How is the temperature of concrete measured?

In This Section

Other Sources for Answers

Search other resources on the ACI website for answers to technical questions

Technical Questions

ACI Committees, Membership, and Staff have answered common questions on a variety of concrete related topics.



How is the temperature of concrete measured?

Q. How is the temperature of concrete measured?

 

A. ASTM C1064 is the standard test method to measure temperature of freshly mixed concrete. The temperature is read from a temperature measuring device inserted into the concrete. Temperature affects the rate of hydration.

 

References: SP-1(02); ACI 209R-92; ASTM C1064

Topics in Concrete: Concrete Fundamentals; Hot Weather; Mass Concrete; Testing of Concrete