. 97, No. 1, Jan.-Feb. 2000, pp. 185-192.

28. Deatherage, J. H.; Burdette, E. G.; and Chew, C. K., “Development Length and Lateral Spacing Requirements of Prestressing Strand for Prestressed Concrete Bridge Girders,” PCI Journal, V. 39, No. 1, 1994, pp. 70-83. doi: 10.15554/pcij.01011994.70.83


ALSO AVAILABLE IN:

Electronic Structural Journal



  

Edit Module Settings to define Page Content Reviewer