Home > Publications > Concrete Resource Subscriptions > ACI PLUS Platform > 562 PLUS Repair Subscription > Repair Search
The ACI 562 PLUS Repair Collection contains all new repair related Standards, Practices & Online Learning. The most recently added include
ACI PRC-325.13-25: Concrete Overlays for Pavement Rehabilitation—Report
ACI SPEC-563-25: Repair of Concrete in Buildings—Specification (SI Units)
On-Demand Course: Serviceability and Performance Evaluation of Concrete Structures (Part 2)
On-Demand Course: Serviceability and Performance Evaluation of Concrete Structures (Part 1)
On-Demand Course: Who Is Responsible? Clarifying Accountability in Concrete Construction and Rehabilitation
ACI CODE-440.13-24: Strengthening Structural Concrete with Fiber-Reinforced Polymer (FRP) Systems—Code Requirements and Commentary (SI Units)
ACI SPEC-548.14-25: Repairing Concrete with Epoxy Mortar - Specification
Title: ACI SPEC-548.14-25: Repairing Concrete with Epoxy Mortar - Specification
Author(s): ACI Committee 548
Document Type: Standards (codes & specs)
Date: August 2025
Abstract: This Specification describes the work of repairing defects in hardened portland-cement concrete with an epoxy mortar. Included are controls for epoxy resin system labeling, storage, handling, surface evaluation and preparation, mixing and application, inspection, quality control, and testing.. Keywords: adhesion to concrete; aggregate; concrete construction; epoxy; epoxy mortar; hardened concrete quality control; repairs; resurfacing.