SPEC-351.5-24: Epoxy Grout Installation between Foundations and Equipment Bases—Specification (SI Units)

Abstract:

This Specification covers minimum requirements for installing epoxy grouting between foundations and equipment bases. Included are requirements for materials, placement, forming, testing, repair, and quality control. A mandatory requirements checklist and an optional requirements checklist are provided to assist the Architect/Engineer in supplementing the requirements of this Specification as required or needed by designating or specifying individual project requirements.