SPEC-548.14-25: Repairing Concrete with Epoxy Mortar - Specification

Abstract:

This Specification describes the work of repairing defects in hardened portland-cement concrete with an epoxy mortar. Included are controls for epoxy resin system labeling, storage, handling, surface evaluation and preparation, mixing and application, inspection, quality control, and testing.