Title: Torsion of Structural Concrete-Plain Cocnrete Rectangular Sections

Author(s): Thomas T.C. Hsu

Publication: Symposium Paper

Volume: 18

Issue:

Appears on pages(s): 203-238

Keywords:

DOI: 10.14359/17570

Date: 1/1/1968

Abstract:
An extensive laboratory investigation of plain and reinforced concrete members subject to torsion is being reported in a series of papers. This paper concerns plain concrete members of rectangular cross-section subjected to pure torsion.




  